# US 2017/0304687 A1 · Method and apparatus for enhancing surface strike performance

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0304687 A1
- Document ID: US20170304687A1
- Status: Published application
- Kind: A1
- Application number: 15/491,645
- Filed: 2017-04-19
- Published: 2017-10-26
- Earliest claimed: 2016-04-20
- Inventors: ADAM C. SCLAFANI
- Web page: https://patentgrep.com/patent/US20170304687A1

## CPC

- A63B 53/047: {iron-type}
- A63B 53/04: Heads
- A63B 53/0466: {wood-type}
- A63B 53/0416: {Heads having an impact surface provided by a face insert}
- A63B 2209/00: Characteristics of used materials
- A63B: APPARATUS FOR PHYSICAL TRAINING, GYMNASTICS, SWIMMING, CLIMBING, OR FENCING; BALL GAMES; TRAINING EQUIPMENT (apparatus for passive exercising, massage A61H)

## Abstract

An apparatus is disclosed having a face which includes a striking surface. The striking surface has a combination of properties configured to enhance performance characteristics, such as a launch angle, carry distance, and spin rate of an associated ball. The combination of properties of the striking surface at least includes an adequate hardness, smoothness, and durability. A method of enhancing surface strike performance is also disclosed. The method includes providing an associated item of sports equipment with a face including a ball striking surface having a combination of properties such as an adequate hardness, smoothness, and durability.

## Claims

### Claim 1

An apparatus for enhancing surface strike performance, comprising:
a face including a striking surface, wherein the striking surface has a combination of properties configured to improve performance characteristics of an associated ball;
wherein the combination of properties of the striking surface includes a hardness of at least Shore D 65, a surface roughness of Ra 1 μm or less, and a resistance to indentation at 1,500 psi or greater for a duration of about 30 minutes measured according to Mil-D-3134F.

### Claim 2 (depends on 1)

The apparatus of claim 1, wherein the performance characteristics include at least one of an increased launch angle, an increased carry distance, and a decreased spin rate of the associated ball.

### Claim 3 (depends on 1)

The apparatus of claim 1, wherein the combination of properties of the striking surface further includes a wear resistance minimum of zero weight loss at a load of 1 kg per 1000 cycles measured according to ASTM-C-501.

### Claim 4 (depends on 1)

The apparatus of claim 1, wherein the combination of properties of the striking surface further includes a flexural strength of greater than about 3,000 psi measured according to ASTM C-580.

### Claim 5 (depends on 1)

The apparatus of claim 1, wherein the combination of properties of the striking surface further includes a tensile strength of greater than about 3,000 psi measured according to ASTM C-307.

### Claim 6 (depends on 1)

The apparatus of claim 1, wherein the combination of properties of the striking surface further includes a compressive strength of greater than about 5,000 psi measured according to ASTM C-579.

### Claim 7 (depends on 1)

The apparatus of claim 1, wherein the striking surface comprises a coating applied to at least a portion of the face.

### Claim 8 (depends on 7)

The apparatus of claim 7, wherein the coating is a polyurethane.

### Claim 9 (depends on 8)

The apparatus of claim 8, wherein the coating has a thickness of about 100 μm to about 200 μm.

### Claim 10 (depends on 1)

The apparatus of claim 1, wherein the striking surface and the face are integral.

### Claim 11 (depends on 1)

The apparatus of claim 1, wherein the striking surface is configured to have one or more ridges and/or grooves.

### Claim 12 (depends on 1)

The apparatus of claim 1, wherein the striking surface is configured to be substantially smooth.

### Claim 13 (depends on 1)

The apparatus of claim 1, wherein the striking surface comprises an insert attached to the face.

### Claim 14 (depends on 13)

The apparatus of claim 13, wherein the insert further comprises a substrate and a coating applied to at least a portion of the substrate.

### Claim 15 (depends on 14)

The apparatus of claim 14, wherein the coating is a polyurethane.

### Claim 16 (depends on 13)

The apparatus of claim 13, wherein the striking surface is configured to have one or more ridges and/or grooves.

### Claim 17 (depends on 13)

The apparatus of claim 13, wherein the striking surface is configured to be substantially smooth.

### Claim 18

A method of enhancing surface strike performance, comprising:
providing a face of an associated item of sports equipment with a striking surface having a combination of properties configured to improve performance characteristics of an associated ball;
wherein the combination of properties of the striking surface includes a hardness of at least Shore D 65, a surface roughness of Ra 1 μm or less, and a resistance to indentation at 1,500 psi or greater for a duration of about 30 minutes measured according to Mil-D-3134F; and
wherein the performance characteristics include at least one of an increased launch angle, an increased carry distance, and a decreased spin rate.

### Claim 19 (depends on 18)

The method of claim 18, further comprising applying a coating of polyurethane to the face to form the striking surface having the combination of properties.

### Claim 20

An apparatus for enhancing surface strike performance, comprising:
a face including a striking surface, wherein the striking surface is formed from a coating applied to at least a portion of the face, and the coating has a combination of properties configured to improve performance characteristics of an associated ball, the combination of properties including a hardness of at least Shore D 65, a surface roughness of Ra 1 μm or less, and a resistance to indentation at 1,500 psi or greater for a duration of about 30 minutes measured according to Mil-D-3134F;
wherein the coating is an oil modified polyurethane having a thickness of about 100 μm to about 200 μm; and
wherein the performance characteristics include at least one of an increased launch angle, an increased carry distance, and a decreased spin rate.