# US 2017/0294579 A1 · Resistive random access memory device and method for fabricating the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0294579 A1
- Document ID: US20170294579A1
- Status: Published application
- Kind: A1
- Application number: 15/634,349
- Filed: 2017-06-27
- Published: 2017-10-12
- Earliest claimed: 2014-09-24
- Assignees: Winbond Electronics Corp.
- Applicants: Winbond Electronics Corp.
- Inventors: Wen-Yueh JANG; Chia Hua HO
- Web page: https://patentgrep.com/patent/US20170294579A1

## CPC

- H10N 70/841: {Electrodes}
- H10N 70/011: {Manufacture or treatment of multistable switching devices}
- H10N 70/021: {Formation of switching materials, e.g. deposition of layers}
- H10N 70/20: Multistable switching devices, e.g. memristors
- H10N 70/826: {adapted for essentially vertical current flow, e.g. sandwich or pillar type devices}
- H10N 70/8833: {Binary metal oxides, e.g. TaOx}
- H10N 70/8836: {Complex metal oxides, e.g. perovskites, spinels}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR

## Abstract

A resistive random access memory device and a method for fabricating the same are presented. The resistive random access memory device includes a first electrode having a first dopant within. A second electrode is disposed on the first electrode. A resistive switching layer is disposed between the first electrode and the second electrode.

## Claims

### Claim 1

A method for fabricating a resistive random access memory device, comprising:
providing a semiconductor substrate;
forming a first electrode on the semiconductor substrate;
doping a dopant in the first electrode;
forming a resistive switching layer on the first electrode; and
forming a second electrode on the resistive switching layer.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein the step of doping the dopant in the first electrode is performed during the formation of the first electrode, and the step of forming the first electrode comprises performing a co-sputtering process using a first electrode material and the dopant as a sputter target.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein the step of doping the dopant into the first electrode is performed after forming the first electrode, and the step of doping the dopant into the first electrode comprises performing an ion implantation to dope the dopant into the first electrode.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein the step of forming the first electrode comprises:
placing a sputter target into a sputter chamber;
placing the semiconductor substrate into the sputter chamber;
introducing a first gas into the sputter chamber, and performing a first sputtering process to the semiconductor substrate to form a metal nitride layer on the semiconductor substrate, which has a first thickness; and
introducing a second gas into the sputter chamber, and performing a second sputtering process to the semiconductor substrate to form a metal oxide layer on the metal nitride layer, wherein the metal oxide layer has a second thickness, and wherein both the first thickness and the second thickness are smaller than a thickness of the second electrode.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein a thickness of the first electrode is smaller than a thickness of the second electrode.

### Claim 6 (depends on 1)

The method as claimed in claim 1, further comprising:
conformally forming a barrier liner layer on the first electrode, the resistive switching layer, and the second electrode.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein the dopant comprises carbon, boron, or combinations thereof.

### Claim 8 (depends on 1)

The method as claimed in claim 1, wherein the step of forming the first electrode comprises:
forming a first metal nitride layer having a first thickness on the on the semiconductor substrate; and
forming a metal oxide layer having a second thickness on the first metal nitride layer.

### Claim 9 (depends on 8)

The method as claimed in claim 8, wherein the first thickness and the second thickness are smaller than a thickness of the second electrode.

### Claim 10 (depends on 8)

The method as claimed in claim 8, wherein the step of forming the first electrode further comprises:
forming a second metal nitride layer having a third thickness on the metal oxide layer.

### Claim 11 (depends on 10)

The method as claimed in claim 10, wherein the first thickness, the second thickness, and the third thickness are smaller than a thickness of the second electrode.

### Claim 12 (depends on 10)

The method as claimed in claim 10, wherein the second metal nitride layer has the dopant within and contacts the resistive switching layer.

### Claim 13

A resistive random access memory device, comprising:
a first electrode having a dopant within;
a second electrode disposed on the first electrode;
a resistive switching layer disposed between the first electrode and the second electrode; and
a barrier liner layer conformally disposed on the first electrode, the resistive switching layer, and the second electrode.

### Claim 14 (depends on 13)

The resistive random access memory device as claimed in claim 13, wherein the first electrode is a bottom electrode, and the second electrode is a top electrode.

### Claim 15 (depends on 13)

The resistive random access memory device as claimed in claim 13, wherein the dopant comprises carbon, boron, or combinations thereof.

### Claim 16 (depends on 13)

The resistive random access memory device as claimed in claim 13, wherein a thickness of the first electrode is smaller than a thickness of the second electrode.

### Claim 17

A resistive random access memory device, comprising:
a first electrode having a dopant within;
a second electrode disposed on the first electrode; and
a resistive switching layer disposed between the first electrode and the second electrode, wherein the dopant is configured to increase a planarity of an interface between the first electrode and the resistive switching layer.

### Claim 18 (depends on 17)

The resistive random access memory device as claimed in claim 17, wherein the dopant comprises carbon, boron, or combinations thereof.

### Claim 19 (depends on 17)

The resistive random access memory device as claimed in claim 17, further comprising:
a barrier liner layer conformally disposed on the first electrode, the resistive switching layer, and the second electrode.

### Claim 20 (depends on 17)

The resistive random access memory device as claimed in claim 17, wherein a thickness of the first electrode is smaller than a thickness of the second electrode.