# US 2017/0294556 A1 · Light emitting diode and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0294556 A1
- Document ID: US20170294556A1
- Status: Published application
- Kind: A1
- Application number: 15/632,127
- Filed: 2017-06-23
- Published: 2017-10-12
- Earliest claimed: 2015-07-24
- Assignees: Industry Foundation of Chonnam National University
- Applicants: Industry Foundation of Chonnam National University
- Inventors: Taeksoo JI; Jinyoung PARK; Jinhong LEE; Wangki KIM; Jaesam SHIM; Kwangjae LEE
- Web page: https://patentgrep.com/patent/US20170294556A1

## CPC

- H10H 20/811: having quantum effect structures or superlattices, e.g. tunnel junctions
- H10H 20/01335: {the light-emitting regions comprising nitride materials}
- H10H 20/812: within the light-emitting regions, e.g. having quantum confinement structures
- H10H 20/824: comprising only Group III-V materials, e.g. GaP
- H10H 20/825: containing nitrogen, e.g. GaN
- H10P 14/3252: {Alternating layers, e.g. superlattice}
- H10P 14/3254: {Graded layers}
- H10H 20/815: having stress relaxation structures, e.g. buffer layers
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A light emitting diode and a method of manufacturing the light emitting diode are provided. The light emitting diode includes an n-type semiconductor layer, an inclined type superlattice thin film layer, an active layer, and a p-type semiconductor layer. The n-type semiconductor layer is disposed on a substrate. The inclined type superlattice thin film layer is disposed on the n-type semiconductor layer and includes a plurality of thin film pairs in which InGaN thin films and GaN thin films are sequentially stacked. The active layer having a quantum well structure is disposed on the inclined type superlattice thin film layer. The p-type semiconductor layer is disposed on the active layer. Composition ratio of Indium (In) included in the InGaN thin film is increased as getting closer to the active layer. Thus, internal residual strain is reduced, and quantum confinement effect is enhanced, and internal quantum efficiency is increased.

## Claims

### Claim 1

A method of manufacturing a light emitting diode, comprising:
forming an n-type semiconductor layer on a substrate;
forming an inclined type superlattice thin film layer including a plurality of thin film pairs in which InGaN thin films and GaN thin films are sequentially stacked on the n-type semiconductor layer;
forming an active layer having a quantum well structure on the inclined type superlattice thin film layer; and
forming a p-type semiconductor layer on the active layer,
wherein composition ratio of indium (In) included in the InGaN thin film is increased as getting closer to the active layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein forming of the inclined type superlattice thin film layer comprises:
a first step of forming the InGaN thin film; and
a second step of removing indium included in an upper portion of the InGaN thin film to form the thin film pairs in which the InGaN thin films and the GaN thin films are sequentially stacked,
wherein the first step and the second step are alternately performed repeatedly a plurality of times.

### Claim 3 (depends on 2)

The method of claim 2, wherein the first step is performed under nitrogen atmosphere using a metal organic chemical vapor deposition (MOCVD) method.

### Claim 4 (depends on 2)

The method of claim 2, wherein the second step comprises supplying hydrogen (H2) on an upper portion of the InGaN thin film and removing indium (In) included in the upper portion of the InGaN thin film.

### Claim 5 (depends on 4)

The method of claim 4, wherein the hydrogen is supplied for 25 seconds to 30 seconds at a speed in a range of 8,000 sccm to 8,500 sccm.

### Claim 6 (depends on 2)

The method of claim 2, wherein the inclined type superlattice thin film layer is formed by alternately performing the first step and the second step repeatedly 2 to 100 times.

### Claim 7 (depends on 2)

The method of claim 2, wherein after the first step and the second step are alternately performed, the steps are performed at a temperature lower than the temperature of previous steps during repeatedly performing of the first step and the second step.

### Claim 8 (depends on 7)

The method of claim 7, wherein during repeatedly performing of the first step and the second step, the steps are performed at a temperature lower than the temperature of previous steps by 5° C.

### Claim 9 (depends on 1)

The method of claim 1, wherein before forming of the active layer of the quantum well structure on the inclined type superlattice thin film layer, further comprising forming a GaN layer on the inclined type superlattice thin film layer.