# US 2017/0294545 A1 · A process for preparing passivated emitter rear contact (perc) solar cells

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0294545 A1
- Document ID: US20170294545A1
- Status: Published application
- Kind: A1
- Application number: 15/514,287
- Filed: 2015-12-31
- Published: 2017-10-12
- Earliest claimed: 2015-07-09
- Assignees: Csi Cells Co., Ltd.
- Applicants: Csi Cells Co., Ltd
- Inventors: Shuai ZOU; Weixu LONG; Xusheng WANG; Guoqiang XING
- Web page: https://patentgrep.com/patent/US20170294545A1

## CPC

- H10F 77/703: {of the semiconductor bodies, e.g. textured active layers}
- H10F 10/14: Photovoltaic cells having only PN homojunction potential barriers
- H10F 10/146: {Back-junction photovoltaic cells, e.g. having interdigitated base-emitter regions on the back side}
- H10F 71/121: {The active layers comprising only Group IV materials}
- H10F 71/129: {Passivating}
- H10F 77/315: {the coatings being antireflective or having enhancing optical properties}
- Y02E 10/547: Monocrystalline silicon PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A process for preparing a passivated emitter rear contact solar cell, which includes the steps as follows: removing the damaged layer on the surface of the silicon wafer and at the same time polishing both surfaces, texturing, forming PN junction, etching, removing the glass impurity, depositing a passivation film on the back surface, depositing a passivating antireflective layer on the front surface, making local openings on the back surface, screen printing of metal paste on both the front surface and the back surface and sintering, in which the texturing step employs a catalytic metal etching approach, and the textured structure is a nanometer-level textured structure. The present invention has combined removing the damaged layer on the surface of the silicon wafer and polishing both the front and back surfaces into one single step, and thus has simplified the production process and reduced the production cost.

## Claims

### Claim 1

A process for preparing a passivated emitter rear contact, wherein the following steps: removing a damaged layer on the surface of a silicon wafer and at the same time polishing both surfaces thereof, texturing, forming PN junction, etching, removing the glass impurity, depositing a passivation film on a back surface thereof, depositing a passivating antireflective layer on a front surface thereof, making local openings on the back surface, screen printing of metal paste on both the front surface and the back surface and firing;
wherein the step of texturing employs a catalytic metal etching approach, and the textured surface structure is a nanometer-level structure with textured surface.

### Claim 2 (depends on 1)

The preparation process as set forth in claim 1, wherein the step of removing a damaged layer on the surface of a silicon wafer and at the same time polishing both surfaces thereof is carried out in an acidic liquid or in an alkali liquid, and the operating time thereof is from 2 to 20 minutes, the acidic liquid is a mixture of HNO3 and HF, or a mixture of H2CrO4 and HF; the temperature is from 5 to 45° C.;
in a mixture of HNO3 and HF, the ratio by volume of HNO3 (69%)/HF (49%) or of H2CrO4 (60%)/HF (49%) is greater than 4:1; and
the alkali liquid is selected from a NaOH solution, a KOH solution or a tetramethylammonium hydroxide (TMAH) solution, an operating temperature is within a range of from 5 to 95° C., and a volumetric concentration of the alkali liquid is higher than 1%.

### Claim 3 (depends on 2)

The preparation process as set forth in claim 2, wherein an operating time of the step of removing a damaged layer on the surface of a silicon wafer and at the same time polishing both surfaces thereof is from 2 to 10 minutes.

### Claim 4 (depends on 1)

The preparation process as set forth in claim 1, wherein the step of texturing is carried out as follows: first placing the silicon wafer into a solution containing metal ions for soaking, so as to allow surfaces of the silicon wafer to be covered with a layer of nanometer metal particles;
and then using a chemical etching liquid to treat each of the surfaces of the silicon wafer, so as to form the nanometer-level textured structure, wherein the chemical etching liquid is a solution of hydrofluoric acid that contains an oxidant.

### Claim 5 (depends on 4)

The preparation process as set forth in claim 4, wherein the solution containing metal ions is a metal salt solution that contains hydrofluoric acid.

### Claim 6 (depends on 1)

The preparation process as set forth in claim 1, wherein the texturing step is carried out as follows: placing the silicon wafer into a solution of hydrofluoric acid that contains both an oxidant and a metal salt, so as to form the nanometer-level textured structure on surfaces of the silicon wafer.

### Claim 7 (depends on 4)

The preparation process as set forth in claim 4, wherein the metal ion concentration in the solution is higher than 6E-5 mol/L.

### Claim 8 (depends on 1)

The preparation process as set forth in claim 1, wherein between the texturing step and the PN junction forming step, there is a step of modification etching of the textured surface microstructure, and the specific procedure thereof is as follows: placing the silicon wafer with the textured surface into a chemical etching liquid for modification etching of the microstructure;
the chemical etching liquid is selected from the group consisting of NaOH solution, KOH solution, tetramethylammonium hydroxide (TMAH) solution or a mixed solution of an acidic oxidant and HF acid.

### Claim 9 (depends on 8)

The preparation process as set forth in claim 8, wherein either prior to or following the foregoing modification etching on the textured surface microstructure, a metal particle removing step needs to take place, and the specific procedure thereof is as follows: using an acidic liquid and then deionized water to wash the obtained silicon wafer, so as to remove the metal particles.

### Claim 10 (depends on 6)

The preparation process as set forth in claim 6, wherein the metal ion concentration in the solution is higher than 6E-5 mol/L.