# US 2017/0294521 A1 · Method for manufacturing a semiconductor device having a super junction mosfet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0294521 A1
- Document ID: US20170294521A1
- Status: Published application
- Kind: A1
- Application number: 15/627,434
- Filed: 2017-06-19
- Published: 2017-10-12
- Earliest claimed: 2013-09-18
- Assignees: Fuji Electric Co., Ltd.
- Applicants: Fuji Electric Co., Ltd.
- Inventors: Takahiro TAMURA; Yasuhiko ONISHI
- Web page: https://patentgrep.com/patent/US20170294521A1

## CPC

- H10D 30/025: {of vertical IGFETs (of VDMOS H10D30/0291; of vertical TFTs H10D30/0318)}
- H10D 8/041: {of multilayer diodes}
- H10D 8/50: PIN diodes
- H10D 12/032: {of vertical IGBTs}
- H10D 12/441: {Vertical IGBTs}
- H10D 30/0291: {of vertical DMOS [VDMOS] FETs}
- H10D 30/665: {having edge termination structures}
- H10D 62/10: Shapes, relative sizes or dispositions of the regions of the semiconductor bodies; Shapes of the semiconductor bodies
- H10D 62/111: {Multiple RESURF structures, e.g. double RESURF or 3D-RESURF structures}
- H10D 62/125: {Shapes of junctions between the regions}
- H10D 62/157: {Impurity concentrations or distributions}
- H10D 62/158: {Dispositions}
- H10D 62/393: {Body regions of DMOS transistors or IGBTs (cell layout of DMOS H10D62/127)}
- H10D 62/53: the imperfections being within the semiconductor body
- H10D 84/141: {VDMOS having built-in components}
- H10P 30/20: into semiconductor materials, e.g. for doping
- H10P 34/40: with high-energy radiation
- H10D 62/112: {for preventing surface leakage due to surface inversion layers, e.g. by using channel stoppers}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of manufacturing a super junction MOSFET, which includes a parallel pn layer including a plurality of pn junctions and in which an n-type drift region and a p-type partition region interposed between the pn junctions are alternately arranged and contact each other, a MOS gate structure on the surface of the parallel pn layer, and an n-type buffer layer in contact with an opposite main surface. The impurity concentration of the buffer layer is equal to or less than that of the n-type drift region. At least one of the p-type partition regions in the parallel pn layer is replaced with an n− region with a lower impurity concentration than the n-type drift region.

## Claims

### Claim 1

A method for manufacturing a semiconductor device including a high-concentration buffer layer of a first conductivity type which is provided on a first main surface of a drain layer of the first conductivity type and has a higher impurity concentration than a drift region of the first conductivity type, a low-concentration buffer layer of the first conductivity type which is provided on the high-concentration buffer layer and has a lower impurity concentration than the drift region, and a parallel pn layer which is provided on the low-concentration buffer layer and in which the drift region of the first conductivity type and a partition region of a second conductivity type are alternately arranged, at least one of the partition regions being replaced with a first-conductivity-type region having a lower impurity concentration than the drift region, the method comprising:
a step of adjusting a carrier lifetime of the parallel pn layer to be shorter than a carrier lifetime of the high-concentration buffer layer, using addition of heavy metal or irradiation with a charged particle.

### Claim 2

A method for manufacturing a semiconductor device including a parallel pn layer which is provided over a first main surface of a drain layer of a first conductivity type and in which a drift region of the first conductivity type and a partition region of a second conductivity type are alternately arranged, at least one of the partition regions being replaced with a first-conductivity-type region having a lower impurity concentration than the drift region, the method comprising:
a step of forming a high-concentration buffer layer of the first conductivity type, which has a higher impurity concentration than the drift region, on the first main surface of the drain layer;
a step of forming a low-concentration buffer layer of the first conductivity type, which has a lower impurity concentration than the drift region, on the high-concentration buffer layer;
a step of forming the parallel pn layer on the low-concentration buffer layer; and
a step of adding heavy metal or radiating a charged particle to the parallel pn layer such that a carrier lifetime of the parallel pn layer is shorter than a carrier lifetime of the high-concentration buffer layer.

### Claim 3

A method for manufacturing a semiconductor device including a parallel pn layer which is provided over a first main surface of a drain layer of a first conductivity type and in which a drift region of the first conductivity type and a partition region of a second conductivity type are alternately arranged, at least one of the partition regions being replaced with a first-conductivity-type region having a lower impurity concentration than the drift region, the method comprising:
a step of forming the parallel pn layer on a front surface side of a semiconductor substrate;
a step of forming an element structure on the parallel pn layer on the front surface side of the semiconductor substrate;
a step of forming a low-concentration buffer layer of the first conductivity type, which has a lower impurity concentration than the drift region, on a rear surface side of the semiconductor substrate;
a step of forming a high-concentration buffer layer of the first conductivity type, which has a higher impurity concentration than the drift region, at a position that is shallower than the low-concentration buffer layer from a rear surface of the semiconductor substrate; and
a step of adding heavy metal or radiating a charged particle to the high-concentration buffer layer such that a carrier lifetime of the parallel pn layer is shorter than a carrier lifetime of the high-concentration buffer layer.