# US 2017/0294473 A1 · Image sensing device and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0294473 A1
- Document ID: US20170294473A1
- Status: Published application
- Kind: A1
- Application number: 15/624,055
- Filed: 2017-06-15
- Published: 2017-10-12
- Earliest claimed: 2015-04-17
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company Ltd.
- Inventors: CHIH-CHANG HUANG; CHI-MING LU; JIAN-MING CHEN; JUNG-CHIH TSAO; YAO-HSIANG LIANG
- Web page: https://patentgrep.com/patent/US20170294473A1

## CPC

- H10F 39/811: {Interconnections}
- H10F 39/014: {of CMOS image sensors}
- H10F 39/024: {of coatings or optical elements}
- H10F 39/028: {performed after manufacture of the image sensors, e.g. annealing, gettering of impurities, short-circuit elimination or recrystallisation}
- H10F 39/182: {Colour image sensors}
- H10F 39/199: {Back-illuminated image sensors}
- H10F 39/8037: {the integrated elements comprising a transistor}
- H10F 39/8053: {Colour filters}
- H10F 39/8057: {Optical shielding}
- H10F 39/806: {Optical elements or arrangements associated with the image sensors}
- H10F 39/8063: {Microlenses}
- H10F 39/807: {Pixel isolation structures}
- H10W 20/033: {in openings in dielectrics}
- H10W 20/048: {by using plasmas or gaseous environments, e.g. by nitriding}
- H10W 20/066: {by forming silicides of refractory metals}
- H10W 20/081: {by forming openings in the dielectric parts}
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Some embodiments of the present disclosure provide a back side illuminated. (BSI) image sensor. The back side illuminated (BSI) image sensor includes a semiconductive substrate and an interlayer dielectric (ILD) layer at a front side of the semiconductive substrate. The ILD layer includes a dielectric layer over the semiconductive substrate and a contact partially buried inside the semiconductive substrate. The contact includes a silicide layer including a predetermined thickness proximately in a range from about 600 angstroms to about 1200 angstroms.

## Claims

### Claim 1

A method of manufacturing a back side illuminated (BSI) image sensor, comprising:
receiving a semiconductive substrate;
forming a dielectric layer on a front side of the semiconductive substrate;
forming a recess in the dielectric layer such to expose the front side;
forming a titanium layer inside the recess and on the front side of the semiconductive substrate by using a plasma ignition power in a predetermined range from about 600 watts to 900 watts;
performing a first thermal anneal;
performing a second thermal anneal; and
forming a barrier layer inside the recess.

### Claim 2 (depends on 1)

The method of claim 1, wherein the forming the titanium layer comprises using a first plasma power maintained substantially constant at a first predetermined range lesser than half of the predetermined range.

### Claim 3 (depends on 2)

The method of claim 2, wherein the forming the titanium layer comprises using a second plasma power maintained substantially constant at a second predetermined range proximately double the first predetermined range but lower than the predetermined range.

### Claim 4 (depends on 1)

The method of claim 1, wherein the performing the second thermal anneal comprises forming a silicide layer comprising a predetermined thickness proximately in a range from about 600 angstroms to about 1200 angstroms.

### Claim 5 (depends on 1)

The method of claim 1, further comprising removing an unreacted titanium between the first thermal anneal and the second thermal anneal.

### Claim 6 (depends on 1)

The method of claim 1, wherein the performing the second thermal anneal comprises forming a silicide layer comprising a lattice structure, and the lattice structure comprising a {220} plane or a {311} plane configured to be measured with peaks on an X-ray diffraction pattern of the lattice structure.

### Claim 7

A method of manufacturing a back side illuminated (BSI) image sensor, comprising:
receiving a semiconductive substrate;
forming a dielectric layer on a front side of the semiconductive substrate;
forming a recess in the dielectric layer to expose the front side;
forming a titanium layer inside the recess and on the front side of the semiconductive substrate by using a plasma ignition power in a predetermined range;
performing a first thermal anneal; and
performing a second thermal anneal to form a silicide layer comprising a lattice structure, and the lattice structure comprising a {220} plane configured to be measured with peaks on an X-ray diffraction pattern of the lattice structure.

### Claim 8 (depends on 7)

The method of claim 7, wherein the receiving the semiconductive substrate comprises receiving the semiconductive substrate including a non-silicide portion.

### Claim 9 (depends on 7)

The method of claim 7, wherein the forming the titanium layer comprises using a first plasma power maintained substantially constant at a first predetermined range lesser than half of the predetermined range.

### Claim 10 (depends on 8)

The method of claim 8, wherein the forming the titanium layer comprises using a second plasma power maintained substantially constant at a second predetermined range proximately double the first predetermined range but lower than the predetermined range.

### Claim 11 (depends on 8)

The method of claim 8, wherein the performing the first thermal anneal comprises causing the titanium layer in a bottom portion of the recess to react with the non-silicide portion in the semiconductive substrate to form a silicide layer.

### Claim 12 (depends on 7)

The method of claim 7, wherein the performing the second thermal anneal comprises forming a silicide layer comprising a predetermined thickness proximately in a range from about 600 angstroms to about 1200 angstroms.

### Claim 13 (depends on 7)

The method of claim 7, further comprising removing an unreacted titanium between the first thermal anneal and the second thermal anneal.

### Claim 14

A method of manufacturing a back side illuminated (BSI) image sensor, comprising:
receiving a semiconductive substrate including a non-silicide portion;
forming a dielectric layer on a front side of the semiconductive substrate;
forming a recess in the dielectric layer to expose the front side;
forming a titanium layer inside the recess and on the front side of the semiconductive substrate by using a plasma ignition power in a predetermined range;
performing a first thermal anneal to cause the titanium layer in a bottom portion of the recess to react with the non-silicide portion in the semiconductive substrate to form a silicide layer having a crystallographic structure of C49; and
performing a second thermal anneal to change the crystallographic structure of the silicide layer from C49 to C54.

### Claim 15 (depends on 14)

The method of claim 14, wherein the forming the titanium layer comprises using a first plasma power maintained substantially constant at a first predetermined range lesser than half of the predetermined range.

### Claim 16 (depends on 15)

The method of claim 15, wherein the forming the titanium layer comprises using a second plasma power maintained substantially constant at a second predetermined range proximately double the first predetermined range but lower than the predetermined range.

### Claim 17 (depends on 14)

The method of claim 14, wherein the performing the second thermal anneal comprises forming the silicide layer comprising a predetermined thickness proximately in a range from about 600 angstroms to about 1200 angstroms.

### Claim 18 (depends on 14)

The method of claim 14, further comprising removing an unreacted titanium between the first thermal anneal and the second thermal anneal.

### Claim 19 (depends on 14)

The method of claim 14, wherein the performing the second thermal anneal comprises forming the silicide layer having a lattice structure, including a {220} plane configured to be measured with a peak on an X-ray diffraction pattern of the lattice structure,

### Claim 20 (depends on 14)

The method of claim 14, wherein the performing the second thermal anneal comprises forming the silicide layer having a lattice structure, including a {311} plane configured to be measured with a peak on an X-ray diffraction pattern of the lattice structure.