# US 2017/0294343 A1 · Etching method and fabrication method of semiconductor structures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0294343 A1
- Document ID: US20170294343A1
- Status: Published application
- Kind: A1
- Application number: 15/475,413
- Filed: 2017-03-31
- Published: 2017-10-12
- Earliest claimed: 2016-04-07
- Assignees: Semiconductor Manufacturing International (Shanghai) Corporation; Semiconductor Manufacturing International (Beijing) Corporation
- Applicants: Semiconductor Manufacturing International (Shanghai) Corporation; Semiconductor Manufacturing International (Beijing) Corporation
- Inventors: Min Da HU; Er Hu ZHENG; Cheng Long ZHANG; Hai Yang ZHANG
- Web page: https://patentgrep.com/patent/US20170294343A1

## CPC

- H10W 20/076: {in via holes or trenches}
- H10D 64/021: {using multiple gate spacer layers, e.g. bilayered sidewall spacers}
- H10P 50/283: {by chemical means}
- H10W 20/069: {by forming self-aligned vias or self-aligned contact plugs}
- H10W 20/081: {by forming openings in the dielectric parts}
- H10W 20/0765: {the thin functional dielectric layers being temporary, e.g. sacrificial layers}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

An etching method and a fabrication method of semiconductor structures are provided. The etching method includes forming trenches in a to-be-etched structure, and forming a dielectric layer in the trenches. The etching method further includes etching the dielectric layer in the trenches by an etching process, and controlling at least an etching temperature of the etching process while a polymer is formed on side surface of the to-be-etched structure. During the etching process of the dielectric layer, the polymer undergoes a deposition stage and a removal stage. The deposition stage has a deposition rate of the polymer greater than an etch rate of the polymer, and the removal stage has the deposition rate of the polymer less than the etch rate of the polymer.

## Claims

### Claim 1

An etching method, comprising:
forming trenches in a to-be-etched structure;
forming a dielectric layer in the trenches;
etching the dielectric layer in the trenches by an etching process; and
controlling at least an etching temperature of the etching process while a polymer is formed on side surface of the to-be-etched structure,
wherein during the etching process of the dielectric layer, the polymer undergoes:
a deposition stage, having a deposition rate of the polymer greater than an etch rate of the polymer; and
a removal stage, having the deposition rate less than the etch rate.

### Claim 1 (depends on 10)

The fabrication method according to claim 10, wherein:
a duration of one etching circle is longer than 10 seconds.

### Claim 2 (depends on 1)

The etching method according to claim 1, wherein:
the etching stage and the deposition stage of the polymer form an etching circle, and the etching process of the dielectric layer includes one or more etching circles.

### Claim 3 (depends on 1)

The etching method according to claim 1, wherein:
a relationship between an etching temperature T and an etching time t is;
T=T0+T1sin (2πt/t0)
wherein T0 is an equilibrium temperature, T1 is a maximum value of the etching temperature deviating from the equilibrium temperature T0, and t0 is a duration of an etching circle.

### Claim 4 (depends on 3)

The etching method according to claim 3, wherein:
a duration of one etching circle is longer than 10 seconds.

### Claim 5 (depends on 3)

The etching method according to claim 3, wherein:
the maximum value of the etching temperature deviating from the equilibrium temperature is greater than 30° C.

### Claim 6 (depends on 3)

The etching method according to claim 3, wherein:
the equilibrium temperature is in a range of approximately 60° C.˜80° C.

### Claim 7 (depends on 1)

The etching method according to claim 1, wherein:
the etching process of the dielectric layer includes an anisotropic dry etching.

### Claim 8

A fabrication method for semiconductor structures, comprising:
forming a plurality of device structures on a substrate,
forming sidewall spacers on side surfaces of each device structure to provide trenches on the substrate between sidewall spacers of adjacent device structures;
forming a dielectric layer in the trenches;
etching the dielectric layer in the trenches by an etching process; and
controlling at least an etching temperature of the etching process while a polymer is formed on side surface of the to-be-etched structure,
wherein during the etching process of the dielectric layer, the polymer undergoes:
a deposition stage, having a deposition rate of the polymer greater than an etch rate of the polymer; and
a removal stage, having the, deposition rate less than the etch rate.

### Claim 9 (depends on 8)

The fabrication method according to claim 8, wherein:
the etching stage and the deposition stage of the polymer form an etching circle. and the etching process of the dielectric layer includes one or more etching circles.

### Claim 10 (depends on 8)

The fabrication method according to claim 8, wherein;
the relationship between the etching temperature T and an etching time t is:
T=T0+T1sin (2πt/t0)
wherein T0 is an equilibrium temperature, T1 is a maximum value of the etching temperature deviating from the equilibrium temperature T0 and t0 is a duration of an etching: circle.

### Claim 12 (depends on 10)

The fabrication method according to claim 10, wherein:
the maximum value of the etching temperature deviating from the equilibrium temperature is greater than 30′ C.

### Claim 13 (depends on 10)

The fabrication method according to claim 10, wherein:
the equilibrium temperature is in a range of approximately 60° C.˜80° C.

### Claim 14 (depends on 8)

The fabrication method according to claim 8, wherein:
the device structures include gate electrode structures, and the fabrication method further includes:
forming a source region and a drain region on two sides of each gate electrode structure on the substrate.

### Claim 15 (depends on 14)

The fabrication method according to claim 14, wherein:
the steps of etching the dielectric layer in the trenches includes etching the dielectric layer till the source region or the drain region is exposed, and forming contact holes; and
the fabrication method further includes: forming plugs in the contact holes.

### Claim 16 (depends on 8)

The fabrication method according to claim 8, wherein:
a temperature at which the deposition rate of the polymer is equal to the etch rate of the polymer is an equilibrium temperature,
the etching temperature for etching the dielectric layer includes a first temperature higher than the equilibrium temperature and a second temperature lower than the equilibrium temperature,
the etching temperature of the dielectric layer in the removal stage of the polymer is the first temperature, and
the etching temperature of the dielectric layer in the deposition stage of the polymer is the second temperature.

### Claim 17 (depends on 8)

The fabrication method according to claim 8, wherein:
an etching gas for etching the dielectric layer includes one or more gases selected from CF4, C3F8, and C4F8.

### Claim 18 (depends on 8)

The fabrication method according to claim 8, wherein:
an aspect ratio of the trenches is greater than 7:1.

### Claim 19 (depends on 8)

The fabrication method according to claim 8, wherein:
the trench has a width of less than 25 nm.

### Claim 20 (depends on 8)

The fabrication method according to claim 8, wherein:
the sidewall spacers are formed of a material including silicon nitride, and
the dielectric layer is formed of a material including silicon oxide.