# US 2017/0294331 A1 · Corrosion-resistant member, member for electrostatic chuck, and process for producing corrosion-resistant member

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0294331 A1
- Document ID: US20170294331A1
- Status: Published application
- Kind: A1
- Application number: 15/513,107
- Filed: 2015-08-25
- Published: 2017-10-12
- Earliest claimed: 2014-09-29
- Assignees: Sumitomo Osaka Cement Co., Ltd.
- Applicants: Sumitomo Osaka Cement Co., Ltd.
- Inventors: Megumi OOTOMO; Kentaro TAKAHASHI; Nobuhiro HIDAKA; Hironori KUGIMOTO
- Web page: https://patentgrep.com/patent/US20170294331A1

## CPC

- H10P 72/722: {Details of electrostatic chucks}
- C04B 35/44: based on aluminates
- C04B 35/6263: {characterised by their solids loadings, i.e. the percentage of solids}
- C04B 35/62655: {Drying, e.g. freeze-drying, spray-drying, microwave or supercritical drying}
- C04B 35/638: Removal thereof
- C04B 35/645: Pressure sintering
- C04B 35/6455: {Hot isostatic pressing}
- C04B 2235/3217: Aluminum oxide or oxide forming salts thereof, e.g. bauxite, alpha-alumina
- C04B 2235/3224: Rare earth oxide or oxide forming salts thereof, e.g. scandium oxide
- C04B 2235/5445: submicron sized, i.e. from 0,1 to 1 micron
- C04B 2235/662: Annealing after sintering
- C04B 2235/761: Unit-cell parameters, e.g. lattice constants
- C04B 2235/77: Density
- C04B 2235/96: Properties of ceramic products, e.g. mechanical properties such as strength, toughness, wear resistance
- C04B 2235/9692: Acid, alkali or halogen resistance
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

Provided are a corrosion-resistant member in which, in a case where the corrosion-resistant member is used as a member for an electrostatic chuck, an adsorption force of the electrostatic chuck can be made to be strong when an electric field is applied and a residual adsorption force of the electrostatic chuck can be made to be weak when the application of the electric field is stopped; a member for an electrostatic chuck; and a process for producing a corrosion-resistant member. The corrosion-resistant member includes an oxide which includes samarium and aluminum and has a perovskite type structure. The member for an electrostatic chuck includes the corrosion-resistant member according to the present invention. The process for producing a corrosion-resistant member according to the present invention includes: a step of mixing aluminum oxide powder and samarium oxide powder with a solvent to prepare a slurry including the aluminum oxide powder and the samarium oxide powder; a step of drying the slurry to prepare a mixed powder including the aluminum powder and the samarium oxide powder, and molding the mixed powder to prepare a green body; and a step of calcinating the green body to prepare a sintered body.

## Claims

### Claim 1

A corrosion-resistant member comprising
an oxide which includes samarium and aluminum and has a perovskite type structure.

### Claim 2 (depends on 1)

The corrosion-resistant member according to claim 1,
wherein a proportion of the oxide in the corrosion-resistant member is 80 vol % or higher.

### Claim 3 (depends on 1)

The corrosion-resistant member according to claim 1,
wherein a range of samarium:aluminum (molar ratio) in the oxide is 73:27 to 9:91.

### Claim 4 (depends on 1)

The corrosion-resistant member according to claim 1, having a residual adsorption force of 0.1 to 0.9 kPa,
wherein a voltage of 2.0 kV is applied to the corrosion-resistant member having a thickness of 1 mm for 60 seconds in an atmosphere in which a pressure is lower than 0.5 Pa, a 1-inch silicon wafer is adsorbed on the corrosion-resistant member, an application of the voltage is stopped, and then the residual adsorption force is measured.

### Claim 5 (depends on 1)

A member for an electrostatic chuck comprising
the corrosion-resistant member according to claim 1.

### Claim 6

A process for producing a corrosion-resistant member, the process comprising:
a step of mixing aluminum oxide powder and samarium oxide powder with a solvent to prepare a slurry including the aluminum oxide powder and the samarium oxide powder;
a step of drying the slurry to prepare a mixed powder including the aluminum powder and the samarium oxide powder, and molding the mixed powder to prepare a green body; and
a step of calcinating the green body to prepare a sintered body.

### Claim 7 (depends on 6)

The process for producing a corrosion-resistant member according to claim 6, further comprising
a step of annealing the sintered body.