# US 2017/0294315 A1 · Semiconductor structure and fabrication method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0294315 A1
- Document ID: US20170294315A1
- Status: Published application
- Kind: A1
- Application number: 15/476,249
- Filed: 2017-03-31
- Published: 2017-10-12
- Earliest claimed: 2016-04-07
- Assignees: Semiconductor Manufacturing International (Shanghai) Corporation; Semiconductor Manufacturing International (Beijing) Corporation
- Applicants: Semiconductor Manufacturing International (Shanghai) Corporation; Semiconductor Manufacturing International (Beijing) Corporation
- Inventors: Wu Feng DENG
- Web page: https://patentgrep.com/patent/US20170294315A1

## CPC

- H10D 64/01326: {Aspects related to lithography, isolation or planarisation of the conductor}
- H10D 64/01318: {the conductor comprising a layer of alloy material, compound material or organic material contacting the insulator, e.g. TiN (comprising a layer of alloys of Si, Ge or C H10D64/01314)}
- H10D 64/667: {the conductor comprising a layer of alloy material, compound material or organic material contacting the insulator, e.g. TiN workfunction layers (having lateral variation H10D64/671)}
- H10P 14/44: Physical vapour deposition [PVD]
- H10P 52/403: {of conductive or resistive materials}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10W 20/062: {by smoothing of conductive parts, e.g. by planarisation}
- H10W 20/42: Vias, e.g. via plugs
- H10W 20/4405: {the principal metal being aluminium}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method is provided for fabricating a semiconductor structure. The method includes providing a substrate having a dielectric layer formed on the substrate, where an opening is formed in the dielectric layer, and bottom of the opening exposes surface of the substrate. The method also includes forming a first metal layer over of the dielectric layer, where a temperature for forming the first metal layer is a first temperature. In addition, the method includes forming a second metal layer filling the opening, where a temperature for forming the second metal layer is a second temperature, and the second temperature is higher than the first temperature. Further, the method includes planarizing the second metal layer and the first metal layer until the top surface of the dielectric layer is exposed.

## Claims

### Claim 1

A method for fabricating a semiconductor structure, comprising:
providing a substrate having a dielectric layer formed on the substrate, wherein an opening is formed in the dielectric layer, and bottom of the opening exposes surface of the substrate;
forming a first metal layer over the top of the dielectric layer, wherein a temperature for forming the first metal layer is a first temperature;
forming a second metal layer filling the opening, wherein a temperature for forming the second metal layer is a second temperature, and the second temperature is higher than the first temperature; and
planarizing the second metal layer and the first metal layer until the top surface of the dielectric layer is exposed.

### Claim 2 (depends on 1)

The method according to claim 1, wherein:
the first temperature is in a range of approximately 300-350° C.

### Claim 3 (depends on 1)

The method according to claim 1, wherein:
the second temperature is in a range of approximately 400-450° C.

### Claim 4 (depends on 1)

The method according to claim 1, wherein:
the first metal layer and the second metal layer are made of a same material.

### Claim 5 (depends on 1)

The method according to claim 1, wherein:
the first metal layer and the second metal layer are made of aluminum.

### Claim 6 (depends on 1)

The method according to claim 1, wherein:
a physical vapor deposition process is performed to form the first metal layer or the second metal layer.

### Claim 7 (depends on 1)

The method according to claim 1, wherein
a thickness of the first metal layer is larger than 300 Å.

### Claim 8 (depends on 1)

The method according to claim 1, wherein:
a thickness of the second metal layer is in a range of approximately 2000-5000 Å.

### Claim 9 (depends on 1)

The method according to claim 1, wherein:
the first metal layer is also formed over the bottom of the opening; and
the second metal layer is also formed over the dielectric layer.

### Claim 10 (depends on 1)

The method according to claim 1, wherein a planarization process includes:
performing a first planarization process to remove the second metal layer formed over the dielectric layer;
performing a second planarization process to remove the first metal layer formed over the dielectric layer until the top surface of the liner structure layer is exposed; and
performing a third planarization process until the top surface of the remaining second metal layer and the top surface of the dielectric layer are flush.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the first, planarization process also includes:
removing part of thickness of the first metal layer formed over the dielectric layer, such that the thickness of the first metal layer formed over the dielectric layer reaches a preset thickness.

### Claim 12 (depends on 11)

The method according to claim 11, wherein:
the preset thickness is in a range of approximately 300-1000 Å.

### Claim 13 (depends on 10)

The method according to claim 10, wherein one or more processes in the first planarization process, the second planarization process and the third planarization process include:
a chemical mechanical polishing process.

### Claim 14 (depends on 13)

The method according to claim 13, wherein, during the first planarization process performed by the chemical mechanical polishing process:
pressure is larger than 1.5 Pa; and
a hardness of the polishing pad is in a range of approximately 80-100 MPa.

### Claim 15 (depends on 13)

The method according to claim 13, wherein, during the second planarization process performed by the chemical mechanical polishing process:
a pressure is in a range of approximately 1-2 Pa; and
a hardness of the polishing pad is in a range of approximately 20-40 MPa.

### Claim 16 (depends on 13)

The method according to claim 13, wherein, during the third planarization process performed by the chemical mechanical polishing process:
a pressure is in a range of approximately 1-2 Pa; and
a hardness of the polishing pad is in a range of approximately 20-40 MPa.

### Claim 17 (depends on 1)

The method according to claim 1, after providing the substrate and before forming the first metal layer, further including:
forming a liner structure layer over the bottom and side surfaces of the opening.

### Claim 18 (depends on 17)

The method according to claim 17, wherein, along a direction away from the substrate, the liner structure layer sequentially includes:
a barrier layer;
a work fUnction layer; and
an adhesive layer.

### Claim 19 (depends on 18)

The method according to claim 18, wherein:
the barrier layer includes a tantalum nitride layer;
the work function layer includes a titanium aluminum layer, an aluminum nitride layer, and a titanium layer sequentially formed on the barrier layer; and
the adhesive layer is made of the same material as the first metal layer.

### Claim 20 (depends on 1)

The method according to claim 1, after providing the substrate and before forming the first metal layer, further including:
the semiconductor structure is a metal gate structure; and
forming a gate dielec tric layer covering the bottom of the opening.