# US 2017/0294306 A1 · Formation of a layer on a semiconductor substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0294306 A1
- Document ID: US20170294306A1
- Status: Published application
- Kind: A1
- Application number: 15/093,003
- Filed: 2016-04-07
- Published: 2017-10-12
- Earliest claimed: 2016-04-07
- Assignees: Aixtron SE
- Applicants: Aixtron SE
- Inventors: Maxim Kelman; Zhongyuan Jia; Somnath Nag; Robert Ditizio
- Web page: https://patentgrep.com/patent/US20170294306A1

## CPC

- H10P 14/20: of semiconductor materials
- C23C 16/50: using electric discharges {(generation and control of plasma in discharge tubes for surface treatment H01J37/32, H01J37/34)}
- C23C 16/52: Controlling or regulating the coating process {(C23C16/45557, C23C16/279 take precedence)}
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/3414: {being group IIIA-VIA materials}
- H10P 14/36: {characterised by treatments done before the formation of the materials}
- H10P 14/3602: {In-situ cleaning}
- H10P 14/3822: {Controlling the interface between substrate and epitaxial layer, e.g. by ion implantation followed by annealing}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Described herein are techniques for forming an epitaxial III-V layer on a substrate. In a pre-clean chamber, a native oxygen layer may be replaced with a passivation layer by treating the substrate with a hydrogen plasma (or products of a plasma decomposition). In a deposition chamber, the temperature of the substrate may be elevated to a temperature less than 700° C. While the substrate temperature is elevated, a group V precursor may be flowed into the deposition chamber in order to transform the hydrogen terminated (Si—H) surface of the passivation layer into an Arsenic terminated (Si—As) surface. After the substrate has been cooled, a group III precursor and the group V precursor may be flowed in order to form a nucleation layer. Finally, at an elevated temperature, the group III precursor and group V precursor may be flowed in order to form a bulk III-V layer.

## Claims

### Claim 1

A method for growing an epitaxial III-V layer on a substrate, the method comprising:
in a pre-clean chamber, and while the substrate is at a first temperature, T1, exposing the substrate to a plasma, products of plasma decomposition, or both the plasma and the products of plasma decomposition so as to remove native oxide from the substrate and form a passivation layer on the substrate, wherein T1 is greater than room temperature;
in an oxygen-free environment, (a) transferring the substrate from the pre-clean chamber to a deposition chamber, and (b) cooling the substrate from T1 to a second temperature, T2; and
in the deposition chamber, (a) heating the substrate from T2 to a third temperature, T3, so as to remove the passivation layer on the substrate, and (b) growing the epitaxial III-V layer on the substrate, wherein 50° C.<T3<700° C.

### Claim 2 (depends on 1)

The method of claim 1, wherein growing the epitaxial III-V layer on the substrate comprises sequentially performing the following steps in the deposition chamber:
(i) cooling the substrate from T3 to a fourth temperature, T4;
(ii) when the substrate is at T4, starting a flow of a group III precursor so as to deposit a III-V nucleation layer on the substrate;
(iii) stopping the flow of the group III precursor;
(iv) heating the substrate to a fifth temperature, T5;
(v) when the substrate is at T5, re-starting the flow of the group III precursor so as to deposit a bulk III-V layer over the III-V nucleation layer;
(vi) stopping the flow of the group III precursor; and
(vii) cooling the substrate from T5 to a sixth temperature, T6.

### Claim 3 (depends on 2)

The method of claim 2, further comprising flowing a group V precursor into the deposition chamber, wherein the flow of the group V precursor starts prior to heating the substrate from T2 to T3, and ends after cooling the substrate to T6.

### Claim 4 (depends on 2)

The method of claim 2, further comprising flowing a group V precursor into the deposition chamber, wherein the flow of the group V precursor starts while heating the substrate from T2 to T3, and ends after cooling the substrate to T6.

### Claim 5 (depends on 2)

The method of claim 2, further comprising flowing a group V precursor into the deposition chamber, wherein the flow of the group V precursor starts before cooling the substrate from T3 to T4, and ends after cooling the substrate to T6.

### Claim 6 (depends on 2)

The method of claim 2, further comprising flowing a group V precursor into the deposition chamber, wherein the flow of the group V precursor starts while cooling the substrate from T3 to T4, and ends after cooling the substrate to T6.

### Claim 7 (depends on 1)

The method of claim 1, further comprising depositing an additional layer over the bulk III-V layer.

### Claim 8 (depends on 1)

The method of claim 1, wherein the oxygen-free environment is located in a transfer module.

### Claim 9 (depends on 1)

The method of claim 1, wherein the substrate is a Silicon wafer.

### Claim 10 (depends on 1)

The method of claim 1, wherein 400° C.<T1<650° C.

### Claim 11 (depends on 1)

The method of claim 1, wherein the plasma is a hydrogen gas (H2) plasma.

### Claim 12 (depends on 11)

The method of claim 11, wherein an area of a region where the H2 plasma is formed is substantially equal to an area of a top surface of the substrate.

### Claim 13 (depends on 1)

The method of claim 1, wherein the passivation layer comprises a hydrogen terminated (Si—H) surface.

### Claim 14 (depends on 13)

The method of claim 13, wherein removing the passivation layer comprises transforming the hydrogen terminated (Si—H) surface into an Arsenic terminated (Si—As) surface.

### Claim 15 (depends on 2)

The method of claim 2, wherein the flow of the group III precursor is stopped in step (iii), while the substrate temperature is less than T4.

### Claim 16 (depends on 1)

The method of claim 1, wherein the substrate temperature is always maintained below 700° C. in the deposition chamber.

### Claim at position 17

17-18. (canceled)