# US 2017/0294254 A1 · Amorphous soft magnetic alloy and inductance component using the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0294254 A1
- Document ID: US20170294254A1
- Status: Published application
- Kind: A1
- Application number: 15/626,810
- Filed: 2017-06-19
- Published: 2017-10-12
- Earliest claimed: 2006-02-02
- Assignees: Tokin Corporation; Tohoku University
- Applicants: Tokin Corporation; Tohoku University
- Inventors: Akiri URATA; Teruhiko FUJIWARA; Hiroyuki MATSUMOTO; Yasunobu YAMADA; Akihisa INOUE
- Web page: https://patentgrep.com/patent/US20170294254A1

## CPC

- H01F 1/153: Amorphous metallic alloys, e.g. glassy metals {(making ferrous amorphous alloys C22C33/003)}
- B22F 9/002: {amorphous or microcrystalline}
- C22C 33/003: {making amorphous alloys}
- C22C 33/0207: {Using a mixture of pre-alloyed powders or a master alloy}
- C22C 33/0257: {characterised by the range of the alloying elements}
- C22C 45/02: with iron as the major constituent
- H01F 1/15308: {based on Fe/Ni (H01F1/15325 takes precedence)}
- H01F 41/0226: {from amorphous ribbons}
- H01F 41/0246: {Manufacturing of magnetic circuits by moulding or by pressing powder (magnetic cores made by moulding or by pressing powder H01F27/255; soft magnetic particles H01F1/20, H01F1/36)}
- B22F 2003/248: {Thermal after-treatment}
- B22F 2998/00: Supplementary information concerning processes or compositions relating to powder metallurgy
- B22F 2998/10: Processes characterised by the sequence of their steps
- C22C 28/00: Alloys based on a metal not provided for in groups C22C5/00 - C22C27/00
- H01F 1/15375: {using polymers}
- H01F 3/14: Constrictions; Gaps, e.g. air-gaps (in magnetic shunt paths H01F3/12)
- H01F 17/062: {Toroidal core with turns of coil around it}
- H01F 2017/048: {with encapsulating core, e.g. made of resin and magnetic powder}
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

An amorphous soft magnetic alloy of the formula (Fe1-αTMα)100-w-x-y-zPwBxLySiz TipCqMnrCus, wherein TM is Co or Ni; L is Al, Cr, Zr, Mo or Nb; 0≦α≦0.3, 2≦w≦18 at %, 2≦x≦18 at %, 15≦w+x≦23 at %, 1<y≦5 at %, 0≦z≦4 at %; p, q, r, and s represents an addition ratio such that the total mass of Fe, TM, P, B, L and Si is 100, and 0≦p≦0.3, 0≦q≦0.5, 0≦r≦2, 0≦s≦1 and r+s>0; the composition fulfills one of the following conditions: L is Cr, Zr, Mo or Nb; or L is a combination of Al and Cr, Zr, Mo or Nb, wherein 0<Al≦5 at %, 1≦Cr≦4 at %, 0<Zr≦5 at %, 2≦Mo≦5 at %, and 2≦Nb≦5 at %; the alloy has a crystallization start temperature (Tx) which is 550° C. or less, a glass transition temperature (Tg) which is 520° C. or less, and a supercooled liquid region represented by ΔTx=Tx−Tg, which is 20° C. or more.

## Claims

### Claim 1

An amorphous soft magnetic alloy comprising a composition expressed by a formula of (Fe1-αTMα)100-w-x-y-zPwBxLySizTipCqMnrCus, wherein unavoidable impurities are contained, TM is at least one element selected from the group consisting of Co and Ni, L is at least one element selected from the group consisting of Al, Cr, Zr, Mo, and Nb, wherein 0≦α≦0.3, 2≦w≦18 at %, 2≦x≦18 at %, 15≦w+x≦23 at %, 1<y≦5 at %, 0≦z≦4 at %, and p, q, r, and s each represents an addition ratio such that the total mass of Fe, TM, P, B, L and Si is 100, and are defined as 0≦p≦0.3, 0≦q≦0.5, 0≦r≦2, 0≦s≦1 and r+s>0, and said composition fulfills one of the following conditions (A) and (B):
(A) L is at least one element selected from the group consisting of Cr, Zr, Mo and Nb; and
(B) L is a combination of Al and at least one element selected from the group consisting of Cr, Zr, Mo and Nb, wherein 0<Al≦5 at %, 1≦Cr≦4 at %, 0<Zr≦5 at %, 2≦Mo≦5 at %, and 2≦Nb≦5 at %,
wherein said alloy has a crystallization start temperature (Tx) which is 550° C. or less, a glass transition temperature (Tg) which is 520° C. or less, and a supercooled liquid region represented by ΔTx=Tx−Tg, which is 20° C. or more.

### Claim 2 (depends on 1)

An amorphous soft magnetic alloy according to claim 1, wherein said alloy has a saturation magnetic flux density which is 1.2 T or more.

### Claim 3 (depends on 1)

An amorphous soft magnetic alloy according to claim 1, wherein said alloy has a Curie temperature which is 240° C. or more.

### Claim 4 (depends on 1)

An amorphous soft magnetic alloy member made of the amorphous soft magnetic alloy according to claim 1, wherein said amorphous soft magnetic alloy member has a thickness of 0.5 mm or more and a cross-sectional area of 0.15 mm2 or more.

### Claim 5 (depends on 1)

An amorphous soft magnetic alloy ribbon made of the amorphous soft magnetic alloy according to claim 1, wherein said amorphous soft magnetic alloy ribbon has a thickness of 1 to 200 μm.

### Claim 6 (depends on 5)

An amorphous soft magnetic alloy ribbon according to claim 5, wherein said amorphous soft magnetic alloy ribbon has a magnetic permeability of 5000 or more at a frequency of 1 kHz.

### Claim 7 (depends on 1)

An amorphous soft magnetic alloy powder made of the amorphous soft magnetic alloy according to claim 1, wherein said amorphous soft magnetic alloy powder has a particle size of 200 μm or less (excluding zero).

### Claim 8 (depends on 7)

An amorphous soft magnetic alloy powder according to claim 7, wherein said amorphous soft magnetic alloy powder contains at least one of an amorphous soft magnetic alloy powder produced by water atomization and an amorphous soft magnetic alloy powder produced by gas atomization, and 50% or more in number of particles of the powder have a particle size greater than 3 μm.

### Claim 9 (depends on 7)

An amorphous soft magnetic alloy powder according to claim 7, wherein said amorphous soft magnetic alloy powder contains at least one of an amorphous soft magnetic alloy powder produced by water atomization and an amorphous soft magnetic alloy powder produced by gas atomization, is adapted to pass through a sieve having a mesh size of 250 μm, and has a particle size with a center diameter of 192 μm or less.

### Claim 10 (depends on 7)

An amorphous soft magnetic alloy powder according to claim 7, wherein said amorphous soft magnetic alloy powder contains at least one of an amorphous soft magnetic alloy powder produced by water atomization and an amorphous soft magnetic alloy powder produced by gas atomization, is adapted to pass through a sieve having a mesh size of 150 μm, and has a particle size with a center diameter of 96 μm or less.

### Claim 11 (depends on 7)

An amorphous soft magnetic alloy powder according to claim 7, wherein said amorphous soft magnetic alloy powder contains at least one of an amorphous soft magnetic alloy powder produced by water atomization and an amorphous soft magnetic alloy powder produced by gas atomization, is adapted to pass through a sieve having a mesh size of 45 μm, and has a particle size with a center diameter of 30 μm or less.

### Claim 12 (depends on 7)

An amorphous soft magnetic alloy powder according to claim 7, wherein said amorphous soft magnetic alloy powder contains at least one of an amorphous soft magnetic alloy powder produced by water atomization and an amorphous soft magnetic alloy powder produced by gas atomization, is adapted to pass through a sieve having a mesh size of 45 μm, and has a particle size with a center diameter of 20 μm or less.

### Claim 13 (depends on 7)

An amorphous soft magnetic alloy powder according to claim 7, wherein said amorphous soft magnetic alloy powder has an aspect ratio of about 1 to 2.

### Claim 14 (depends on 4)

A magnetic core formed by machining the amorphous soft magnetic alloy member according to claim 4.

### Claim 15 (depends on 5)

A magnetic core formed by annularly winding the amorphous soft magnetic alloy ribbon according to claim 5.

### Claim 16 (depends on 15)

A magnetic core according to claim 15, formed by annularly winding said amorphous soft magnetic alloy ribbon through an insulator.

### Claim 17 (depends on 5)

A magnetic core formed by laminating substantially same-shaped pieces of the amorphous soft magnetic alloy ribbon according to claim 5.

### Claim 18 (depends on 17)

A magnetic core according to claim 17, formed by laminating said substantially same-shaped pieces of said amorphous soft magnetic alloy ribbon through insulators interposed therebetween.

### Claim 19 (depends on 7)

A magnetic core formed by molding a mixture of a material powder comprising the amorphous soft magnetic alloy powder according to claim 7 and a binder added thereto in an amount of 10% or less by mass.

### Claim 20 (depends on 19)

A magnetic core according to claim 19, wherein a mixing ratio of said binder in said mixture is 5% or less by mass, a space factor of said material powder in said magnetic core is 70% or more, a magnetic flux density is 0.4 T or more in applying a magnetic field of 1.6×104 A/m, and a resistivity is 1 Ω·cm or more.

### Claim 21 (depends on 19)

A magnetic core according to claim 19, wherein a mixing ratio of said binder in said mixture is 3% or less by mass, a molding temperature is equal to or higher than a softening point of said binder, a space factor of said material powder in said magnetic core is 80% or more, a magnetic flux density is 0.6 T or more in applying a magnetic field of 1.6×104 A/m, and a resistivity is 0.1 Ω·cm or more.

### Claim 22 (depends on 19)

A magnetic core according to claim 19, wherein a mixing ratio of said binder in said mixture is 1% or less by mass, a molding temperature is in a supercooled liquid region of said amorphous soft magnetic alloy powder, a space factor of said material powder in said magnetic core is 90% or more, a magnetic flux density is 0.9 T or more in applying a magnetic field of 1.6×104 A/m, and a resistivity is 0.01 Ω·cm or more.

### Claim 23 (depends on 19)

A magnetic core according to claim 19, wherein said material powder contains a soft magnetic alloy powder in an amount of 5 to 50% by volume, said soft magnetic alloy powder having a smaller center particle size and a lower hardness as compared with said amorphous soft magnetic alloy powder.

### Claim 24 (depends on 14)

A magnetic core according to claim 14, wherein said magnetic core is formed by heat treatment in a temperature region equal to or higher than a Curie temperature and equal to or lower than a crystallization start temperature of said amorphous soft magnetic alloy.

### Claim 25 (depends on 14)

An inductance component formed by applying a coil with at least one turn to the magnetic core according to claim 14.

### Claim 26 (depends on 19)

An inductance component formed by integrally molding the magnetic core according to claim 19 and a coil, wherein said coil is formed by winding a linear conductor by at least one turn and is disposed in said magnetic core.

### Claim 27 (depends on 9)

An inductance component formed by applying a coil with at least one turn to a magnetic core formed by molding a mixture of a material powder comprised of the amorphous soft magnetic alloy powder according to claim 9 and a binder added thereto in an amount of 5% or less by mass, a space factor of said material powder in said magnetic core being 50% or more, wherein a peak value of Q(1/tan δ) of said inductance component in a frequency band of 10 kHz or more is 20 or more.

### Claim 28 (depends on 10)

An inductance component formed by applying a coil with at least one turn to a magnetic core formed by molding a mixture of a material powder comprised of the amorphous soft magnetic alloy powder according to claim 10 and a binder added thereto in an amount of 5% or less by mass, a space factor of said material powder in said magnetic core being 50% or more, wherein a peak value of Q(1/tan δ) of said inductance component in a frequency band of 100 kHz or more is 25 or more.

### Claim 29 (depends on 11)

An inductance component formed by applying a coil with at least one turn to a magnetic core formed by molding a mixture of a material powder comprised of the amorphous soft magnetic alloy powder according to claim 11 and a binder added thereto in an amount of 5% or less by mass, a space factor of said material powder in said magnetic core being 50% or more, wherein a peak value of Q(1/tan δ) of said inductance component in a frequency band of 500 kHz or more is 40 or more.

### Claim 30 (depends on 12)

An inductance component formed by applying a coil with at least one turn to a magnetic core formed by molding a mixture of a material powder comprising the amorphous soft magnetic alloy powder according to claim 12 and a binder added thereto in an amount of 5% or less by mass, a space factor of said material powder in said magnetic core being 50% or more, wherein a peak value of Q(1/tan δ) of said inductance component in a frequency band of 1 MHz or more is 50 or more.

### Claim 31 (depends on 27)

An inductance component according to claim 27, wherein said coil is formed by winding a linear conductor by at least one turn and is disposed in said magnetic core, and said magnetic core and said coil are integrally molded.

### Claim 32 (depends on 25)

An inductance component according to claim 25, wherein said magnetic core is formed with a gap.

### Claim 33 (depends on 25)

An inductance component according to claim 25, wherein said magnetic core is formed by heat treatment in a temperature region equal to or higher than a Curie temperature and equal to or lower than a crystallization start temperature of said amorphous soft magnetic alloy.

### Claim 34 (depends on 13)

An inductance component formed by applying a coil with at least one turn to a magnetic core formed by molding a mixture of a material powder comprised of the amorphous soft magnetic alloy powder according to claim 13 and a binder added thereto in an amount of 5% or less by mass, a space factor of said material powder in said magnetic core being 50% or more, wherein a peak value of Q(1/tan δ) of said inductance component in a frequency band of 10 kHz or more is 20 or more.

### Claim 35 (depends on 13)

An inductance component formed by applying a coil with at least one turn to a magnetic core formed by molding a mixture of a material powder comprised of the amorphous soft magnetic alloy powder according to claim 13 and a binder added thereto in an amount of 5% or less by mass, a space factor of said material powder in said magnetic core being 50% or more, wherein a peak value of Q(1/tan δ) of said inductance component in a frequency band of 100 kHz or more is 25 or more.

### Claim 36 (depends on 13)

An inductance component formed by applying a coil with at least one turn to a magnetic core formed by molding a mixture of a material powder comprised of the amorphous soft magnetic alloy powder according to claim 13 and a binder added thereto in an amount of 5% or less by mass, a space factor of said material powder in said magnetic core being 50% or more, wherein a peak value of Q(1/tan δ) of said inductance component in a frequency band of 500 kHz or more is 40 or more.

### Claim 37 (depends on 13)

An inductance component formed by applying a coil with at least one turn to a magnetic core formed by molding a mixture of a material powder comprising the amorphous soft magnetic alloy powder according to claim 13 and a binder added thereto in an amount of 5% or less by mass, a space factor of said material powder in said magnetic core being 50% or more, wherein a peak value of Q(1/tan δ) of said inductance component in a frequency band of 1 MHz or more is 50 or more.

### Claim 38 (depends on 34)

An inductance component according to claim 34, wherein said coil is formed by winding a linear conductor by at least one turn and is disposed in said magnetic core, and said magnetic core and said coil are integrally molded.