# US 2017/0294241 A1 · Corrosion reduction in a molten salt reactor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0294241 A1
- Document ID: US20170294241A1
- Status: Published application
- Kind: A1
- Application number: 15/342,513
- Filed: 2016-11-03
- Published: 2017-10-12
- Earliest claimed: 2015-11-05
- Assignees: Elysium Industries Limited
- Applicants: Elysium Industries Limited
- Inventors: Andrew McCall Dodson; Michael Simpson; William Wangard; Edward Pheil
- Web page: https://patentgrep.com/patent/US20170294241A1

## CPC

- C23F 13/16: Electrodes characterised by the combination of the structure and the material
- B01J 19/0013: {Controlling the temperature of the process}
- B01J 19/02: Apparatus characterised by being constructed of material selected for its chemically-resistant properties
- C23F 13/04: Controlling or regulating desired parameters
- C23F 13/14: Material for sacrificial anodes
- C23F 13/22: Monitoring arrangements therefor
- G21C 1/03: cooled by a coolant not essentially pressurised, e.g. pool-type reactors
- G21C 1/22: using liquid or gaseous fuel
- G21C 17/022: for monitoring liquid coolants or moderators
- G21C 19/31: for molten metals
- C23F 2201/00: Type of materials to be protected by cathodic protection
- C23F 2213/21: combining at least two types of anodic or cathodic protection
- Y02E 30/30: Nuclear fission reactors
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- G21C: NUCLEAR REACTORS (fusion reactors, hybrid fission-fusion reactors G21B; nuclear explosives G21J)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A molten salt reactor comprising a reactor vessel and a molten salt contained within the reactor vessel. There is a corrosion reduction unit configured to process the molten salt to maintain an oxidation reduction ratio, (E(o)/E(r)), in the molten salt at a substantially constant level, wherein E(o) is an element (E) at a higher oxidation state (o) and E(r) is the element (E) at a lower oxidation state (r).

## Claims

### Claim 1

A molten salt reactor comprising:
a reactor vessel
a molten salt contained within the reactor vessel; and
a corrosion reduction unit configured to process the molten salt to maintain an oxidation reduction ratio, (E(o)/E(r)), in the molten salt at a substantially constant level, wherein E(o) is an element (E) at a higher oxidation state (o) and E(r) is the element (E) at a lower oxidation state (r).

### Claim 2 (depends on 1)

The molten salt reactor of claim 1, wherein the oxidation reduction ratio (E(o)/E(r)) is at a level between 1/20 to 1/2000.

### Claim 3 (depends on 1)

The molten salt reactor of claim 1, wherein the corrosion reduction unit comprises:
a chamber having a first opening in communication with the reactor vessel through which the molten salt from the reaction vessel enters the chamber and a second opening through which the molten salt exits the chamber; and
a first electrode disposed within the chamber including a sacrificial material which comprises at least one type of actinide.

### Claim 4 (depends on 3)

The molten salt reactor of claim 3, wherein the corrosion reduction unit further comprises:
a second electrode disposed within the chamber that is electrically connected to the first electrode; and
a controller electrically connected to the first and second electrodes to control the potential difference between the first and second electrodes.

### Claim 5 (depends on 4)

The molten salt reactor of claim 4, wherein the corrosion reduction unit further comprises a reference electrode in the chamber to detect the potential difference between the first electrode and the molten salt.

### Claim 6 (depends on 5)

The molten salt reactor of claim 5, wherein the controller is configured to apply a potential difference between the first electrode and second electrode to maintain the oxidation reduction ratio, (E(o)/E(r)) in the molten salt at the substantially constant level.

### Claim 7 (depends on 6)

The molten salt reactor of claim 6, wherein corrosion reduction unit further includes an ammeter connected between the first electrode and the controller to detect a reaction rate of the sacrificial material; wherein the controller is configured compare the detected reaction rate to a target reaction rate and to apply the potential difference between the first electrode and the second electrode based on the comparison of the detected reaction rate to the target reaction rate.

### Claim 8 (depends on 3)

The molten salt reactor of claim 3, further comprising:
a first line interconnecting the reactor vessel to the first opening of the chamber; and
a second line interconnecting the second opening of the chamber to the reactor vessel.

### Claim 9 (depends on 8)

The molten salt reactor of claim 8, further including a pump to transport the molten salt from the reactor vessel to the chamber through the first line and from the chamber to the reactor vessel through the second line.

### Claim 10 (depends on 5)

The molten salt reactor of claim 5, wherein the chamber further comprises a third opening on a top surface of the chamber, the third opening is configured to enable insertion into and removal from the chamber of the first electrode and the reference electrode when replacement is required due to consumption of sacrificial material.

### Claim 11

A method reducing corrosion in a molten salt reactor comprising:
providing a reactor vessel;
providing a molten salt contained within the reactor vessel; and
processing the molten salt to maintain an oxidation reduction ratio, (E(o)/E(r)), in the molten salt at a substantially constant level, wherein E(o) is an element (E) at a higher oxidation state (o) and E(r) is the element (E) at a lower oxidation state (r).

### Claim 12 (depends on 11)

The method of claim 11, wherein the oxidation reduction ratio (E(o)/E(r)) is approximately 1/2000.

### Claim 13 (depends on 11)

The method of claim 11, further comprising:
providing a chamber having a first opening in communication with the reactor vessel through which the molten salt from the reaction vessel enters the chamber and a second opening through which the molten salt exits the chamber; and
disposing a first electrode within the chamber including a sacrificial material which comprises at least one type of actinide.

### Claim 14 (depends on 13)

The method of claim 13, further comprising:
disposing a second electrode within the chamber that is electrically connected to the first electrode; and
controlling the potential difference between the first and second electrodes.

### Claim 15 (depends on 14)

The method of claim 14, further comprising using a reference electrode in the chamber to detect the potential difference between the first electrode and the molten salt.

### Claim 16 (depends on 15)

The method of claim 15, wherein the step of controlling includes applying a potential difference between the first electrode and second electrode to maintain the oxidation reduction ratio, (E(o)/E(r)) in the molten salt at the substantially constant level.

### Claim 17 (depends on 16)

The method of claim 16, further including providing an ammeter connected between the first electrode and the controller to detect a reaction rate of the sacrificial material; and wherein the step of controlling includes comparing the detected reaction rate to a target reaction rate and applying the potential difference between the first electrode and the second electrode based on the comparison of the detected reaction rate to the target reaction rate.

### Claim 18 (depends on 13)

The method of claim 13, further comprising:
interconnecting the reactor vessel to the first opening of the chamber with a first line; and
interconnecting the second opening of the chamber to the reactor vessel with a second line.

### Claim 19 (depends on 18)

The method of claim 18, further including pumping the molten salt from the reactor vessel to the chamber through the first line and from the chamber to the reactor vessel through the second line.

### Claim 20 (depends on 15)

The method of claim 15, further comprising providing a third opening on a top surface of the chamber and removing from the chamber the first electrode and the reference electrode when replacement is required to due consumption of sacrificial material and inserting a replacement first electrode and a replacement reference electrode.