# US 2017/0293222 A1 · Increasing and controlling sensitivity of non-linear metallic thin-film resists

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0293222 A1
- Document ID: US20170293222A1
- Status: Published application
- Kind: A1
- Application number: 15/632,736
- Filed: 2017-06-26
- Published: 2017-10-12
- Earliest claimed: 2014-03-10
- Assignees: Nikon Research Corporation of America
- Applicants: Nikon Corporation
- Inventors: Shane R. Palmer
- Web page: https://patentgrep.com/patent/US20170293222A1

## CPC

- G03F 7/095: having more than one photosensitive layer (G03F7/075 takes precedence)
- G03F 7/0043: {Chalcogenides; Silicon, germanium, arsenic or derivatives thereof; Metals, oxides or alloys thereof (G03F7/0044 takes precedence)}
- G03F 7/091: {characterised by antireflection means or light filtering or absorbing means, e.g. anti-halation, contrast enhancement}
- G03F 7/094: {Multilayer resist systems, e.g. planarising layers}
- G03F 7/16: Coating processes; Apparatus therefor (applying coatings to base materials in general B05; applying photosensitive compositions to base for photographic purposes G03C1/74)
- G03F 7/2022: {Multi-step exposure, e.g. hybrid; backside exposure; blanket exposure, e.g. for image reversal; edge exposure, e.g. for edge bead removal; corrective exposure}
- G03F 7/2041: {in the presence of a fluid, e.g. immersion; using fluid cooling means}
- G03F 7/26: Processing photosensitive materials; Apparatus therefor (G03F7/12 - G03F7/24 take precedence)
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

Non-linear metallic thermal resist structure having more than two layers of different metals and effective eutectic temperature that is lower than eutectic temperature of a reference non-linear metallic thermal resist having only two layer of same different metals. Optionally, at least one the layers of such resist structure is doped with material different from host metals and/or deposited under conditions resulting in strain or stress in a layer at hand. Method of multi-exposure-based patterning of a substrate carrying such structure with laser pulses characterized by irradiance at levels equal to or below 10 mJ/cm2. The sequence of steps producing the required pattern on the substrate may be explicitly lacking a step of removal of a portion of the resist structure between two consecutive exposures.

## Claims

### Claim 1

A non-linear metallic thermal (NLMT) resist comprising:
a thin-film stack that includes at least three thin-film layers made of first and second different host materials,
wherein first and second layers of said stack that are in immediate contact with one another are made of the first and second different host materials, respectively, while a third layer that is separated from the first layer by the second layer and is in immediate contact with the second layer is made of the first host material;
species in at least one of said at least three thin-films layers, said species being different from any of the first and second host materials;
said thin-film stack configured to form an alloy of said first and second host materials in response to being irradiated with pre-determined radiation;
said thin-film stack characterized by a curve that represents a rate of absorbance of said incident radiation as a function of depth of the thin-film stack, said depth being measured from a surface of the thin-film stack on which said pre-determined radiation is incident;
said curve having a positive slope in each segment thereof, different segments of said curve representing absorption of said pre-determined radiation in a corresponding one of said at least three thin-film layers.

### Claim 2 (depends on 1)

The NLMT resist according to claim 1, wherein a thickness of each constituent layer of the thin-film stack is less than 5 nm.

### Claim 3 (depends on 1)

The NLMT resist according to claim 1, wherein said species includes metallic or semiconductor species chosen to define defects, in said at least one of the at least three thin-film layers, said defects containing a gaseous element.

### Claim 4 (depends on 1)

The NLMT resist according to claim 1, wherein said first and second host materials include In ad Bi, respectively, and wherein said species include any of Pb, Sn, Ga, Si, Ge, Hg, Zr, and Ti.

### Claim 5 (depends on 1)

The NLMT resist according to claim 1, wherein said species are configured to induce strain or stress in the at least one of said at least three layers.

### Claim 6 (depends on 1)

The NLMT resist according to claim 1, wherein the pre-determined radiation is characterized by an irradiance level of no more than 2.3 mJ/cm2.

### Claim 7

A non-linear metallic thermal (NLMT) resist comprising:
a thin-film stack that includes
three or more alternating thin-film layers made, respectively, of first and second different host materials having respectively corresponding first and second lattice constants, and
a fourth layer between any two of said three or more alternating thin-film layers,
wherein material of said fourth layer has a lattice constant that is different from any of the first and second lattice constants;
said thin-film stack configured to form an alloy of said first and second host materials in response to being irradiated with pre-determined radiation;
said thin-film stack characterized by a curve that represents a rate of absorbance of said incident radiation as a function of depth of the thin-film stack, said depth being measured from a surface of the thin-film stack on which said pre-determined radiation is incident;
said curve having a positive slope in each segment thereof, different segments of said curve representing absorption of said pre-determined radiation in a corresponding one of said at least three thin-film layers.

### Claim 8 (depends on 7)

The NLMT resist according to claim 7, wherein a thickness of each constituent layer of the thin-film stack is less than 5 nm.

### Claim 9 (depends on 7)

The NLMT resist according to claim 7, wherein said species includes metallic or semiconductor species chosen to define defects, in said at least one of the at least three thin-film layers, said defects containing a gaseous element.

### Claim 10 (depends on 8)

The NLMT resist according to claim 8, wherein said first and second host materials include In ad Bi, respectively, and wherein said species include any of Pb, Sn, Ga, Si, Ge, Hg, Zr, and Ti.

### Claim 11 (depends on 8)

The NLMT resist according to claim 8, wherein said species are configured to induce strain or stress in the at least one of said at least three layers.

### Claim 12 (depends on 1)

The NLMT resist according to claim 1, wherein the pre-determined radiation is characterized by an irradiance level of no more than 2.3 mJ/cm2.

### Claim 13 (depends on 1)

The NLMT resist according to claim 1, wherein the pre-determined radiation is pulsed radiation characterized by irradiance of no more than 10 mJ/cm2.

### Claim 14

A metallic thermal resist film stack, comprising:
a first film of a first material;
a second film of a second material that is different than the first material, the first film and the second film in direct contact with one another;
a third film of the first material, the third film in direct contact to the second film and separated from the first film by the second film; and
a metallic or semiconductor species in at least one of the three film layers, said species being different from the first and second materials,
wherein the first, second and third films each exhibit a rate of absorption of radiation as a function of depth relative to a surface of the film stack upon which the radiation is incident thereon, wherein the rate of absorption of the first, second and third films when plotted vs. depth, each exhibit a positive slope respectively.

### Claim 15 (depends on 14)

The metallic thermal resist film stack of claim 14, further configured to form an alloy in response to the irradiation of the metallic or semiconductor species and the first, second and third films with radiation.

### Claim 16 (depends on 14)

The metallic thermal resist film stack of claim 14, further characterized as having an alloying threshold of exposure that corresponds to a light irradiance of radiation that is equal to or less than 2.3 mJ/cm2.

### Claim 17 (depends on 14)

The metallic thermal resist film stack of claim 14, wherein each of the first, second and third films are selected from the group consisting of Ga, In, Bi, Sb, Sn, Pb, Ca, or Al.

### Claim 18 (depends on 14)

The metallic thermal resist film stack of claim 14, wherein the film stack includes more than three films.

### Claim 19 (depends on 14)

The metallic thermal resist film stack of claim 14, wherein the film stack ranges from 3 to 10 films including the first, second and third films.

### Claim 20 (depends on 14)

The metallic thermal resist film stack of claim 14, wherein each of the first, second and third films have a thickness of 5 nm or less.

### Claim 21 (depends on 14)

The metallic thermal resist film stack of claim 14, wherein at least one of the first, second and third film layers includes distributed dopant sites for reducing an effective eutectic temperature for forming an alloy.

### Claim 22 (depends on 21)

The metallic thermal resist film stack of claim 21, wherein said distributed dopant sites are defined by at least one of Pb, Sn, Ga, Si, Ge, Hg, Zr, and Ti.

### Claim 23 (depends on 14)

The metallic thermal resist film stack of claim 14, wherein the metallic or semiconductor species in the at least one of the three films layers is a dopant that alters the lattice structure of the at least one of the three film layers.

### Claim 24 (depends on 1)

A method, comprising:
(a) forming a layer of material to be patterned onto a surface of a substrate;
(b) forming a metallic thermal resist film stack as recited in claim 1, the metallic thermal resist film stack characterized as having an alloying threshold of exposure that corresponds to light irradiance that is equal to or less than 2.3 mJ/cm2;
(c) forming an alloyed resist layer by irradiating the metallic thermal resist film stack with light radiation that is equal to or less than 2.3 mJ/cm2;
(d) selectively patterning the alloyed resist layer so that portions of the underlying layer of material are exposed; and
(e) processing the substrate so that the layer of material is patterned based on the selectively patterning of the resist layer.

### Claim 25 (depends on 24)

The method claim 24, further comprising:
(e) removing the selectively patterned alloyed resist layer;
(f) forming a second layer of material to be patterned over the patterned layer of material; and
(g) repeating steps (b) through (e) to pattern the second layer of material.