# US 2017/0292657 A1 · Temperature-stable paraffin inhibitor compositions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0292657 A1
- Document ID: US20170292657A1
- Status: Published application
- Kind: A1
- Application number: 15/480,959
- Filed: 2017-04-06
- Published: 2017-10-12
- Earliest claimed: 2016-04-07
- Assignees: Ecolab USA Inc.
- Applicants: Ecolab USA Inc.
- Inventors: Kousik Kundu
- Web page: https://patentgrep.com/patent/US20170292657A1

## CPC

- F17D 3/12: for injecting a composition into the line
- C09K 8/506: containing organic compounds
- C09K 8/524: organic depositions, e.g. paraffins or asphaltenes
- F17D: PIPE-LINE SYSTEMS; PIPE-LINES (pumps or compressors F04; fluid dynamics F15D; valves or the like F16K; pipes, laying pipes, supports, joints, branches, repairing, work on the entire line, accessories F16L; steam traps or the like F16T; fluid-pressure electric cables H01B9/06)
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

Disclosed are compositions including up to 20 wt % of a paraffin inhibiting polymer, a refined petroleum distillate and one or more low Log P molecules, wherein the compositions are stable and flow at a temperature between about 0° C. and −40° C., in many cases between about −20° C. and −40° C. The low Log P molecules are non-polymeric, have a Log P of less than 1, are liquids at 20° C. (1 atm), and have boiling points over 60° C., in many cases over 100° C. The compositions are useful paraffin inhibitor concentrates for use in the petroleum industry wherein the concentrates are stable, pumpable, and pourable at temperatures as low as −40° C. and as high as 60° C.

## Claims

### Claim 1

A paraffin inhibiting composition comprising:
about 1 wt % to 30 wt % of a paraffin inhibiting polymer, at least one refined petroleum solvent, and one or more low Log P molecules, wherein the composition is a stable nonaqueous composition that flows at −40° C.

### Claim 2 (depends on 1)

The paraffin inhibiting composition of claim 1 wherein the composition comprises about 2 wt % to 20 wt % of the paraffin inhibiting polymer.

### Claim 3 (depends on 1)

The paraffin inhibiting composition of claim 1 wherein the composition comprises about or about 10 wt % to 90 wt % of the at least one refined petroleum solvent.

### Claim 4 (depends on 1)

The paraffin inhibiting composition of claim 1 wherein the composition comprises about 1 wt % to 50 wt % of the one or more low Log P molecules.

### Claim 5 (depends on 1)

The paraffin inhibiting composition of claim 1 wherein the composition comprises about 1 wt % to 10 wt % of the one or more low Log P molecules.

### Claim 6 (depends on 1)

The paraffin inhibiting composition of claim 1 wherein the one or more low Log P molecules are non-polymeric, have a Log P between about −2 and about 0, a molecular weight of about 20 to about 200, and overall carbon content of about 8 carbon atoms or less.

### Claim 7 (depends on 1)

The paraffin inhibiting composition of claim 1 wherein the one or more low Log P molecules has Log P between about −1 and about 0.

### Claim 8 (depends on 1)

The paraffin inhibiting composition of claim 1 wherein the one or more low Log P molecules comprise one or more of methanol, isopropanol, 1, 2-propanediol, 1, 4-dioxane, butyrolactone, 2-pyrrolidone, 2-methoxyethanol, dimethylethanolamine, n-ethyl formamide, and 3-ketomorpholine.

### Claim 9 (depends on 1)

The paraffin inhibiting composition of claim 1 wherein the one or more low Log P molecules are substantially free of hydroxyl moieties.

### Claim 10 (depends on 1)

The paraffin inhibiting composition of claim 1 further comprising diethaminetriamine or a reaction product thereof.

### Claim 11 (depends on 1)

The paraffin inhibiting composition of claim 1 wherein the paraffin inhibiting polymer comprises one or more of polymers a, b, c, and d:
a. an alkylphenol-formaldehyde copolymer having the formula (I)
wherein R1=C9-C50 alkyl and n=2-200;
b. a copolymer comprising the residues of one or more alpha olefin monomers and a maleic anhydride monomer, the one or more alpha olefin monomers having the formula (II)
wherein R2, R3, R4, and R5 are independently selected from hydrogen and C5-C60 alkyl, with the proviso that at least two thereof are hydrogen; and the maleic anhydride monomer has the formula (III)
wherein R6 and R7 are independently hydrogen or C1-C60 alkyl, optionally wherein the maleic anhydride residue is further reacted with about 0.01 to 2.0 equivalents of a C12-C60 alkanol or amine per equivalent of anhydride;
c. an alkyl maleimide copolymer having the formula (IV)
wherein R8=C1-C50 alkyl, R9=C1-C50 alkyl, and n=1-200;
d. an acrylate having the formula (V)
wherein R10=C15-C25 alkyl, R11=C10-C15 alkyl, and n=1-100.

### Claim 12 (depends on 1)

The paraffin inhibiting composition of claim 1 wherein:
the paraffin inhibiting polymer comprises an alkylphenol-formaldehyde copolymer and the paraffin inhibiting polymer is about 1 wt % to about 20 wt % of the composition;
the at least one refined petroleum solvent comprises heavy aromatic naphtha and is about 50 wt % to about 80 wt % of the composition; and
the one or more low Log P molecules are about 1 wt % to about 20 wt % of the composition.

### Claim 13 (depends on 1)

The paraffin inhibiting composition of claim 1 wherein:
the paraffin inhibiting polymer comprises a plurality of paraffin inhibiting polymers including an alkylphenol-formaldehyde copolymer and a copolymer comprising the residues of one or more alpha olefin monomers and a maleic anhydride monomer;
each of the paraffin plurality of paraffin inhibiting polymers is about 1 wt % to about 15 wt % of the composition;
the at least one refined petroleum solvent includes one or more of heavy aromatic naphtha and toluene and is about 50 wt % to about 80 wt % of the composition; and
the one or more low Log P molecules is about 1 wt % to about 10 wt % of the composition.

### Claim 14 (depends on 1)

A crude oil composition, comprising:
a crude oil source; and
a paraffin inhibiting composition of claim 1;
wherein the paraffin inhibiting polymer is present in the crude oil source at about 5 ppm to 10000 ppm.

### Claim 15 (depends on 1)

A method of applying a paraffin inhibitor to a crude oil source, the method comprising:
forming a paraffin inhibitor concentrate of claim 1;
storing the paraffin inhibiting composition in an enclosed container at a first temperature between about −40° C. and 60° C.;
removing the paraffin inhibiting composition from the container at a second temperature between about −40° C. and 60° C.; and
applying the paraffin inhibiting composition to a crude oil source,
wherein the removing and the applying are accomplished using a mechanical pump.

### Claim 16 (depends on 15)

The method of claim 15 wherein the first temperature, the second temperature, or both the first and second temperature is between about −40° C. and −20° C.

### Claim 17 (depends on 15)

The method of claim 15 further comprising quenching the paraffin inhibiting polymer with a weak base having one or more amine moieties with the paraffin inhibiting polymer prior to forming the paraffin inhibitor concentrate.

### Claim 18 (depends on 17)

The method of claim 17 wherein the weak base having one or more amine moieties includes diethylaminetriamine.

### Claim 19 (depends on 15)

The method of claim 15 wherein the forming comprises mixing about 2 wt % to 20 wt % of the paraffin inhibiting polymer, about 10 wt % to 90 wt % of the at least one refined petroleum solvent, and about 1 wt % to 50 wt % of the one or more low Log P molecules.