# US 2017/0292478 A1 · Device for lowering the pour point of crude oil or heavy fuel oil

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0292478 A1
- Document ID: US20170292478A1
- Status: Published application
- Kind: A1
- Application number: 15/513,000
- Filed: 2015-09-24
- Published: 2017-10-12
- Earliest claimed: 2014-09-25
- Inventors: Antun Drvar
- Web page: https://patentgrep.com/patent/US20170292478A1

## CPC

- F02M 27/04: by electric means, {ionisation, polarisation} or magnetism
- B01J 16/00: Chemical processes in general for reacting liquids with non- particulate solids, e.g. sheet material; Apparatus specially adapted therefor (B01J19/08 takes precedence)
- B01J 19/0006: {Controlling or regulating processes (controlling or regulating in general G05)}
- B01J 19/006: {Baffles}
- B01J 19/2405: {provoking a turbulent flow of the reactants, such as in cyclones, or having a high Reynolds-number}
- B01J 19/242: {in series}
- C10G 32/02: by electric or magnetic means
- C22C 1/02: by melting {(C22C1/1036 takes precedence)}
- C22C 9/04: with zinc as the next major constituent
- C22F 1/08: of copper or alloys based thereon
- F02M 37/0064: {for engines being fed with multiple fuels or fuels having special properties, e.g. bio-fuels; varying the fuel composition (controlling engines working with pluralities of fuels F02D19/06)}
- B01J 2219/00063: of the reactants
- B01J 2219/00065: Pressure measurement
- B01J 2219/00069: Flow rate measurement
- B01J 2219/00162: controlling the pressure
- B01J 2219/00164: controlling the flow
- B01J 2219/00772: in a helix
- C10G 2300/304: Pour point, cloud point, cold flow properties
- F02M: SUPPLYING COMBUSTION ENGINES IN GENERAL WITH COMBUSTIBLE MIXTURES OR CONSTITUENTS THEREOF
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C10G: CRACKING HYDROCARBON OILS; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVE HYDROGENATION, OLIGOMERISATION, POLYMERISATION (cracking to hydrogen or synthesis gas C01B; cracking or pyrolysis of hydrocarbon gases to individual hydrocarbons or mixtures thereof of definite or specified constitution C07C; cracking to cokes C10B); RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, OR GASES; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS; REFORMING OF NAPHTHA; MINERAL WAXES
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

A device for treating crude oil or heavy fuel oil with a method that can lower the pour point to at least 0° C. Crude oil or heavy fuel oil treated thusly maintains this property for at least one year. The device for lowering the pour point of crude oil or heavy fuel oil uses a specific ionization method. The method is conducted by passing a heated medium through the main ionization device which is grounded and which includes three parallelly connected segments whereby each segment includes a protective copper tube inside which a protective insulating shell is situated, inside which a copper housing is situated. In each copper housing there is one cylindrical-shaped external core in which an internal core is placed, and the external core and internal core are manufactured as two different alloys by composition. Also described is a process for casting the external core and internal core.

## Claims

### Claim 1

A device for lowering a pour point of crude oil or heavy fuel oil and bunker fuel using a specific ionization method, and the method is conducted by passing heated crude oil or heavy fuel oil through a main ionization device, which is grounded and which comprises three parallelly connected segments whereby each segment comprises a protective copper tube inside which a protective insulating shell is situated, inside which a copper housing is situated, and in each copper housing there is one cylindrical-shaped external core in which an internal core is placed, and the external core and internal core are manufactured as two different alloys by composition wherein the alloy of the internal core is of the following composition:
Component
by weight (%)
aluminum
1.94
copper OFHC99.92
54.00
tin, 99.9% purity
1.80
zinc, 99.9% purity
22.10
antimony
0.05
iron
0.08
nickel
11.74
lead
8.00
gold
0.05
silver, 90% purity
0.04
tungsten
0.01
vanadium
0.02
phosphorus
0.02
sulfur
0.02
silicon
0.06
manganese
0.04
platinum
0.03
and wherein the alloy of the external core is of the following composition:
Component
by weight (%)
aluminum
2.40
copper OFHC99.92
52.73
gold
0.05
antimony
0.06
zinc, 99.9% purity
22.80
silver
0.04
tin, 99.9% purity
1.80
chromium
0.04
nickel
11.74
cobalt
0.05
tungsten
0.01
vanadium
0.02
lead
8.00
iron
0.08
phosphorus
0.05
sulfur
0.02
manganese
0.04
silicon
0.03
platinum
0.04

### Claim 2 (depends on 1)

The device according to claim 1, wherein the main ionization device contains at least three main ionization segments that are interconnected parallelly, and each ionization segment individually comprises a protective copper tube inside which a protective insulating shell is located, in which the copper housing and external core and internal core are situated.

### Claim 3 (depends on 1)

The device according to claim 1, wherein at least 6 ionization devices are serially connected, each of which comprises three main ionization segments in order to lower the pour point of crude oil or heavy fuel oil to 0° C., and therefore remain at that temperature for at least one year.

### Claim 4 (depends on 1)

The device according to claim 1, wherein the length of one internal core and external core of the ionization segment does not exceed 28.5 cm, and an increase in the capacity of the device can is realized by increasing a cross section of the core.

### Claim 5 (depends on 1)

The device according to claim 1, wherein the internal core has the shape of a trapezoid thread in order to achieve maximum contact of the medium over the area of the cores by friction.

### Claim 6 (depends on 5)

The device according to claim 5, wherein the internal core has a starting left trapezoidal thread, and after ¼ of the length of the core, the core is converted to a right trapezoidal thread, which after 2/4 of the length of the core once again coverts to a left trapezoidal thread, and at the final ¼, the core again converts to a right trapezoidal thread.

### Claim 7 (depends on 5)

The device according to claim 5, wherein the internal core has a starting right trapezoidal thread, and after ¼ of the length of the core, the core is converted to a left trapezoidal thread, which after 2/4 of the length of the core once again coverts to a right trapezoidal thread, and at the final ¼, the core again converts to a left trapezoidal thread.

### Claim 8 (depends on 1)

The device according to claim 1, wherein the external core has a cylindrical shape with a lengthwise bore through its axial length, which has hemispherical protrusions on its inside rim in order to additionally increase the turbulence of the medium in the device and its friction over the area of the cores.

### Claim 9 (depends on 8)

The device according to claim 8, wherein the external core has on its inside four main rows of 56 hemispherical protrusions arranged at 90° and between every two of the four primary rows, an additional row of 48 hemispherical protrusions is situated; the first additional row is positioned at 45°, the second at 135°, the third at 225°, and the last additional row at 315°.

### Claim 10 (depends on 1)

The device according to claim 1, wherein the composition of the insulting shell is such that it contains 50% polyamide and 50% fiberglass.

### Claim 11 (depends on 1)

A process of manufacturing an internal core of an ionization device comprising:
a. Placing aluminum, cooper, tin, antimony and iron in a mold in the percentages defined in claim 1;
b. Heating the metals in the mold, and the mold is heated to a temperature of approximately 980 to 1200° C., until a molten compound of metals is obtained;
c. Raising the temperature to 1425-1540° C., and nickel, lead, gold, silver, tungsten, vanadium, phosphorous, sulfur, silicon and manganese are added into the molten compound of metals in the percentages as defined in claim 1;
d. Maintaining the temperature of the molten compound of metals at a temperature of at least approximately 1500° C. for at least 5 minutes, and at most for 10 minutes;
e. Due to its low melting point, adding zinc 5 minutes before the molten compound of metals is cast in an appropriate mold;
f. Adding an appropriate amount of borax into the molten compound of metals so that the impurities from the materials would rise to the surface, where they are physically removed;
g. Casting into the molds then follows, and cooling of the cast compound to room temperature, upon which cleaning is performed as necessary, with mandatory sandblasting of the cast elements;
h. The core must then be rid of exterior unevenness; and
i. The internal core that has been processed thusly is again heated to approximately 200° C. and briefly immersed in molten platinum in order to create a thin film on the entire surface.

### Claim 12 (depends on 1)

A process of manufacturing an external core of an ionization device comprising:
a. Placing aluminum, cooper, tin, antimony and iron in a mold in the percentages as defined in claim 1;
b. Heating of the metals in the mold, and the mold is heated to a temperature of approximately 980 to 1200° C., until a molten compound of metals is obtained;
c. Raising the temperature to 1425-1540° C., and nickel, lead, gold, silver, tungsten, vanadium, phosphorous, sulfur, chrome, cobalt, silicon and manganese are added into the molten compound of metals in the percentages as defined in claim 1;
d. Maintaining the temperature of the molten compound of metals at a temperature of at least approximately 1500° C. for at least 5 minutes, and at most for 10 minutes;
e. Due to its low melting point, adding zinc 5 minutes before the molten compound of metals is cast in an appropriate mold;
f. Adding an appropriate amount of borax into the molten compound of metals so that the impurities from the materials would rise to the surface, where they are physically removed;
g. Casting into the molds then follows, and cooling of the cast compound to room temperature, upon which cleaning is performed as necessary, with mandatory sandblasting of the cast elements;
h. The core must then be rid of exterior unevenness; and
i. The external core that has been processed thusly is again heated to approximately 200° C. and briefly immersed in molten platinum in order to create a thin film on the entire surface.

### Claim 13 (depends on 1)

The process of obtaining ionized liquid crude oil or heavy fuel oil using the device according to claim 1, wherein the preferred inlet pressure of the liquid crude oil or heavy fuel oil is at least 25 bars, and optimal ionization is achieved at a temperature of approximately 90° C. at a pressure of 25 bars.

### Claim 14 (depends on 13)

The process of obtaining ionized liquid crude oil or heavy fuel oil according to claim 13, wherein for temperatures of the inlet medium that are lowered for each 10° C., the ionization assembly is extended by one additional ionization device, which comprises three main parallelly connected segments, while the inlet pressure of the medium for each 10° C. decrease in temperature must be increased by 2 bars.

### Claim 15 (depends on 1)

The device for lowering the pour point of crude oil or heavy fuel oil according to claim 1, wherein the service is used directly on oil wells for the production and transportation of crude oil or heavy fuel oil, in refineries for the production and transportation of crude oil or heavy fuel oil, and for the storage of crude oil or heavy fuel oil.

### Claim 16 (depends on 2)

The device according to claim 2, wherein at least 6 ionization devices are serially connected, each of which comprises three main ionization segments in order to lower the pour point of crude oil or heavy fuel oil to 0° C., and therefore remain at that temperature for at least one year.