# US 2017/0292223 A1 · Wet strengthened fiber products, wet strengthening resins, and methods for making and using same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0292223 A1
- Document ID: US20170292223A1
- Status: Published application
- Kind: A1
- Application number: 15/634,615
- Filed: 2017-06-27
- Published: 2017-10-12
- Earliest claimed: 2014-03-27
- Assignees: Georgia-Pacific Chemicals LLC
- Applicants: Georgia-Pacific Chemicals LLC
- Inventors: Cornel Hagiopol; David F. Townsend; Clay E. Ringold; James W. Johnston
- Web page: https://patentgrep.com/patent/US20170292223A1

## CPC

- D21H 21/20: Wet strength agents
- C08G 73/0286: {Preparatory process from polyamidoamines and epihalohydrins}
- C08L 25/08: Copolymers of styrene (C08L29/08, C08L35/06, C08L55/02 take precedence)
- C08L 77/00: Compositions of polyamides obtained by reactions forming a carboxylic amide link in the main chain (of polyhydrazides C08L79/06; of polyamideimides or polyamide acids C08L79/08); Compositions of derivatives of such polymers
- C09D 125/08: Copolymers of styrene (C09D129/08, C09D135/06, C09D155/02 take precedence)
- D21H 17/40: unsaturated
- D21H 17/44: cationic
- D21H 17/45: Nitrogen-containing groups
- D21H 17/455: {comprising tertiary amine or being at least partially quaternised}
- D21H 17/55: Polyamides; Polyaminoamides; Polyester-amides
- D21H 17/72: {of organic material}
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

Wet strengthened fiber products, wet strengthening resins, and methods for making such wet strengthened fiber products and wet strengthening resins. The wet strengthened fiber product can include a fiber web and an at least partially cured wet strengthening resin, which prior to at least partially curing, the wet strengthening resin can include a polyamide-epihalohydrin (PAE) resin and a cationic styrene maleimide (SMI) resin. The PAE resin can include a reaction product of a polyamidoamine and an epihalohydrin and the cationic SMI resin can include a reaction product of a styrene maleic anhydride (SMA) copolymer and an amine. The wet strengthened fiber product can include the wet strengthening resin in an amount of about 0.05 wt % to about 5 wt %, based on a dried weight of the wet strengthened fiber product.

## Claims

### Claim 1

A wet strengthening resin, comprising:
a polyamide-epihalohydrin resin comprising a reaction product of a polyamidoamine and an epihalohydrin; and
a cationic styrene maleimide resin comprising a reaction product of a styrene maleic anhydride copolymer and an amine compound, a weight average molecular weight of about 500 to about 200,000, and a styrene to maleimide molar ratio of about 1:1 to about 5:1, wherein the wet strengthening resin comprises about 5 wt % to about 95 wt % of the cationic styrene maleimide resin, based on a combined weight of the polyamide-epihalohydrin resin and the cationic styrene maleimide resin.

### Claim 2 (depends on 1)

The wet strengthening resin of claim 1, wherein the cationic styrene maleimide resin has the chemical formula:
wherein:
R+ is a cationic molecular group;
A− is an anion;
m is an integer of 1 to about 5; and
n is an integer of about 5 to about 800.

### Claim 3 (depends on 2)

The wet strengthening resin of claim 2, wherein the cationic molecular group is a cationic ammonium group, wherein the anion is a carboxylate, and the carboxylate is an acetate anion, a citrate anion, an oxalate anion, a lactate anion, a formate anion, or a mixture thereof.

### Claim 4 (depends on 3)

The wet strengthening resin of claim 3, wherein m is equal to 1 and n is an integer of about 5 to about 100.

### Claim 5 (depends on 3)

The wet strengthening resin of claim 3, wherein m is equal to 3 and n is an integer of about 50 to about 300.

### Claim 6 (depends on 1)

The wet strengthening resin of claim 1, wherein the cationic styrene maleimide resin has the chemical formula:
wherein:
R1 is a substituted or unsubstituted organic diyl group;
R2, R3, and R4 are each independently selected from a hydrogen or a substituted or unsubstituted linear, branched, cyclic, heterocyclic, or aromatic hydrocarbyl group;
A− is an anion;
m is an integer of 1 to about 5; and
n is an integer of about 5 to about 800.

### Claim 7 (depends on 6)

The wet strengthening resin of claim 6, wherein R1 is selected from the group consisting of: methanediyl, ethanediyl, propanediyl, butanediyl, pentanediyl, and a mixture thereof, wherein R2, R3, and R4 are each independently selected from the group consisting of: hydrogen, methyl, ethyl, propyl, butyl, and pentyl.

### Claim 8 (depends on 1)

The wet strengthening resin of claim 1, wherein the cationic styrene maleimide resin has the chemical formula:
wherein:
A− is an anion; and
n1, n2, and n3 are each independently of about 5 to about 800.

### Claim 9 (depends on 8)

The wet strengthening resin of claim 8, wherein the anion is a carboxylate, wherein n1 is about 5 to about 100, n2 is about 20 to about 200, and n3 is about 50 to about 300.

### Claim 10 (depends on 1)

The wet strengthening resin of claim 1, wherein the cationic styrene maleimide resin has the chemical formula:
wherein n1 is about 5 to about 100, n2 is about 20 to about 200, and n3 is about 50 to about 300.

### Claim 11 (depends on 1)

The wet strengthening resin of claim 1, wherein the cationic styrene maleimide resin comprises a copolymer of styrene and dimethylaminopropylamine maleimide acetate.

### Claim 12 (depends on 1)

The wet strengthening resin of claim 1, wherein the polyamide-epihalohydrin resin has a weight average molecular weight of about 20,000 to about 3,000,000, an azetidinium ion ratio of about 0.55 to about 0.80, and a charge density of about 1.5 mEq/g to about 3.0 mEq/g of solids.

### Claim 13

A process for making a wet strengthening resin, comprising:
combining a polyamide-epihalohydrin resin and a cationic styrene maleimide resin to produce a wet strengthening resin, wherein:
the polyamide-epihalohydrin resin comprises a reaction product of a polyamidoamine and an epihalohydrin,
the cationic styrene maleimide resin comprises a reaction product of a styrene maleic anhydride copolymer and an amine compound, a weight average molecular weight of about 500 to about 200,000, and a styrene to maleimide molar ratio of about 1:1 to about 5:1, and
the wet strengthening resin comprises about 5 wt % to about 95 wt % of the cationic styrene maleimide resin, based on the combined weight of the polyamide-epihalohydrin resin and the cationic styrene maleimide resin.

### Claim 14 (depends on 13)

The process of claim 13, wherein the polyamide-epihalohydrin resin has a weight average molecular weight of about 20,000 to about 3,000,000, an azetidinium ion ratio of about 0.55 to about 0.80, and a charge density of about 1.5 mEq/g to about 3.0 mEq/g of solids.

### Claim 15 (depends on 13)

The process of claim 13, wherein the cationic styrene maleimide resin comprises copolymers of styrene and dimethylaminopropylamine maleimide acetate.

### Claim 16 (depends on 13)

The process of claim 13, wherein the polyamide-epihalohydrin resin has a weight average molecular weight of about 20,000 to about 3,000,000, an azetidinium ion ratio of about 0.55 to about 0.80, and a charge density of about 1.5 mEq/g to about 3.0 mEq/g of solids, and wherein the cationic styrene maleimide resin comprises a copolymer of styrene and dimethylaminopropylamine maleimide acetate.

### Claim 17

A fiber mixture, comprising:
a plurality of fibers; and
a wet strengthening resin, comprising:
a polyamide-epihalohydrin resin comprising a reaction product of a polyamidoamine and an epihalohydrin; and
a cationic styrene maleimide resin comprising a reaction product of a styrene maleic anhydride copolymer and an amine compound, a weight average molecular weight of about 500 to about 200,000, and a styrene to maleimide molar ratio of about 1:1 to about 5:1, wherein the wet strengthening resin comprises about 5 wt % to about 95 wt % of the cationic styrene maleimide resin, based on a combined weight of the polyamide-epihalohydrin resin and the cationic styrene maleimide resin.

### Claim 18 (depends on 17)

The fiber mixture of claim 17, wherein the plurality of fibers comprises cellulosic fibers.

### Claim 19 (depends on 18)

The fiber mixture of claim 18, wherein the polyamide-epihalohydrin resin has a weight average molecular weight of about 20,000 to about 3,000,000, an azetidinium ion ratio of about 0.55 to about 0.80, and a charge density of about 1.5 mEq/g to about 3.0 mEq/g of solids.

### Claim 20 (depends on 19)

The fiber mixture of claim 19, wherein the cationic styrene maleimide resin comprises copolymers of styrene and dimethylaminopropylamine maleimide acetate.