# US 2017/0292190 A1 · Anti-multipactor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0292190 A1
- Document ID: US20170292190A1
- Status: Published application
- Kind: A1
- Application number: 15/511,220
- Filed: 2015-09-16
- Published: 2017-10-12
- Earliest claimed: 2014-09-16
- Assignees: Consejo Superior De Investigaciones Cientificas (Csic); European Space Agency (ESA); Tesat-Spacecomo GmbH & Co. KG
- Applicants: Consejo Superior De Investigaciones CientíFicas (Csic); European Space Agency (Esa); Tesat-Spacecomo GmbH & Co. KG
- Inventors: Isabel MONTERO HERRERO; Lydya Sabina AGUILERA MAESTRO; David RABOSO GARCIA-BAQUERO; Ulrich WOCHNER
- Web page: https://patentgrep.com/patent/US20170292190A1

## CPC

- C23C 18/1669: {Agitation, e.g. air introduction}
- C23C 18/165: {Multilayered product (layered product B32B)}
- C23C 18/1841: {with use of metal first}
- C23C 18/38: Coating with copper
- C23C 18/44: using reducing agents
- G21F 1/125: {comprising metals}
- H01J 23/12: Vessels; Containers
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- G21F: PROTECTION AGAINST X-RADIATION, GAMMA RADIATION, CORPUSCULAR RADIATION OR PARTICLE BOMBARDMENT; TREATING RADIOACTIVELY CONTAMINATED MATERIAL; DECONTAMINATION ARRANGEMENTS THEREFOR (radiation protection by pharmaceutical means A61K8/00, A61Q17/04; in cosmonautic vehicles B64G1/54; combined with a reactor G21C11/00; combined with X-ray tubes H01J35/16; combined with X-ray apparatus H05G1/02)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

The invention relates to anti-multipactor coating deposited onto a substrate that can be exposed to the air and its procedure of obtainment by simple chemical methods. Furthermore, the present invention relates to its use for the fabrication of high power devices working at high frequencies.

## Claims

### Claim 1

Anti-multipactor coating deposited onto a substrate characterized in that
it comprises at least two contacting high conductive metal layers with an electrical conductivity greater than 4×107 S·m−1,
it has a secondary electron emission yield below 1 in air, between 0.4 and 0.9 for a incident electron energy range between 0 and 5000 eV,
it has a final surface roughness with a grooves aspect ratio greater than 4, with a surface grooves density greater than 70%,
and it has a insertion loss of between 0.1 and 0.14 dB, wherein the substrate consists of a metal or a mixture of metals.

### Claim 2 (depends on 1)

Anti-multipactor coating according to claim 1, wherein the substrate consists of a metal or a mixture of metals selected from Ni doped with P, Al, Cu and Ag.

### Claim 3 (depends on 1, 2)

Anti-multipactor coating according to any of claim 1 or 2, wherein the high conductive metal of each layer is selected independently from Ag and Cu.

### Claim 4 (depends on 1, 2, 3)

A process of obtainment of the anti-multipactor coating deposited onto a substrate according to any of claims 1 to 3, wherein the process comprises at least the following steps:
a) deposition of a high conductive metal layer, with an electrical conductivity greater than 4×107 S·m−1, onto a substrate,
b) etching of the deposited high conductive metal layer of step a) by an acid dissolution, c) activating of the etched layer obtained in step b), and d) electroless plating of a high conductive metal, of an electrical conductivity greater than 4×107 S·m−1, onto the activated etched layer obtained in step c) using a solution of high conductive metal ions and a reducing agent.

### Claim 5

The process of obtainment, according to the previous claim, wherein the high conductive metal layer of step a) is made of Ag or Cu.

### Claim 6 (depends on 4, 5)

The process of obtainment according to any of claim 4 or 5, wherein the deposition of step a) is performed by conventional chemical deposition techniques such as plating, chemical solution deposition, spin coating, chemical vapor deposition and atom layer deposition, and/or physical deposition techniques such as electron beam evaporator, molecular beam epitaxy, pulsed laser deposition, sputtering, cathodic arc deposition and electrospray deposition.

### Claim 7 (depends on 4, 5, 6)

The process of obtainment, according to any of claims 4 to 6, wherein the acid dissolution of step b) comprises hydrofluoric acid, nitric acid, acetic acid, deionized water or a mixture thereof.

### Claim 8 (depends on 4, 5, 6, 7)

The process of obtainment, according to any of claims 4 to 7, wherein step c) is performed by adding an aqueous solution of SnCl2 or PdCl2.

### Claim 9 (depends on 4, 5, 6, 7, 8)

The process of obtainment, according to any of claims 4 to 8, wherein step c) is performed by adding an aqueous solution of SnCl2 in a concentration range between 0.05-1.2% in weight to the etched layer obtained in step b).

### Claim 10 (depends on 4, 5, 6, 7, 8, 9)

The process of obtainment, according to any of claims 4 to 9, wherein the high conductive metal used during step d) of electroless plating is selected from Ag or Cu.

### Claim 11 (depends on 4, 5, 6, 7, 8, 9, 10)

The process of obtainment, according to any of claims 4 to 10, wherein step d) of electroless plating is performed under continuous agitation and using a bath temperature between 30 and 80° C.

### Claim 12 (depends on 4, 5, 6, 7, 8, 9, 10, 11)

The process of obtainment, according to any of claims 4 to 11, wherein the solution of high conductive metal ions of step d) is an aqueous solution of AgNO3.

### Claim 13 (depends on 4, 5, 6, 7, 8, 9, 10, 11, 12)

The process of obtainment, according to any of claims 4 to 12, wherein the reducing agent of step d) is selected from triethanolamine, diethanolamine or monoethanolamine.

### Claim 14 (depends on 1, 2, 3)

Use of the anti-multipactor coating deposited onto a substrate according to any of claims 1 to 3 for the fabrication of high power devices, operating at powers higher than 0.1 kW, working at high frequencies, from MHz range up to tens of GHz.

### Claim 15

Use according to the previous claim, wherein the device is a microwave, a radio frequency device for space, thermonuclear or large accelerator instrumentation.