# US 2017/0292180 A1 · Wrought product made of a magnesium-lithium-aluminum alloy

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0292180 A1
- Document ID: US20170292180A1
- Status: Published application
- Kind: A1
- Application number: 15/514,398
- Filed: 2015-09-29
- Published: 2017-10-12
- Earliest claimed: 2014-09-29
- Assignees: Constellium Issoire
- Applicants: Constellium Issoire
- Inventors: Gaëlle POUGET; Bernard BES
- Web page: https://patentgrep.com/patent/US20170292180A1

## CPC

- C22F 1/047: of alloys with magnesium as the next major constituent
- C22C 21/06: with magnesium as the next major constituent
- C22C 21/08: with silicon
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The invention relates to a wrought product made of an aluminum alloy having the composition in % by weight, Mg: 4.0-5.0; Li: 1.0-1.8; Mn: 0.3-0.5; Zr: 0.05-0.15; Ag: ≦0.5; Fe: ≦0.1; Ti: <0.15; Si: ≦0.05; other elements ≦0.05 each and ≦0.15 in association; the remainder is aluminum. The invention further relates to a method for manufacturing a wrought product wherein an unprocessed form of aluminum alloy is cast, which has the composition, in % by weight: Mg: 4.0-5.0; Li: 1.0-1.8; Mn: 0.3-0.5; Zr: 0.05-0.15; Ag: ≦0.5; Fe: ≦0.1; Ti: <0.15; Si: ≦0.05; other elements ≦0.05 each and ≦0.15 in combination; the remainder is aluminum; optionally, said unprocessed form is homogenized; said unprocessed form is hot worked to obtain a hot-worked product; optionally, said hot-worked product is solution heat treated at a temperature from 360° C. to 460° C., preferably from 380° C. to 420° C., for 15 minutes to 8 hours; said hot-worked product is quenched; optionally, said worked and quenched product is straightened; optionally, the worked product is cold worked under controlled conditions to obtain permanent cold working set from 1 to 10%, preferably from 2 to 6%, most preferably from 3 to 5%; said worked and quenched product is aged. The invention further relates to the use of said wrought product to produce aircraft structural elements.

## Claims

### Claim 1

Wrought product made of an aluminum alloy comprising in % by weight, Mg: 4.0-5.0; Li: 1.0-1.8; Mn: 0.3-0.5; Zr: 0.05-0.15; Ag: ≦0.5; Fe: ≦0.1; Ti: <0.15; Si: ≦0.05; other elements ≦0.05 each and ≦0.15 in combination; the remainder is aluminum.

### Claim 2 (depends on 1)

Wrought product according to claim 1 having a Mn content, in % by weight, of 0.35 to 0.45.

### Claim 3 (depends on 1)

Wrought product according to claim 1 having a Zn content, in % by weight, less than 0.04%, optionally less than or equal to 0.03%.

### Claim 4 (depends on 1)

Wrought product according to claim 1 having an Fe content, in % by weight, less than 0.08%, optionally less than or equal to 0.07%, optionally less than or equal to 0.06%.

### Claim 5 (depends on 1)

Wrought product according to claim 1 having an Li content, in % by weight, less than 1.6%, optionally less than or equal to 1.5%, optionally less than or equal to 1.4%.

### Claim 6 (depends on 1)

Wrought product according to claim 1, having less delamination on the rupture surfaces of the K1c specimens obtained according to standard ASTM E399 than an identical wrought product, having for a difference in its Mn content, in % by weight, less than 0.3%.

### Claim 7 (depends on 1)

Wrought product according to claim 1, having at mid-thickness, for a thickness between 0.5 and 15 mm, an ultimate tensile strength Rm (L) greater than that of an identical wrought product, having a difference in its Mn content, in % by weight.

### Claim 8 (depends on 1)

Wrought product according to claim 1, having at mid-thickness, for a thickness between 0.5 and 15 mm, a tensile yield strength Rp0.2 (L) greater than that of an identical wrought product, having for a difference in its Mn content, in % by weight.

### Claim 9

Method for manufacturing a wrought product comprising:
(a) casting an unprocessed form of aluminum alloy, which comprises, in % by weight: Mg: 4.0-5.0; Li: 1.0-1.8; Mn: 0.3-0.5; Zr: 0.05-0.15; Ag: ≦0.5; Fe: ≦0.1; Ti: <0.15; Si: ≦0.05; other elements ≦0.05 each and ≦0.15 in combination; the remainder is aluminum;
(b) optionally, homogenizing said unprocessed form;
(c) hot working said unprocessed form to obtain a hot-worked product;
(d) optionally, solution heat treating said hot-worked product at a temperature from 360° C. to 460° C., optionally from 380° C. to 420° C. for 15 minutes to 8 hours;
(e) quenching said hot-worked product;
(f) optionally, straightening/flattening said worked and quenched product;
(g) optionally, cold working the worked and quenched product in a controlled manner in order to obtain a permanent cold working set from 1 to 10%, optionally from 2 to 6%, optionally from 3 to 5%;
(h) artificially aging said hot-worked and quenched product.

### Claim 10 (depends on 9)

Method according to claim 9 wherein said aging (h) is carried out before cold working in a controlled manner (g).

### Claim 11 (depends on 9)

Method according to claim 9 wherein the hot working of (c) is a working by extruding an unprocessed form.

### Claim 12 (depends on 9)

Method according to claim 9 wherein the quenching of (e) is a press quenching.

### Claim 13 (depends on 1)

A wrought product according to claim 1 used for an aircraft structural element, optionally a fuselage skin, a circumferential frame, a fuselage stiffener or stringer or a rib.

### Claim 14 (depends on 9)

A wrought product obtained according to claim 9 used for an aircraft structural element, optionally a fuselage skin, a circumferential frame, a fuselage stiffener or stringer or a rib.