# US 2017/0292047 A1 · Hexene-1 Containing Amorphous Polyalphaolefins For Improved Hot Melt Adhesives

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0292047 A1
- Document ID: US20170292047A1
- Status: Published application
- Kind: A1
- Application number: 15/486,115
- Filed: 2017-04-12
- Published: 2017-10-12
- Earliest claimed: 2016-04-12
- Assignees: Rextac LLC
- Applicants: REXtac LLC
- Inventors: Andres Sustic; John Passmore; Nick Fowler; John J. DeCair
- Web page: https://patentgrep.com/patent/US20170292047A1

## CPC

- C09J 123/14: Copolymers of propene (C09J123/16 takes precedence)
- C08J 3/00: Processes of treating or compounding macromolecular substances
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

Propylene-co-hexene-1-co-butene-1 terpolymers, made either with or without an in-reactor-added organosilicon external donor, are used in the formulation of improved-performance, APAO-based, hot melt adhesives. The addition of an external donor during the manufacture of hexene-1 based amorphous polyalpha-olefins (APAO's) results in products having enhanced physical and mechanical properties compared to similar adhesive products made without the addition of the external donor.

## Claims

### Claim 1

A hot-melt formulation comprising:
a propylene-co-hexene-1-co-butene-1 terpolymer made using a supported Ziegler-Natta catalyst, at a process temperature between about 130° F. and about 175° F. and at a reactor pressure sufficient to maintain propylene in the liquid phase (in the absence of any added solvent) and the hydrogen concentration present during the manufacture of the subject terpolymers is adjusted so that their melt viscosity, measured at 190° C., is less than 3500 cps, preferably less than 3000 cps, optionally in the presence of an organo-silane external donor and optionally with,
a tackifier; and/or
a styrenic block copolymer; and/or
a high melt flow index metallocene or single-site catalyzed polyethylene; and/or
a high melt flow rate polypropylene, either a homopolymer or random copolymer, of varying degrees of crystallinity or isotacticity, functionalized or without any polar functionality; and/or
a wax component; and/or
a liquid plasticizer.

### Claim 2 (depends on 1)

The hot-melt formulation of claim 1 wherein the copolymer is made in the presence of an externally-added organosilicon donor.

### Claim 3 (depends on 8)

The hot-melt formulation of claim 8 wherein the terpolymer is made in the presence of an externally-added organosilicon donor.

### Claim 4 (depends on 1)

The hot-melt formulation of claim 1 comprising a propylene-co-hexene-1 copolymer with a boiling heptane insolubility of less than 20 wt. %.

### Claim 5 (depends on 1)

The hot-melt formulation of claim 1 comprising a propylene-co-hexene-1 copolymer manufactured in the absence of any added solvent

### Claim 6 (depends on 1)

The hot-melt formulation of claim 1 wherein the liquid plasticizer comprises a naphthenic oil.

### Claim 7 (depends on 8)

The hot-melt formulation of claim 8 wherein the liquid plasticizer comprises a naphthenic oil.

### Claim 8 (depends on 1)

The hot-melt formulation of claim 1 wherein the liquid plasticizer comprises a paraffinic oil.

### Claim 9 (depends on 8)

The hot-melt formulation of claim 8 wherein the liquid plasticizer comprises a paraffinic oil.

### Claim 10 (depends on 1)

The hot-melt formulation of claim 1 wherein the wax component comprises a paraffinic wax.

### Claim 11 (depends on 8)

The hot-melt formulation of claim 8 wherein the wax component comprises a paraffinic wax.

### Claim 12 (depends on 1)

The hot-melt formulation of claim 1 wherein the wax component comprises a metallocene wax.

### Claim 13 (depends on 2)

The hot-melt formulation of claim 2 wherein the wax component comprises a metallocene wax.

### Claim 14 (depends on 1)

The hot-melt formulation of claim 1 wherein the terpolymer is made at a process temperature between about 130° F. and about 175° F. and at a reactor pressure sufficient to maintain propylene in the liquid phase (in the absence of any added solvent).

### Claim 15 (depends on 1)

The hot-melt formulation of claim 1 wherein the hydrogen concentration present during the manufacture of the terpolymer is adjusted such that its melt viscosity, measured at 375° F., is less than 3500 cps.

### Claim 16 (depends on 1)

The hot-melt formulation of claim 1 wherein the hydrogen concentration present during the manufacture of the terpolymer is adjusted such that its melt viscosity, measured at 375° F., is less than 3000 cps.