# US 2017/0291826 A1 · Production of high strength hydrochloric acid from calcium chloride feed streams by crystallization

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0291826 A1
- Document ID: US20170291826A1
- Status: Published application
- Kind: A1
- Application number: 15/091,666
- Filed: 2016-04-06
- Published: 2017-10-12
- Earliest claimed: 2016-04-06
- Assignees: The Royal Institution for the Advancement of Learning/Mcgill University
- Applicants: The Royal Institution for the Advancement of Learning/Mcgill University
- Inventors: George DEMOPOULOS; Thomas FELDMANN
- Web page: https://patentgrep.com/patent/US20170291826A1

## CPC

- C01F 11/46: Sulfates (dehydration of gypsum {for the production of calcium sulfate cements} C04B11/02)
- C01B 7/035: {Preparation of hydrogen chloride from chlorides}
- C22B 3/10: Hydrochloric acid {, other halogenated acids or salts thereof}
- C22B 3/44: by chemical processes (treatment or purification of solutions by liquid-liquid extraction C22B3/26, by ion-exchange extraction C22B3/42)
- C22B 59/00: Obtaining rare earth metals
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2002/88: by thermal analysis data, e.g. TGA, DTA, DSC
- C01P 2004/03: obtained by SEM
- Y02P 10/20: Recycling
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present relates to a method for producing calcium sulfate solid crystals and hydrochloric acid (HCl) from a calcium chloride solution comprising the steps of feeding a continuous stirred-tank reactor with a calcium chloride solution, sulfuric acid and water; mixing the calcium chloride solution, sulfuric acid and water in the reactor; and maintaining the reactor a temperature of less than about 70° C., converting the calcium chloride solution, sulfuric acid and water into HCl and calcium sulfate solid crystals. The method described herein can be incorporated as a means for regenerating HCl from CaCl2 solutions which are generated in the metallurgical industry when processing calcium-bearing ores for recovering metals like rare earth elements.

## Claims

### Claim 1

A method for producing calcium sulfate solid crystals and azeotropic hydrochloric acid (HCl) from a calcium chloride solution comprising the steps of:
feeding a continuous-stirred tank reactor with a calcium chloride solution, sulfuric acid and water;
mixing the calcium chloride solution, sulfuric acid and water in the reactor; and
maintaining the reactor at a temperature of less than about 70° C.,
converting the calcium chloride solution, sulfuric acid and water into azeotropic HCl and calcium sulfate solid crystals.

### Claim 2 (depends on 1)

The method of claim 1, wherein the calcium sulfate solid crystals are crystals of at least one of calcium sulfate dihydrate, calcium sulfate α-hemihydrate and mixture thereof.

### Claim 3

(canceled)

### Claim 4 (depends on 1)

The method of claim 1, wherein up to 30 wt % (9.5 mol/L) of super-azeotropic HCl is obtained.

### Claim 5 (depends on 1)

The method of claim 1, wherein the ratio of sulfate to calcium in the reactor is 0.90 to 0.98.

### Claim 6 (depends on 1)

The method of claim 1, wherein the temperature of the reactor is about less than 60° C.

### Claim 7 (depends on 1)

The method of claim 1, wherein the temperature of the reactor is about 40° C.-70° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein the temperature of the reactor is about 40° C. or less.

### Claim 9 (depends on 1)

The method of claim 1, wherein the reactor is continuously fed with calcium chloride solution, sulfuric acid and water, continuously producing azeotropic HCl and calcium sulfate solid crystals.

### Claim 10 (depends on 1)

The method of claim 1, wherein the calcium chloride solution is a feed stream from the processing of calcium-bearing ores.

### Claim 11 (depends on 1)

The method of claim 1, wherein calcium chloride solution, sulfuric acid and water are fed in multiple parallel reactors.

### Claim 12

A process of extracting metals from calcium-bearing ores comprising the steps of:
leaching the ores with HCl, producing a leachate containing a calcium chloride solution and metals;
separating the metals from the calcium chloride solution;
feeding a continuous-stirred tank reactor with the calcium chloride solution, sulfuric acid and water;
mixing the calcium chloride solution, sulfuric acid and water in the reactor;
maintaining the reactor at a temperature of less than about 70° C., converting the calcium chloride solution, sulfuric acid and water into azeotropic HCl and calcium sulfate solid crystals; and
recycling the HCl to the leaching of the ores.

### Claim 13 (depends on 12)

The process of claim 12, wherein the calcium sulfate solid crystals are crystals of at least one of calcium sulfate dihydrate, calcium sulfate α-hemihydrate and mixture thereof.

### Claim 14

(canceled)

### Claim 15 (depends on 12)

The process of claim 12, wherein the metals are rare earth metals.

### Claim 16 (depends on 1)

A construction board comprising calcium sulfate α-hemihydrate produced by the method of claim 1.