# US 2017/0291137 A1 · Method for converting lime-based wet flue gas desulfurization systems to limestone-based systems

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0291137 A1
- Document ID: US20170291137A1
- Status: Published application
- Kind: A1
- Application number: 15/485,904
- Filed: 2017-04-12
- Published: 2017-10-12
- Earliest claimed: 2016-04-12
- Assignees: AECOM Technical Services, Inc.
- Applicants: AECOM Technical Services, Inc.
- Inventors: James David Colley; Sterling Michael Gray
- Web page: https://patentgrep.com/patent/US20170291137A1

## CPC

- B01D 53/501: {by treating the gases with a solution or a suspension of an alkali or earth-alkali or ammonium compound}
- B01D 53/80: Semi-solid phase processes, i.e. by using slurries
- B01D 2251/404: of calcium
- B01D 2251/606: Carbonates
- B01D 2251/70: Organic acids
- B01D 2258/0283: Flue gases
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)

## Abstract

A flue gas desulfurization unit is converted from operating with lime or magnesium enhanced lime under inhibited oxidation into a unit that operates using limestone under inhibited oxidation conditions. A ball mill grinding unit may be installed to crush the limestone thereby producing a suspended slurry of fine limestone particles which is pumped to the reaction vessel. When installed, the ball mill may be installed in the process immediately downstream of the existing slaking equipment. The suspended solution may be maintained at a pH in the range of 3.0 to 6.5, optimally at approximately 5.0 to increase the dissolution rate of the limestone reagent produced by the ball mill. The post-conversion process may also require the addition of organic acids and oxidation inhibitors to achieve better SO2 removal from the flue gas.

## Claims

### Claim 1

A method for converting an existing lime-based inhibited oxidation SO2 scrubbing process for utility or industrial boilers into limestone-based inhibited oxidation SO2 scrubbing process, comprising:
adding a limestone grinding system an existing lime-based inhibited oxidation SO2 scrubbing system;
grinding limestone in the limestone grinding system;
depositing ground limestone from the limestone grinding system into a slurry; and
pumping the slurry into a flue gas desulfurization reaction vessel wherein the pH is maintained between 3.0 and 6.5.

### Claim 2 (depends on 1)

The method of claim 1, wherein the limestone grinding system is located downstream from an existing slaking unit which pre-crushes the limestone prior to entering the limestone grinding system.

### Claim 3 (depends on 1)

The method of claim 1, wherein the limestone grinding system is a ball mill grinder.

### Claim 4 (depends on 1)

The method of claim 1, wherein the pH in the reaction vessel is maintained between 4.5 and 5.6.

### Claim 5 (depends on 1)

The method of claim 1, wherein the pH in the reaction vessel is maintained at approximately 5.0.

### Claim 6 (depends on 1)

The method of claim 1, further including addition of an organic acid to achieve better SO2 removal from flue gas.

### Claim 7 (depends on 1)

The method of claim 1, further including addition of an organic acid to achieve better SO2 removal from flue gas, wherein the organic acid is one or more of formic, acetic, glycolic, maleic, lactic, adipic, succinic or glutaric.

### Claim 8 (depends on 1)

The method of claim 1, further including addition of an organic acid to achieve better SO2 removal from flue gas, wherein the organic acid is a salt of one or more of formic, acetic, glycolic, maleic, lactic, adipic, succinic or glutaric.

### Claim 9 (depends on 1)

The method of claim 1, further including addition of an organic acid to achieve better SO2 removal from flue gas, wherein the organic acid is adibasic organic acid, such as adipic, malaeic, succinic, glutaric or an analog thereof.

### Claim 10 (depends on 1)

The method of claim 1, further including addition of an organic acid to achieve better SO2 removal from flue gas, wherein the organic acid is a compound based on glycolic acid, such as glycolic acid or any analog thereof.

### Claim 11 (depends on 1)

The method of claim 1, further including addition of an oxidation inhibitor.

### Claim 12 (depends on 1)

The method of claim 1, further including addition of an oxidation inhibitor, wherein the oxidation inhibitor is one or more of sodium thiosulfate, emulsified sulfur or soluble iodide salts.

### Claim 13

A method for converting an existing lime-based inhibited oxidation SO2 scrubbing process for utility or industrial boilers into limestone-based forced oxidation SO2 scrubbing process, comprising:
adding a limestone grinding system to an existing lime-based inhibited oxidation SO2 scrubbing system;
grinding limestone in the limestone grinding system;
depositing the ground limestone into a slurry; and
pumping the slurry into a flue gas desulfurization reaction vessel wherein the pH is maintained between 3.0 and 6.5.

### Claim 14 (depends on 13)

The method of claim 13, wherein the limestone grinding system is located downstream from an existing slaking unit which pre-crushes the limestone prior to entering the limestone grinding system.

### Claim 15 (depends on 13)

The method of claim 13, wherein the pH in the reaction vessel is maintained between 4.5 and 5.6.

### Claim 16 (depends on 13)

The method of claim 13, wherein the pH in the reaction vessel is maintained at approximately 5.0.

### Claim 17

A method for converting an existing lime-based forced oxidation SO2 scrubbing process for utility or industrial boilers into limestone-based forced oxidation SO2 scrubbing process, comprising:
adding a limestone grinding system to an existing lime-based forced oxidation SO2 scrubbing system;
grinding limestone in the limestone grinding system;
depositing ground limestone from the limestone grinding system into a slurry; and
pumping the slurry into a flue gas desulfurization reaction vessel wherein the pH is maintained between 3.0 and 6.5.

### Claim 18 (depends on 17)

The method of claim 17, wherein the limestone grinding system is located downstream from an existing slaking unit which pre-crushes the limestone prior to entering the limestone grinding system.

### Claim 19 (depends on 17)

The method of claim 17, wherein the pH in the reaction vessel is maintained between 4.5 and 5.6.

### Claim 20 (depends on 17)

The method of claim 17, wherein the pH in the reaction vessel is maintained at approximately 5.0.

### Claim 21

A method for converting an existing lime-based forced oxidation SO2 scrubbing process for utility or industrial boilers into limestone-based inhibited oxidation SO2 scrubbing process, comprising:
adding a limestone grinding system to an existing lime-based forced oxidation SO2 scrubbing system;
grinding limestone in the limestone grinding system;
depositing ground limestone from the limestone grinding system into a slurry; and
pumping the slurry into a flue gas desulfurization reaction vessel, wherein the pH in the reaction vessel is maintained between 3.0 and 6.5.

### Claim 22 (depends on 21)

The method of claim 21, wherein the limestone grinding system is located downstream from an existing slaking unit which pre-crushes the limestone prior to entering the limestone grinding system.

### Claim 23 (depends on 21)

The method of claim 21, wherein the pH in the reaction vessel is maintained between 4.5 and 5.6.

### Claim 24 (depends on 21)

The method of claim 21, wherein the pH in the reaction vessel is maintained at approximately 5.0.