# US 2017/0288720 A1 · Electronic product metal shell with an antenna groove and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0288720 A1
- Document ID: US20170288720A1
- Status: Published application
- Kind: A1
- Application number: 15/631,915
- Filed: 2017-06-23
- Published: 2017-10-05
- Earliest claimed: 2014-12-26
- Assignees: BYD Company Limited
- Applicants: BYD Company Limited
- Inventors: BAORONG JIANG; CHONGCHONG LIAO; AIHUA LI; LIANG CHEN
- Web page: https://patentgrep.com/patent/US20170288720A1

## CPC

- H05K 5/04: Metal casings
- C23F 1/28: for etching iron group metals
- H01Q 1/243: {with built-in antennas}
- H04M 1/0202: {Portable telephone sets, e.g. cordless phones, mobile phones or bar type handsets (constructional features of telephone transmitters or receivers, e.g. of speakers or microphones H04M1/03)}
- H04M 1/026: {Details of the structure or mounting of specific components}
- H04M 1/0283: {for providing a decorative aspect, e.g. customization of casings, exchangeable faceplate}
- H05K 3/067: {Etchants}
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- H01Q: ANTENNAS, i.e. RADIO AERIALS (radiators or antennas for microwave heating H05B6/72)
- H04M: TELEPHONIC COMMUNICATION (circuits for controlling other apparatus via a telephone cable and not involving telephone switching apparatus G08)

## Abstract

The present disclosure provides an electronic product metal shell with an antenna groove and a method of manufacturing the same. The electronic product metal shell includes a metal layer, a hard anodic oxidation layer, a step recess, an antenna groove and a non-conductive material filled in the antenna groove. The metal layer may have a first surface and a second surface. The hard anodic oxidation layer may be coated on the first surface and the second surface of the metal layer. The step recess may be formed through the hard anodic oxidation layer on the first surface of the metal layer and partially into the metal layer. The antenna groove may be formed within the step recess extending through the metal layer to expose an inner side of the hard anodic oxidation layer on the second surface of the metal layer.

## Claims

### Claim 1

An electronic product metal shell comprising:
a metal layer having a first surface and a second surface;
a hard anodic oxidation layer coated on the first surface and the second surface of the metal layer;
a step recess formed through the hard anodic oxidation layer on the first surface of the metal layer and partially into the metal layer;
an antenna groove disposed within the step recess and extending through the metal layer to expose an inner side of the hard anodic oxidation layer on the second surface of the metal layer; and
a non-conductive material filled in the antenna groove.

### Claim 2 (depends on 1)

The electronic product metal shell of claim 1, wherein the step recess has a width of about 1.0 centimeter to about 5.0 centimeters and a depth of about 0.1 millimeters to about 0.8 millimeters, preferably a depth of about 0.3 millimeters to about 0.5 millimeters.

### Claim 3 (depends on 1)

The electronic product metal shell of claim 1, wherein an opening of the antenna groove facing a first surface of the electronic product metal shell is defined as an upper opening, the antenna groove has a sectional structure of trapezoid that the upper opening has a size larger than a lower opening of the antenna groove, the upper opening has a width of about 2 millimeters to about 5 millimeters, preferably about 2 millimeters to about 5 millimeters, and the lower opening has a width of about 0.8 millimeters to about 1.4 millimeters, preferably about 0.8 millimeters to about 1.2 millimeters.

### Claim 4 (depends on 1)

The electronic product metal shell of claim 1, wherein the metal layer has a thickness of about 0.5 millimeters to about 1.5 millimeters, and the hard anodic oxidation layer has a thickness of about 0.02 millimeters to about 0.06 millimeters.

### Claim 5 (depends on 1)

The electronic product metal shell of claim 1, wherein the metal layer includes an aluminum alloy layer.

### Claim 6 (depends on 1)

The electronic product metal shell of claim 1, wherein the electronic product metal shell includes a cell phone metal shell or a tablet computer metal shell.

### Claim 7

A method of manufacturing an electronic product metal shell, comprising steps of:
(1) applying a hard anodizing treatment and an ink spraying treatment to a metal layer in sequence, so as to form a hard anodic oxidation layer and an ink layer respectively;
(2) forming a step recess through the hard anodic oxidation layer on a first surface of the metal layer and partially into the metal layer, and an antenna groove disposed within the step recess and extending through the metal layer to expose an inner side of the hard anodic oxidation layer on a second surface of the metal layer;
(3) removing the ink layer; and
(4) filling a non-conductive material in the antenna groove.

### Claim 8 (depends on 7)

The method of claim 7, wherein in step (2), forming the step recess comprises: forming a step recess pattern on the first surface of the metal shell, removing the ink layer and the hard anodic oxidation layer corresponding to the step recess pattern, and removing a first part of the metal layer to obtain the step recess.

### Claim 9 (depends on 8)

The method of claim 8, wherein after removing the first part of the metal layer, the remaining part of the metal layer has a thickness of about 20% to about 80% of an overall thickness of the metal layer.

### Claim 10 (depends on 8)

The method of claim 8, wherein the first part of the meal layer is removed via etching, the etching is carried out under a temperature of about 20 Celsius degrees to about 30 Celsius degrees for about 40 minutes to about 50 minutes, with an etching solution including an aqueous solution having ferric trichloride and hydrochloric acid, and per one liter of the etching solution, the ferric trichloride has a content of about 800 grams to about 1000 grams, and the hydrochloric acid has a content of about 35 grams to about 75 grams.

### Claim 11 (depends on 7)

The method of claim 7, wherein in step (2), forming the antenna groove within the step recess includes: spraying ink on the step recess, forming an antenna groove slit within the step recess to remove the ink corresponding to the antenna groove slit, and removing the metal layer corresponding to the antenna groove slit to expose the inner side of the hard anodic oxidation layer coated on the second surface of the metal layer.

### Claim 12 (depends on 11)

The method of claim 11, wherein spraying ink includes: spraying a UV ink to form an ink layer having a thickness of about 30 microns to about 60 microns, then baking the electronic product metal shell under about 110 Celsius degrees to about 120 Celsius degrees for about 20 minutes to about 30 minutes, and exposing the electronic product metal shell under ultraviolet ray for about 1 minute to about 2 minutes.

### Claim 13 (depends on 11)

The method of claim 11, wherein the antenna groove slit formed has a width of about 0.02 millimeters to about 0.1 millimeters.

### Claim 14 (depends on 11)

The method of claim 11, wherein the metal layer corresponding to the antenna groove slit is removed via etching, the etching is carried out under a temperature of about 20 Celsius degrees to about 30 Celsius degrees for about 40 minutes to about 50 minutes, with an etching solution including an aqueous solution having ferric trichloride and hydrochloric acid, and per one liter of the etching solution, the ferric trichloride has a content of about 800 grams to about 1000 grams, and the hydrochloric acid has a content of about 35 grams to about 75 grams.

### Claim 15 (depends on 7)

The method of claim 7, wherein in step (1), the hard anodizing treatment comprises: applying an alkaline etching treatment, a desmutting treatment, a oxidizing treatment and a sealing treatment to the metal layer in sequence, and washing the metal layer after each one of the alkaline etching treatment, the desmutting treatment, the oxidizing treatment and the sealing treatment respectively, preferably, the oxidizing treatment is carried out under a condition of: a temperature of about 5 Celsius degrees to about 12 Celsius degrees for about 30 minutes to about 50 minutes, an impulse waveform of positive square wave pulse, a duty ratio of about 50% to about 90%, a frequency of about 500 Hz to about 1000 Hz, a current density of about 2 A/dm2 to about 7 A/dm2, an oxidant solution including an aqueous solution of sulfuric acid, oxalic acid/malic acid, wherein per 1 liter of the oxidant solution, the sulfuric acid has a content of about 120 grams to 220 grams, the oxalic acid or the malic acid has a content of about 8 grams to about 20 grams.

### Claim 16 (depends on 7)

The method of claim 7, wherein in step (1), the ink spraying treatment comprises:
spraying a UV ink to form a ink layer having a thickness of about 40 microns to about 60 microns, baking the electronic product metal shell under about 110 Celsius degrees to about 120 Celsius degrees for about 20 minutes to about 30 minutes, and exposing the electronic product metal shell under ultraviolet ray for about 1 minute to about 2 minutes.

### Claim 17 (depends on 7)

The method of claim 7, wherein in step (3), the ink layer is removed by a neutral paint remover.

### Claim 18 (depends on 7)

The method of claim 7, wherein in step (4), the non-conductive material includes at least one selected from a group consisting of UV glue, thermal curing glue, and cold setting adhesive.

### Claim 19 (depends on 7)

The method of claim 7, wherein the metal layer includes an aluminum alloy layer.

### Claim 20 (depends on 7)

The method of claim 7, wherein the electronic product metal shell includes a cell phone metal shell or a tablet computer metal shell.