# US 2017/0288628 A1 · Acoustic resonator including monolithic piezoelectric layer having opposite polarities

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0288628 A1
- Document ID: US20170288628A1
- Status: Published application
- Kind: A1
- Application number: 15/086,397
- Filed: 2016-03-31
- Published: 2017-10-05
- Earliest claimed: 2016-03-31
- Assignees: Avago Technologies General IP (Singapore) Pte. Ltd.
- Applicants: Avago Technologies General IP (Singapore) Pte. Ltd.
- Inventors: Kevin J. Grannen; Chris Feng; John Choy
- Web page: https://patentgrep.com/patent/US20170288628A1

## CPC

- H03H 3/02: for the manufacture of piezoelectric or electrostrictive resonators or networks (H03H3/08 takes precedence)
- C23C 14/0057: {using reactive gases other than O2, H2O, N2, NH3 or CH4}
- C23C 14/0617: {AIII BV compounds, where A is Al, Ga, In or Tl and B is N, P, As, Sb or Bi}
- C23C 14/0641: {Nitrides (C23C14/0617 takes precedence)}
- C23C 14/165: {by cathodic sputtering}
- H03H 2003/021: {the resonators or networks being of the air-gap type}
- H03H: IMPEDANCE NETWORKS, e.g. RESONANT CIRCUITS; RESONATORS (waveguides, resonators, lines or other devices of the waveguide type H01P)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A method is provided for forming a piezoelectric layer during a corresponding deposition sequence. The method includes sputtering aluminum nitride onto a sputtering substrate inside a reaction chamber having a gas atmosphere, the gas atmosphere initially including nitrogen gas and an inert gas, causing growth of the piezoelectric layer with a polarity in a negative direction. The method further includes adding a predetermined amount of oxygen containing gas to the gas atmosphere over a predetermined period of time, while continuing the sputtering of the aluminum nitride onto the sputtering substrate during a remainder of the deposition sequence, such that the piezoelectric layer is monolithic. The predetermined amount of oxygen containing gas causes the polarity of the aluminum nitride piezoelectric layer to invert from the negative direction to a positive direction, opposite the negative direction.

## Claims

### Claim 1

A method of forming a piezoelectric layer during a corresponding deposition sequence, the method comprising:
sputtering aluminum nitride (AlN) onto a sputtering substrate inside a reaction chamber having a gas atmosphere, the gas atmosphere initially comprising nitrogen (N2) gas and an inert gas, causing growth of the piezoelectric layer with a polarity in a negative direction; and
adding a predetermined amount of diatomic or triatomic oxygen containing gas to the gas atmosphere over a predetermined period of time, while continuing the sputtering of the aluminum nitride (AlN) onto the sputtering substrate during a remainder of the deposition sequence, such that the piezoelectric layer is monolithic,
wherein the predetermined amount of oxygen containing gas causes the polarity of the aluminum nitride (AlN) piezoelectric layer to invert from the negative direction to a positive direction, opposite the negative direction.

### Claim 2 (depends on 1)

The method of claim 1, wherein there is no discernible interface in the piezoelectric layer where the polarity of the piezoelectric layer inverts from the negative direction to the positive direction.

### Claim 3 (depends on 1)

The method of claim 1, wherein the inert gas comprises argon (Ar) gas.

### Claim 4 (depends on 1)

The method of claim 1, the oxygen containing gas comprises oxygen (O2) gas or ozone (O3) gas.

### Claim 5 (depends on 4)

The method of claim 4, wherein the predetermined amount of oxygen containing gas added to the gas atmosphere is in a range from about 50 micromoles to about 5millimoles.

### Claim 6 (depends on 5)

The method of claim 5, wherein the predetermined period of time during which the predetermined amount of oxygen containing gas is added to the gas atmosphere is in a range from about one (1) second to about sixty (60) seconds.

### Claim 7 (depends on 1)

The method of claim 1, wherein the polarity in the negative direction is directed substantially toward the sputtering substrate, and the polarity in the positive direction is directed substantially away from the sputtering substrate.

### Claim 8 (depends on 1)

The method of claim 1, wherein the sputtering substrate is formed of one of molybdenum (Mo) or tungsten (W).

### Claim 9 (depends on 1)

The method of claim 1, wherein the predetermined amount of oxygen containing gas is added to cause the polarity of the piezoelectric layer to invert approximately half way through the deposition sequence, such that half of the monolithic piezoelectric layer has the polarity in the negative direction and half of the monolithic piezoelectric layer has the polarity in the positive direction.

### Claim 10

A method of forming a bulk acoustic wave (BAW) resonator, comprising:
depositing a first electrode layer over a resonator substrate and an acoustic reflector;
depositing a monolithic piezoelectric layer on the first electrode layer during a deposition sequence, wherein depositing the piezoelectric layer comprises:
sputtering aluminum nitride (AlN) on the first electrode layer inside a reaction chamber having a gas atmosphere, the gas atmosphere initially comprising nitrogen (N2) gas and argon (Ar) gas, causing growth of the piezoelectric layer with a polarity in a negative direction; and
adding a predetermined amount of oxygen gas to the gas atmosphere over a predetermined period of time, while continuing the sputtering of the aluminum nitride (AlN) onto the first electrode layer during a remainder of the deposition sequence, such that the piezoelectric layer is monolithic, wherein the predetermined amount of oxygen gas causes the polarity of the piezoelectric layer to invert from the negative direction to a positive direction, opposite the negative direction; and
depositing a second electrode layer over the monolithic piezoelectric layer.

### Claim 11 (depends on 10)

The method of claim 10, wherein adding the predetermined amount of oxygen gas causes the polarity of the monolithic piezoelectric layer to invert at half way through the deposition sequence, such that a first half of the monolithic piezoelectric layer has the polarity in the negative direction and a second half of the monolithic piezoelectric layer has the polarity in the positive direction.

### Claim 12 (depends on 11)

The method of claim 11, wherein the monolithic piezoelectric layer, having the first half with the polarity in the negative direction and the second half with the polarity in the positive direction, causes the BAW resonator to resonate at a second harmonic of a resonance frequency of the BAW resonator, as opposed to a first harmonic of the resonance frequency.

### Claim 13 (depends on 12)

The method of claim 12, wherein by resonating at the second harmonic, the BAW resonator resonates at a frequency over twice the resonance frequency of a BAW resonator without a monolithic piezoelectric layer having different polarities, but having a piezoelectric layer with the same thickness.

### Claim 14 (depends on 10)

The method of claim 10, wherein the acoustic reflector comprises an air cavity formed in the substrate.

### Claim 15 (depends on 10)

The method of claim 10, wherein the acoustic reflector comprises a distributed Bragg reflector (DBR).

### Claim 16 (depends on 10)

The method of claim 10, wherein the polarity in the negative direction is directed substantially toward the first electrode layer, and the polarity in the positive direction is directed substantially away from the first electrode layer.

### Claim 17

A method of forming a piezoelectric layer of aluminum nitride (AlN), doped with a rare earth element, during a corresponding deposition sequence, the method comprising:
sputtering aluminum nitride (AlN) and the rare earth element onto a metal sputtering substrate inside a reaction chamber having a gas atmosphere, the gas atmosphere initially comprising nitrogen (N2) gas and argon (Ar) gas, causing growth of the piezoelectric layer with a negative polarity; and
adding a predetermined amount of oxygen containing gas to the gas atmosphere over a predetermined period of time, while continuing the sputtering of the aluminum nitride (AlN) and the rare earth element onto the metal sputtering substrate during a remainder of the deposition sequence, such that the piezoelectric layer is monolithic,
wherein the predetermined amount of oxygen containing gas causes the negative polarity of the piezoelectric layer to invert to a positive polarity, opposite the negative polarity, at half way through the deposition sequence, such that a first half of the piezoelectric layer has the negative polarity and a second half of the monolithic piezoelectric layer has the positive polarity.

### Claim 18 (depends on 17)

The method of claim 17, wherein the rare earth element comprises scandium (Sc).

### Claim 19 (depends on 17)

The method of claim 17, wherein the negative polarity is in a negative direction directed substantially toward the metal sputtering substrate, and the positive polarity in a positive direction directed substantially away from the metal sputtering substrate.

### Claim 20 (depends on 17)

The method of claim 17, wherein the oxygen containing gas comprises oxygen (O2) gas or ozone (O3) gas.