# US 2017/0288276 A1 · Method for Producing a Lithium-Ion Cell

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0288276 A1
- Document ID: US20170288276A1
- Status: Published application
- Kind: A1
- Application number: 15/625,159
- Filed: 2017-06-16
- Published: 2017-10-05
- Earliest claimed: 2014-12-18
- Assignees: Bayerische Motoren Werke Aktiengesellschaft
- Applicants: Bayerische Motoren Werke Aktiengesellschaft
- Inventors: Nikolaos TSIOUVARAS; Thomas WOEHRLE
- Web page: https://patentgrep.com/patent/US20170288276A1

## CPC

- H01M 10/0587: of accumulators having only wound construction elements, i.e. wound positive electrodes, wound negative electrodes and wound separators
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/0416: {involving impregnation with a solution, dispersion, paste or dry powder (H01M4/0438 takes precedence)}
- H01M 4/0435: {Rolling or calendering}
- H01M 4/139: Processes of manufacture
- H01M 10/0431: {Cells with wound or folded electrodes (H01M10/045 takes precedence)}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0583: of accumulators with folded construction elements except wound ones, i.e. folded positive or negative electrodes or separators, e.g. with "Z"-shaped electrodes or separators
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for producing a lithium-ion cell is provided. The electrochemically active coating of an electrode is brought into contact with an electrolyte or an auxiliary liquid before a winding or cutting operation. This method is suitable in particular for continuously producing lithium-ion cells by means of processes proceeding at high speed, such as winding processes.

## Claims

### Claim 1

A method for producing a lithium-ion cell, comprising the following steps:
A) providing a first electrode having a first electrode collector and a first electrochemically active coating applied onto the first electrode collector, and a second electrode having a second electrode collector and a second electrochemically active coating applied onto the second electrode collector,
B) contacting at least part of the first and/or second electrochemically active coating with an electrolyte,
C) cutting, winding and/or folding the first and/or second electrode, wherein step C) is carried out after step B), and
D) combining the first electrode with a separator and the second electrode.

### Claim 2 (depends on 1)

The method according to claim 1, wherein step C) is carried out before and/or after step D).

### Claim 3 (depends on 1)

The method according to claim 1, wherein after the contacting in step B), the part of the first and/or second electrochemically active coating has the electrolyte in a volume fraction of at most 60% in relation to the total volume of the part of the first and/or second electrochemically active coating.

### Claim 4 (depends on 1)

The method according to claim 1, wherein after the contacting in step B), the part of the first and/or second electrochemically active coating has the electrolyte in a volume fraction of at least 10% in relation to the total volume of the part of the first and/or second electrochemically active coating.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the electrolyte comprises an organic carbonate.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the first and/or second electrochemically active coating has a layer thickness of at least 75 μm.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the first and/or second electrode is coherent in sheet form in a longitudinal direction.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the first and/or second electrode is conveyed in step C) along the longitudinal direction at a speed of at least 5 m/min.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the first and/or second electrochemically active coating contains no plasticizer.

### Claim 10

A method for producing a lithium-ion cell, comprising the following steps:
A′) providing a first electrode having a first electrode collector and a first electrochemically active coating applied onto the first electrode collector, and a second electrode having a second electrode collector and a second electrochemically active coating applied onto the second electrode collector,
B′) contacting at least part of the first and/or second electrochemically active coating with an auxiliary liquid,
C′) cutting, winding and/or folding the first and/or second electrode, wherein step C′) is carried out after step B′),
D′) combining the first electrode with a separator and the second electrode, and
E′) supplying an electrolyte.

### Claim 11 (depends on 10)

The method according to claim 10, wherein step C′) is carried out before and/or after step D′).

### Claim 12 (depends on 10)

The method according to claim 10, wherein after the contacting in step B′), the part of the first and/or second electrochemically active coating has the auxiliary liquid in a volume fraction of at most 60% in relation to the total volume of the part of the first and/or second electrochemically active coating.

### Claim 13 (depends on 10)

The method according to claim 10, wherein after the contacting in step B′), the part of the first and/or second electrochemically active coating has the auxiliary liquid in a volume fraction of at least 10% in relation to the total volume of the part of the first and/or second electrochemically active coating.

### Claim 14 (depends on 10)

The method according to claim 10, wherein the auxiliary liquid has a boiling point of at most 120° C. under chemical standard conditions.

### Claim 15 (depends on 10)

The method according to claim 10, wherein the auxiliary liquid is anhydrous and/or aprotic.

### Claim 16 (depends on 10)

The method according to claim 10, wherein the first and/or second electrochemically active coating has a layer thickness of at least 75 μm.

### Claim 17 (depends on 10)

The method according to claim 10, wherein the first and/or second electrode is coherent in sheet form in a longitudinal direction.

### Claim 18 (depends on 17)

The method according to claim 17, wherein the first and/or second electrode is conveyed in step C′) along the longitudinal direction at a speed of at least 5 m/min.

### Claim 19 (depends on 10)

The method according to claim 10, wherein the first and/or second electrochemically active coating contains no plasticizer.