# US 2017/0288222 A1 · Method of producing positive electrode active material for nonaqueous electrolyte secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0288222 A1
- Document ID: US20170288222A1
- Status: Published application
- Kind: A1
- Application number: 15/474,584
- Filed: 2017-03-30
- Published: 2017-10-05
- Earliest claimed: 2016-03-31
- Assignees: Nichia Corporation
- Applicants: Nichia Corporation
- Inventors: Kenichi KOBAYASHI
- Web page: https://patentgrep.com/patent/US20170288222A1

## CPC

- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- C01G 53/40: Complex oxides containing nickel and at least one other metal element
- C01G 53/504: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.5, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.5
- C01G 53/506: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.8, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.8
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- C01P 2004/03: obtained by SEM
- C01P 2004/51: Particles with a specific particle size distribution
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/40: Electric properties
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method of producing a positive electrode active material for a nonaqueous electrolyte secondary battery, the method includes preparing nickel-containing composite oxide particles having a ratio 1D90/1D10 of a 90% particle size 1D90 to a 10% particle size 1D10 in volume-based cumulative particle size distribution of 3 or less; obtaining a raw material mixture containing the composite oxide particles and a lithium compound and having a ratio of a total number of moles of lithium to a total number of moles of metal elements contained in the composite oxide in a range of 1 to 1.3; subjecting the raw material mixture to a heat treatment to obtain a heat-treated material; subjecting the heat-treated material to a dry-dispersion treatment to obtain a first dispersion; and bringing the first dispersion into contact with a liquid medium to obtain a second dispersion.

## Claims

### Claim 1

A method of producing a positive electrode active material for a nonaqueous electrolyte secondary battery, comprising:
preparing nickel-containing composite oxide particles having a ratio 1D90/1D10 of a 90% particle size 1D90 to a 10% particle size 1D10 in volume-based cumulative particle size distribution of 3 or less;
obtaining a raw material mixture containing the composite oxide particles and a lithium compound and having a ratio of a total number of moles of lithium to a total number of moles of metal elements contained in the composite oxide in a range of 1 to 1.3;
subjecting the raw material mixture to a heat treatment to obtain a heat-treated material;
subjecting the heat-treated material to a dry-dispersion treatment to obtain a first dispersion; and
bringing the first dispersion into contact with a liquid medium to obtain a second dispersion,
wherein the positive electrode active material includes lithium-transition metal composite oxide particles having a ratio 2D50/2DSEM of a 50% particle size 2D50 in volume-based cumulative particle size distribution to an average particle size 2DSEM based on electron microscopic observation in a range of 1 to 4, and
wherein the lithium-transition metal composite oxide particles have a composition represented by the following formula (1):
LipNixCoyM1zO2+α (1)
wherein p, x, y, z, and α satisfy 1.0≦p≦1.3, 0.6≦x<0.95, 0≦y≦0.4, 0≦z≦0.5, x+y÷z=1, and −0.1≦α≦0.1, and M1 represents at least one of Mn and Al.

### Claim 2 (depends on 1)

The method according to claim 1, wherein p in formula (1) satisfies 1.0≦p≦1.1.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the lithium-transition metal composite oxide particles have a ratio 2D90/2D10 of a 90% particle size 2D90 to a 10% particle size 2D10 in volume-based cumulative particle size distribution of 4 or less.

### Claim 4 (depends on 2)

The method according to claim 2, wherein the lithium-transition metal composite oxide particles have a ratio 2D90/2D10 of a 90% particle size 2D90 to a 10% particle size 2D10 in volume-based cumulative particle size distribution of 4 or less.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the heat treatment of the raw material mixture includes heat-treating at a first temperature and heat-treating at a second temperature higher than the first temperature.

### Claim 6 (depends on 2)

The method according to claim 2, wherein the heat treatment of the raw material mixture includes heat-treating at a first temperature and heat-treating at a second temperature higher than the first temperature.

### Claim 7 (depends on 3)

The method according to claim 3, wherein the heat treatment of the raw material mixture includes heat-treating at a first temperature and heat-treating at a second temperature higher than the first temperature.

### Claim 8 (depends on 4)

The method according to claim 4, wherein the heat treatment of the raw material mixture includes heat-treating at a first temperature and heat-treating at a second temperature higher than the first temperature.

### Claim 9 (depends on 5)

The method according to claim 5, wherein the heat treatment of the raw material mixture further includes, after heat-treating at the second temperature, heat-treating at a third temperature lower than the second temperature.

### Claim 10 (depends on 6)

The method according to claim 6, wherein the heat treatment of the raw material mixture further includes, after heat-treating at the second temperature, heat-treating at a third temperature lower than the second temperature.

### Claim 11 (depends on 7)

The method according to claim 7, wherein the heat treatment of the raw material mixture further includes, after heat-treating at the second temperature, heat-treating at a third temperature lower than the second temperature.

### Claim 12 (depends on 8)

The method according to claim 8, wherein the heat treatment of the raw material mixture further includes, after heat-treating at the second temperature, heat-treating at a third temperature lower than the second temperature.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the heat treatment of the raw material mixture is performed in an oxygen-containing atmosphere.

### Claim 14 (depends on 1)

The method according to claim 1, wherein, in the step of bringing the first dispersion into contact with a liquid medium, the mass ratio of the liquid medium to the first dispersion in a range of 2 mass % to 20 mass %.

### Claim 15 (depends on 1)

The method according to claim 1, wherein the lithium-transition metal composite oxide particles have a ratio 2D90/2D10 of the 90% particle size 2D90 to the 10% particle size 2D10 in volume-based cumulative particle size distribution of 4 or less.

### Claim 16 (depends on 1)

The method according to claim 1, wherein the ratio 2D50/2DSEM of the 2D50 to the 2DSEM is in a range of 1 to 3.