# US 2017/0288204 A1 · Method for making battery slurry

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0288204 A1
- Document ID: US20170288204A1
- Status: Published application
- Kind: A1
- Application number: 15/625,584
- Filed: 2017-06-16
- Published: 2017-10-05
- Earliest claimed: 2014-12-16
- Assignees: Jiangsu Huadong Institute of Li-Ion Battery Co., Ltd.; Tsinghua University
- Applicants: Jiangsu Huadong Institute of Li-Ion Battery Co., Ltd.; Tsinghua University
- Inventors: Xiang-Ming He; Hong-Sheng Zhang; Jian-Jun Li; Li Wang; Yu-Ming Shang; Guan-Nan Qian
- Web page: https://patentgrep.com/patent/US20170288204A1

## CPC

- H01M 4/04: Processes of manufacture in general
- H01M 4/139: Processes of manufacture
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for making a battery slurry is disclosed. The method comprises providing a plurality of solid raw materials and at least one liquid raw material, the at least one liquid raw material is divided into a first part solvent and a second part solvent to be used; mixing the plurality of solid raw materials to obtain a dry powder; kneading the dry powder and the first part solvent to obtain a doughy mixture; and dispersing the doughy mixture to the second part solvent to obtain the battery slurry.

## Claims

### Claim 1

A method for making a battery slurry, comprising:
providing a plurality of solid raw materials and at least one liquid raw material, the at least one liquid raw material comprising a first part solvent and a second part solvent;
mixing the plurality of solid raw materials to obtain a dry powder;
kneading the dry powder and the first part solvent to obtain a doughy mixture; and
dispersing the doughy mixture to the second part solvent to obtain the battery slurry.

### Claim 2 (depends on 1)

The method of claim 1, wherein the plurality of solid raw materials are mixed in a vacuum environment.

### Claim 3 (depends on 2)

The method of claim 2, wherein the plurality of solid raw materials are mixed at a temperature range from about 30° C. to about 150° C.

### Claim 4 (depends on 2)

The method of claim 2, wherein the plurality of solid raw materials are mixed for a period of about 30 minutes to about 120 minutes

### Claim 5 (depends on 1)

The method of claim 1, wherein a mass ratio of the dry powder to the first part solvent is in a range from about 1:9 to about 1:1.

### Claim 6 (depends on 1)

The method of claim 1, wherein the dry powder and the first part solvent are kneaded in a vacuum environment.

### Claim 7 (depends on 6)

The method of claim 6, wherein a vacuum pressure of the vacuum environment is lower than −0.09 MPa.

### Claim 8 (depends on 6)

The method of claim 6, wherein the dry powder and the first part solvent are kneaded at a temperature range from about 25° C. to about 45° C.

### Claim 9 (depends on 6)

The method of claim 6, wherein the dry powder and the first part solvent are kneaded for a period of about 30 minutes to about 120 minutes.

### Claim 10 (depends on 1)

The method of claim 1, wherein the doughy mixture is dispersed to the second part solvent by stirring at a speed greater than or equal to about 15 m/s.

### Claim 11 (depends on 10)

The method of claim 10, wherein the speed is in a range from about 15 m/s to about 70 m/s.

### Claim 12 (depends on 10)

The method of claim 10, wherein the doughy mixture and the second part solvent are dispersed for a period of about 5 minutes to about 30 minutes.

### Claim 13 (depends on 1)

The method of claim 1, wherein the doughy mixture and the second part solvent are dispersed at a temperature range from about 25° C. to about 45° C.

### Claim 14 (depends on 1)

The method of claim 1, wherein a component of the first part solvent is the same as a component of the second part solvent.

### Claim 15 (depends on 1)

The method of claim 1, wherein the battery slurry is an electrode slurry of the lithium ion battery, the plurality of solid raw materials comprise an active material, a conducting agent, and a binder, and at least one liquid raw materials can be at least one of N-methyl-2-pyrrolidone (NMP), N,N-dimethyl formamide (DMF), N,N-diethyl formamide (DEF), dimethyl sulfoxide (DMSO), tetrahydrofuran (THF), acetone, ethanol, and deionized water.