# US 2017/0288200 A1 · Battery connection sheet and method for preparing the same, battery connection assembly, battery module, battery package and electric vehicle

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0288200 A1
- Document ID: US20170288200A1
- Status: Published application
- Kind: A1
- Application number: 15/626,381
- Filed: 2017-06-19
- Published: 2017-10-05
- Earliest claimed: 2014-12-23
- Assignees: BYD Company Limited
- Applicants: BYD Company Limited
- Inventors: QINGBO PENG; WEIXIN ZHENG; ZHIPEI LU; YAN ZHU; JIANHUA ZHU
- Web page: https://patentgrep.com/patent/US20170288200A1

## CPC

- B23K 20/233: without ferrous layer
- B23K 20/06: by means of high energy impulses, e.g. magnetic energy
- B23K 20/2336: {both layers being aluminium}
- H01M 50/503: characterised by the shape of the interconnectors
- H01M 50/509: characterised by the type of connection, e.g. mixed connections
- H01R 4/625: {Soldered or welded connections}
- H01R 31/06: Intermediate parts for linking two coupling parts, e.g. adapter (with a holder adapted for supporting apparatus to which its counterpart is attached H01R33/94)
- H01R 43/0207: {Ultrasonic-, H.F.-, cold- or impact welding}
- B23K 2101/36: Electric or electronic devices
- B23K 2103/10: Aluminium or alloys thereof
- B23K 2103/12: Copper or alloys thereof
- H01M 2220/20: Batteries in motive systems, e.g. vehicle, ship, plane
- H01R 11/288: {Interconnections between batteries}
- Y02E 60/10: Energy storage using batteries
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01R: ELECTRICALLY-CONDUCTIVE CONNECTIONS; STRUCTURAL ASSOCIATIONS OF A PLURALITY OF MUTUALLY-INSULATED ELECTRICAL CONNECTING ELEMENTS; COUPLING DEVICES; CURRENT COLLECTORS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present disclosure discloses a battery connection sheet, including: a first part, including a first metal sheet, a first buffer portion and a first connection portion, and a second part, including a second metal sheet connected with the first connection portion via electromagnetic pulse welding.

## Claims

### Claim 1

A battery connection sheet, comprising:
a first part, comprising a first metal sheet, a first buffer portion and a first connection portion, and
a second part, comprising a second metal sheet connected with the first connection portion via electromagnetic pulse welding.

### Claim 2 (depends on 1)

The battery connection sheet according to claim 1, the first part is of an integral structure, and the first buffer portion is located between the first metal sheet and the first connection portion.

### Claim 3 (depends on 1)

The battery connection sheet according to claim 1, wherein the first buffer portion has a sinusoidal shape.

### Claim 4 (depends on 3)

The battery connection sheet according to claim 3, wherein the first buffer portion comprises:
a first end, connected to the first metal sheet,
a second end, connected to the first connection portion,
a first wave trough, close to the first end, and
a first wave crest, located between the first wave trough and the second end.

### Claim 5 (depends on 4)

The battery connection sheet according to claim 4, wherein the first buffer portion has a thickness thereof decreasing gradually from the first end to the first wave trough, and decreasing gradually from the second end to the first wave crest.

### Claim 6 (depends on 4)

The battery connection sheet according to claim 4, wherein the first end, the second end, the first metal sheet and the first connection portion have a same thickness.

### Claim 7 (depends on 4)

The battery connection sheet according to claim 4, wherein the first wave trough has a thickness of about 25% to about 35% based on a thickness of the first metal sheet, the first wave crest has a thickness of about 25% to about 35% based on the thickness of the first metal sheet, and the first buffer portion has a span of about 100% to about 400% based on the thickness of the first metal sheet.

### Claim 8 (depends on 1)

The battery connection sheet according to claim 1, wherein the first connection portion comprises a first sidestep at an end thereof with a first recess, the second metal sheet comprises a second sidestep at an end thereof with a second recess, and the first sidestep and the second sidestep are engaged to each other.

### Claim 9 (depends on 8)

The battery connection sheet according to claim 8, wherein a depth of the first recess is the same as a thickness of the second sidestep, and a depth of the second recess is the same as a thickness of the first sidestep.

### Claim 10 (depends on 1)

The battery connection sheet according to claim 1, wherein a surface of the first connection portion contacted to the second metal sheet has no transition layer thereon.

### Claim 11 (depends on 1)

The battery connection sheet according to claim 1, wherein the first metal sheet is configured with at least one mounting hole, and the second metal sheet is configured with at least one mounting hole.

### Claim 12

A method for preparing a battery connection sheet, comprising:
providing a first part having a first metal sheet, a first buffer portion and a first connection portion,
providing a second part having a second metal sheet,
obtaining a connection between the second metal sheet and the first connection portion through electromagnetic pulse welding the first part or the second part.

### Claim 13 (depends on 12)

The method according to claim 12, further comprising
providing a first sidestep at an end of the first connection portion with a first recess, and
providing a second sidestep at an end of the second metal sheet with a second recess;
wherein the electromagnetic pulse welding is performed at the first sidestep or the second sidestep.

### Claim 14 (depends on 12)

The method according to claim 12, wherein the first buffer portion is formed by stretching to obtain a sinusoidal shape.

### Claim 15 (depends on 12)

The method according to claim 12, wherein the first part and the second part are made of different metals.

### Claim 16 (depends on 12)

The method according to claim 12, wherein the first metal sheet, the first buffer portion and the first connection portion are made of a same metal.

### Claim 17 (depends on 12)

The method according to claim 12, wherein each of the first metal sheet, the first buffer portion, the first connection portion and the second metal sheet is made of at least one material selected from a group consisting of copper, copper alloy, aluminum, and aluminum alloy respectively.

### Claim 18 (depends on 12)

The method according to claim 12, further comprising:
molding at least one mounting hole at the first metal sheet, and
molding at least one mounting hole at the second metal sheet.

### Claim 19

A battery connection assembly, comprising:
a plurality of connection bodies, and
a plurality of connection metal sheets, configured to connect the plurality of connection bodies, each comprising:
two second connection portions at two ends thereof respectively, and
a second buffer portion between the two second connection portions;
wherein the connection body comprises a first part which includes a first metal sheet, a first buffer portion and a first connection portion, and a second part which includes a second metal sheet connected with the first connection portion via electromagnetic pulse welding; and
the connection body is contacted with the second connection portion of the connection metal sheet via electromagnetic pulse welding.

### Claim 20 (depends on 19)

The battery connection assembly according to claim 19, wherein the second buffer portion has a sinusoidal shape, the second buffer portion comprises a second wave trough and a second wave crest, and the second buffer portion has a thickness decreasing gradually from one end to the second wave trough, and decreasing gradually from another end to the second wave crest.