# US 2017/0288145 A1 · Method of forming a graphene structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0288145 A1
- Document ID: US20170288145A1
- Status: Published application
- Kind: A1
- Application number: 15/626,234
- Filed: 2017-06-19
- Published: 2017-10-05
- Earliest claimed: 2014-12-31
- Assignees: Infineon Technologies AG
- Applicants: Infineon Technologies AG
- Inventors: Hans-Joachim Schulze; Peter Irsigler; Guenther Ruhl
- Web page: https://patentgrep.com/patent/US20170288145A1

## CPC

- H10K 85/221: {Carbon nanotubes}
- C01B 32/16: Preparation
- C01B 32/184: Preparation
- C01B 32/188: by epitaxial growth
- H10D 30/01: Manufacture or treatment
- H10D 30/014: {of FETs having zero-dimensional [0D] or one-dimensional [1D] channels, e.g. quantum wire FETs, single-electron transistors [SET] or Coulomb blockade transistors}
- H10D 30/43: having one-dimensional [1D] charge carrier gas channels, e.g. quantum wire FETs or transistors having 1D quantum-confined channels
- H10D 30/472: {having lower bandgap active layer formed on top of wider bandgap layer, e.g. inverted HEMT}
- H10D 62/122: {oriented at angles to substrates, e.g. perpendicular to substrates}
- H10D 62/123: {comprising junctions}
- H10D 62/8303: {Diamond}
- H10D 62/882: {Graphene}
- H10K 71/10: Deposition of organic active material
- H10K 71/40: Thermal treatment, e.g. annealing in the presence of a solvent vapour
- H10K 71/80: using temporary substrates
- H10P 14/20: of semiconductor materials
- H10P 14/2902: {being Group IVA materials}
- H10P 14/2904: {Silicon carbide}
- H10P 14/2925: {Surface structures}
- H10P 14/3406: {Carbon, e.g. diamond-like carbon}
- H10P 14/3451: {Structure}
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 40/00: Manufacture or treatment of nanostructures
- H10K 10/484: {characterised by the channel regions}
- H10K 10/491: {Vertical transistors, e.g. vertical carbon nanotube field effect transistors [CNT-FETs]}
- Y10S 977/742: Carbon nanotubes, CNTs
- Y10S 977/842: for carbon nanotubes or fullerenes
- Y10S 977/932: for electronic or optoelectronic application
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

In various embodiments, a method of forming a graphene structure is provided. The method may include forming a body including at least one protrusion, and forming a graphene layer at an outer peripheral surface of the at least one protrusion.

## Claims

### Claim 1

A method of forming a graphene structure, comprising:
forming at least one opening in a body; and
forming a graphene layer at an inner peripheral surface of the at least one opening.

### Claim 2 (depends on 1)

The method of claim 1, further comprising at least partially removing the body from an outer peripheral surface of the graphene layer.

### Claim 3 (depends on 1)

The method of claim 1,
wherein the body comprises silicon carbide.

### Claim 4 (depends on 3)

The method of claim 3, wherein forming the graphene layer at the inner peripheral surface of the at least one opening comprises annealing the body so that the graphene layer forms at an inner peripheral surface of the at least one opening.

### Claim 5 (depends on 4)

The method of claim 4, wherein process parameters of the annealing comprise at least one of an annealing temperature, an annealing duration, an atmospheric pressure, and constituents of the atmosphere.

### Claim 6 (depends on 4)

The method of claim 4, wherein an annealing temperature is in a range from about 1150° C. to about 1800° C.

### Claim 7 (depends on 4)

The method of claim 4, wherein an annealing duration is in a range from about 5 minutes to about 60 minutes.

### Claim 8 (depends on 1)

The method of claim 1, wherein the graphene layer is a closed surface.

### Claim 9 (depends on 1)

The method of claim 1, wherein the graphene layer is a carbon nanotube.

### Claim 10 (depends on 9)

The method of claim 9, wherein the carbon nanotube is unfilled.

### Claim 11 (depends on 2)

The method of claim 2, wherein at least partially removing the body from an outer peripheral surface of the graphene layer comprises etching the body.

### Claim 12 (depends on 1)

The method of claim 1, comprising removing the graphene layer from the body.

### Claim 13

A method of forming a graphene structure, comprising:
forming at least one cylindrical opening in a body, wherein a diameter of the opening is chosen to fulfill a relation d=78.3□((n+m)2−n×m)0.5 pm, wherein n and m are integer values, at least one of n and m being greater than 0; and
forming a graphene layer at an inner peripheral surface of the at least one opening.

### Claim 14 (depends on 13)

The method of claim 13, further comprising at least partially removing the body from an outer peripheral surface of the graphene layer.

### Claim 15 (depends on 14)

The method of claim 14, wherein at least partially removing the body from an outer peripheral surface of the graphene layer comprises etching the body.

### Claim 16 (depends on 13)

The method of claim 13,
wherein the body comprises silicon carbide.

### Claim 17 (depends on 16)

The method of claim 16, wherein forming the graphene layer at the inner peripheral surface of the at least one opening comprises annealing the body so that the graphene layer forms at an inner peripheral surface of the at least one opening.

### Claim 18 (depends on 13)

The method of claim 13, wherein the graphene layer is a carbon nanotube.