# US 2017/0287794 A1 · Methods for manufacturing semiconductor device and for detecting end point of dry etching

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0287794 A1
- Document ID: US20170287794A1
- Status: Published application
- Kind: A1
- Application number: 15/630,385
- Filed: 2017-06-22
- Published: 2017-10-05
- Earliest claimed: 2015-08-27
- Assignees: Renesas Electronics Corporation
- Applicants: Renesas Electronics Corporation
- Inventors: Toshikazu HANAWA; Kazuhide FUKAYA; Kentaro YAMADA
- Web page: https://patentgrep.com/patent/US20170287794A1

## CPC

- H10P 74/238: {comprising acting in response to an ongoing measurement without interruption of processing, e.g. endpoint detection or in-situ thickness measurement}
- G01N 21/68: using high frequency electric fields
- G01N 21/73: using plasma burners or torches
- G01N 21/84: Systems specially adapted for particular applications
- H01J 37/32963: {End-point detection}
- H10P 50/283: {by chemical means}
- H10W 20/035: {combinations of barrier, adhesion or liner layers, e.g. multi-layered barrier layers}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10W 20/081: {by forming openings in the dielectric parts}
- H10W 20/42: Vias, e.g. via plugs
- H10W 20/425: {Barrier, adhesion or liner layers}
- H10W 20/48: Insulating materials thereof
- G01N 2021/8411: {Application to online plant, process monitoring}
- G01N 2021/8427: {Coatings}
- G01N 2201/1247: Thresholding
- H01J 2237/334: Etching
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A via hole is accurately formed in an interlayer insulating film over a metal wiring. Of emission spectra of plasma to be used for dry etching of the interlayer insulating film, the emission intensities of at least CO, CN, and AlF are monitored such that an end point of the dry etching of the interlayer insulating film is detected based on the emission intensities thereof.

## Claims

### Claim 1

A manufacturing method of a semiconductor device, comprising the steps of:
(a) forming, over a main surface of a semiconductor substrate, laminated wiring including, sequentially from below, three layers of a titanium nitride film, an aluminum film, and a titanium nitride film;
(b) forming an insulating film over the laminated wiring so as to cover the laminated wiring;
(c) coating a photoresist film over the insulating film in order to form a via hole pattern by lithography; and
(d) forming a via hole in the insulating film by dry etching using the via hole pattern as a mask,
wherein, when the dry etching of the insulating film is performed, an end point of the dry etching of the insulating film is detected by monitoring emission intensities of at least CO and CN.

### Claim 2 (depends on 1)

The manufacturing method of a semiconductor device according to claim 1,
wherein the insulating film is a silicon oxide film, and the dry etching is performed by using etching gas containing a fluorine component.

### Claim 3 (depends on 1)

The manufacturing method of a semiconductor device according to claim 1,
wherein operational processing is performed using the monitored emission intensities of CO and CN, and the end point of the dry etching of the insulating film is detected based on a result of the operational processing.

### Claim 4 (depends on 3)

The manufacturing method of a semiconductor device according to claim 3,
wherein the end point of the dry etching of the insulating film is detected based on a CO/CN ratio and an Al/CN ratio.

### Claim 5 (depends on 1)

The manufacturing method of a semiconductor device according to claim 1,
wherein the dry etching of the insulating film includes a main etching step and an over-etching step, and emission intensity of AlF is monitored at least in the over-etching step.

### Claim 6 (depends on 5)

The manufacturing method of a semiconductor device according to claim 5,
wherein a state of the dry etching is monitored by performing secondary differential processing using the monitored emission intensity of AlF and by controlling an inflection point of a calculated secondary differential value.

### Claim 7 (depends on 6)

The manufacturing method of a semiconductor device according to claim 6,
wherein, when a secondary differential value calculated from the emission intensity of AlF becomes more than a preset value, it is determined that abnormality has been caused in the dry etching, and an alarm is issued.

### Claim 8

A method of detecting an end point of dry etching comprising:
monitoring emission intensities of at least CO and CN of emission spectra of plasma to be used for dry etching; and
detecting an end point of the dry etching based on the monitored emission intensities of CO and CN.

### Claim 9 (depends on 8)

The method of detecting an end point of dry etching according to claim 8,
wherein the dry etching is used for forming a via hole in a silicon oxide film formed over aluminum wiring, and is performed by using etching gas containing a fluorine component.

### Claim 10 (depends on 8)

The method of detecting an end point of dry etching according to claim 8,
wherein operational processing is performed using the monitored emission intensities of CO and CN, and an end point of dry etching is detected based on a result of the operational processing.

### Claim 11 (depends on 10)

The method of detecting an end point of dry etching according to claim 10,
wherein an end point of dry etching is detected based on a CO/CN ratio and an Al/CN ratio.

### Claim 12 (depends on 8)

The method of detecting an end point of dry etching according to claim 8,
wherein the dry etching includes a main etching step and an over-etching step, and emission intensity of AlF is monitored at least in the over-etching step.

### Claim 13 (depends on 12)

The method of detecting an end point of dry etching according to claim 12,
wherein a state of the dry etching is monitored by performing secondary differential processing using the monitored emission intensity of AlF and by controlling an inflection point of a secondary differential value from the secondary differential processing.

### Claim 14 (depends on 13)

The method of detecting an end point of dry etching according to claim 13,
wherein, when a secondary differential value calculated from the emission intensity of AlF becomes more than a preset value, it is determined that abnormality has been caused in the dry etching, and an alarm is issued.

### Claim 15

A manufacturing method of a semiconductor device, comprising the steps of:
(a) forming, over a main surface of a semiconductor substrate, laminated wiring including, sequentially from below, three layers of a titanium nitride film, an aluminum film, and a titanium nitride film;
(b) forming an insulating film over the laminated wiring so as to cover the laminated wiring;
(c) coating a photoresist film over the insulating film in order to form a via hole pattern by lithography; and
(d) forming a via hole in the insulating film by dry etching using the via hole pattern as a mask,
wherein, when the dry etching of the insulating film is performed, an end point of the dry etching of the insulating film is detected by monitoring emission intensities of at least two of CO, CN and AlF.