# US 2017/0287723 A1 · Semiconductor device and method for fabricating the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0287723 A1
- Document ID: US20170287723A1
- Status: Published application
- Kind: A1
- Application number: 15/629,760
- Filed: 2017-06-22
- Published: 2017-10-05
- Earliest claimed: 2016-01-20
- Assignees: United Microelectronics Corp.
- Applicants: United Microelectronics Corp.
- Inventors: Huang-Ren Wei; Hsuan-Sheng Lin
- Web page: https://patentgrep.com/patent/US20170287723A1

## CPC

- H10P 50/692: {characterised by their composition, e.g. multilayer masks or materials}
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 62/117: {Shapes of semiconductor bodies}
- H10D 84/0151: {Manufacturing their isolation regions}
- H10D 84/0158: {the components including FinFETs}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10P 50/242: {of Group IV materials}
- H10P 50/642: {Chemical etching}
- H10P 50/694: {characterised by their behaviour during the process, e.g. soluble masks or redeposited masks}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method for fabricating semiconductor device includes the steps of: providing a substrate; forming a fin-shaped structure on the substrate; performing a first etching process to remove part of the fin-shaped structure for forming a trench; and performing a second etching process to extend the depth of the trench and divide the fin-shaped structure into a first portion and a second portion.

## Claims

### Claim 1

A method for fabricating semiconductor device, comprising:
providing a substrate;
forming a fin-shaped structure on the substrate;
performing a first etching process to remove part of the fin-shaped structure for forming a trench; and
performing a second etching process to extend the depth of the trench and divide the fin-shaped structure into a first portion and a second portion.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
forming a hard mask on the fin-shaped structure; and
performing the first etching process to remove part of the hard mask and part of the fin-shaped structure while forming a passivation layer on the hard mask.

### Claim 3 (depends on 2)

The method of claim 2, further comprising:
forming a dielectric layer on the hard mask; and
performing the first etching process and forming the passivation layer on the dielectric layer and the hard mask.

### Claim 4 (depends on 2)

The method of claim 2, wherein the hard mask comprises an oxide-nitride-oxide stack.

### Claim 5 (depends on 2)

The method of claim 2, wherein the passivation layer comprises SiO2.

### Claim 6 (depends on 2)

The method of claim 2, further comprising performing the second etching process to remove part of the passivation layer and part of the fin-shaped structure.

### Claim 7 (depends on 1)

The method of claim 1, further comprising using a first etchant for performing the first etching process and a second etchant for performing the second etching process, wherein the first etchant is different from the second etchant.

### Claim 8 (depends on 7)

The method of claim 7, wherein the first etchant is selected from the group consisting of Cl2, O2, and SiCl4.

### Claim 9 (depends on 7)

The method of claim 7, wherein the second etchant is selected from the group consisting of Cl2 and O2.