# US 2017/0287694 A1 · Photolithographic patterning of electronic devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0287694 A1
- Document ID: US20170287694A1
- Status: Published application
- Kind: A1
- Application number: 15/631,616
- Filed: 2017-06-23
- Published: 2017-10-05
- Earliest claimed: 2014-12-24
- Assignees: Orthogonal, Inc.
- Applicants: Orthogonal, Inc.
- Inventors: Douglas Robert ROBELLO; Terrence Robert O'TOOLE; Frank Xavier BYRNE; Diane Carol FREEMAN
- Web page: https://patentgrep.com/patent/US20170287694A1

## CPC

- H10P 76/202: {for lift-off processes}
- C08F 214/18: Monomers containing fluorine
- C08K 3/16: Halogen-containing compounds
- C09D 4/00: Coating compositions, e.g. paints, varnishes or lacquers, based on organic non-macromolecular compounds having at least one polymerisable carbon-to-carbon unsaturated bond {; Coating compositions, based on monomers of macromolecular compounds of groups C09D183/00 - C09D183/16}
- G03F 7/0046: {with perfluoro compounds, e.g. for dry lithography (G03F7/0048 takes precedence)}
- G03F 7/038: Macromolecular compounds which are rendered insoluble or differentially wettable (G03F7/075 takes precedence; macromolecular azides G03F7/012; macromolecular diazonium compounds G03F7/021)
- G03F 7/0388: {with ethylenic or acetylenic bands in the side chains of the photopolymer}
- G03F 7/0392: {the macromolecular compound being present in a chemically amplified positive photoresist composition}
- G03F 7/0397: {the macromolecular compound having an alicyclic moiety in a side chain}
- G03F 7/325: {Non-aqueous compositions}
- H10K 71/166: {using selective deposition, e.g. using a mask}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES

## Abstract

A method of patterning a device includes forming a fluorinated photopolymer layer over a device substrate. The photopolymer layer has a lower portion proximate the device substrate and an upper portion distal the device substrate. The fluorinated photopolymer layer includes a radiation-absorbing dye and a fluorinated photopolymer having a solubility-altering reactive group. The photopolymer layer is exposed to patterned radiation to form exposed and unexposed areas in accordance with the patterned radiation and a developed structure is formed by removing unexposed areas using a developing agent that includes a first fluorinated solvent. The lower portion of the exposed area of the photopolymer layer has a dissolution rate in the developing agent that is at least 5 times higher than a dissolution rate for the upper portion.

## Claims

### Claim 1

A method of patterning a device comprising:
forming over a device substrate a fluorinated photopolymer layer having a lower portion proximate the device substrate and an upper portion distal the device substrate, the fluorinated photopolymer layer comprising a radiation-absorbing dye and a fluorinated photopolymer having a solubility-altering reactive group;
exposing the photopolymer layer to patterned radiation to form exposed and unexposed areas in accordance with the patterned radiation; and
forming a developed structure by removing unexposed areas in a developing agent comprising a first fluorinated solvent,
wherein
the lower portion of the exposed area of the photopolymer layer has a dissolution rate in the developing agent that is at least 5 times higher than a dissolution rate for the upper portion.

### Claim 2 (depends on 1)

The method of claim 1 wherein the radiation-absorbing dye is covalently attached the fluorinated photopolymer.

### Claim 3 (depends on 1)

The method of claim 1 wherein the fluorinated photopolymer is a copolymer comprising a first repeating unit having a fluorine-containing group, a second repeating unit having a solubility-altering reactive group, and a third repeating unit having a radiation-absorbing dye.

### Claim 4 (depends on 1)

The method of claim 1 wherein the fluorinated photopolymer has a fluorine content of at least 10% by weight.

### Claim 5 (depends on 1)

The method of claim 1 wherein the developed structure has an undercut profile.

### Claim 6 (depends on 1)

The method of claim 1 further comprising treating the developed structure with a lift-off agent comprising a second fluorinated solvent.

### Claim 7

A method of patterning a device comprising:
forming over a device substrate a fluorinated photopolymer layer comprising a radiation-absorbing dye and a fluorinated photopolymer having a solubility-altering reactive group;
exposing the photopolymer layer to patterned radiation to form an exposed photopolymer layer having exposed and unexposed areas in accordance with the patterned radiation; and
contacting the exposed photopolymer layer with a developing agent to remove the unexposed areas, thereby forming a developed structure having a first pattern of photopolymer covering the device substrate and a complementary second pattern of uncovered substrate corresponding to the removed unexposed areas, the developing agent comprising a first fluorinated solvent,
wherein;
the radiation provides a total exposure dose EXP (mJ/cm2) at an exposure wavelength λexp,
the photopolymer layer has a thickness Tf(μm), an absorptivity α (absorbance/μm) at λexp and a speed point SP (mJ/cm2) under conditions used for the exposing and contacting with the developing agent, and
a processing factor, P, is in a range of 0.1 to 0.95 wherein P=[log(EXP/SP)]/(α*Tf).

### Claim 8 (depends on 7)

The method of claim 7 wherein the radiation-absorbing dye is covalently attached the fluorinated photopolymer.

### Claim 9 (depends on 7)

The method of claim 7 wherein the fluorinated photopolymer is a copolymer comprising a first repeating unit having a fluorine-containing group, a second repeating unit having a solubility-altering reactive group, and a third repeating unit having a radiation-absorbing dye.

### Claim 10 (depends on 7)

The method of claim 7 wherein the fluorinated photopolymer has a fluorine content of at least 10% by weight.

### Claim 11 (depends on 7)

The method of claim 7 wherein P is in a range of 0.6 to 0.92.

### Claim 12 (depends on 7)

The method of claim 7 wherein the photopolymer layer has a maximum contrast greater than 5.

### Claim 13 (depends on 7)

The method of claim 7 wherein α is at least 0.3 absorbance units/μm) at λexp.

### Claim 14 (depends on 13)

The method of claim 13 wherein Tf is at least 1.5 μm.

### Claim 15 (depends on 7)

The method of claim 7 wherein the device is an OLED, an OTFT, a bioelectronic device or a MEMS device.

### Claim 16 (depends on 15)

The method of claim 15 wherein the device is a passive matrix OLED device.

### Claim 17

A fluorinated photopolymer composition, comprising:
a fluorinated solvent;
a radiation-absorbing dye; and
a fluorinated photopolymer having a fluorine content of at least 10% by weight comprising one or more solubility-altering reactive groups, wherein
a film formed from the composition has, after removal of the fluorinated solvent, an absorptivity of at least 0.3 absorbance units per μm of film thickness when measured at 365 nm, 405 nm or 436 nm.

### Claim 18 (depends on 17)

The composition of claim 17 wherein the fluorinated photopolymer has a fluorine content in a range of 30 to 60% by weight.

### Claim 19 (depends on 17)

The composition of claim 17 wherein the radiation-absorbing dye is covalently attached the fluorinated photopolymer.

### Claim 20 (depends on 17)

The composition of claim 17 wherein the fluorinated photopolymer further comprises a branching unit.