# US 2017/0287632 A1 · Radially anisotropic sintered ring magnet and its production method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0287632 A1
- Document ID: US20170287632A1
- Status: Published application
- Kind: A1
- Application number: 15/508,333
- Filed: 2015-08-27
- Published: 2017-10-05
- Earliest claimed: 2014-09-03
- Assignees: Hitachi Metals, Ltd.
- Applicants: Hitachi Metals, Ltd.
- Inventors: Takahiro KATOU
- Web page: https://patentgrep.com/patent/US20170287632A1

## CPC

- H01F 41/028: {Radial anisotropy (for rotor or stator bodies H02K15/02)}
- B22F 3/02: Compacting only
- B22F 3/16: in successive or repeated steps
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- H01F 7/021: {Construction of PM (H01F7/0278 takes precedence; PM compositions H01F1/032)}
- H01F 41/0253: {for manufacturing permanent magnets}
- B22F 2202/05: Use of magnetic field
- B22F 2301/355: Rare Earth - Fe intermetallic alloys
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- C22C 2202/02: Magnetic
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A method for producing a radially anisotropic sintered ring magnet by continuously repeating a step of supplying magnetic powder to a die comprising a columnar magnetic core, and a cylindrical outer die having axially connected magnetic member and non-magnetic member, with a cavity between the core and the cylindrical outer die, and a step of compression-molding the magnetic powder in a radial magnetic field applied between the magnetic core and the magnetic member of the outer die, plural times in one die, to form a final green body composed of pluralities of integrally connected green bodies; and sintering the final green body; the magnetic field being applied in a state where an upper end of the magnetic member of the cylindrical outer die is higher than an upper surface of the magnetic powder supplied.

## Claims

### Claim 1

A method for producing a radially anisotropic sintered ring magnet comprising
continuously repeating a step of supplying magnetic powder to a die comprising a columnar magnetic core, and a cylindrical outer die having axially connected magnetic member and non-magnetic member, with a cavity between said core and said cylindrical outer die, and a step of compression-molding said magnetic powder in a radial magnetic field applied between said magnetic core and said magnetic member of said outer die, plural times in one die, to form a final green body composed of pluralities of integrally connected green bodies; and
sintering said final green body;
said magnetic field being applied in a state where an upper end of the magnetic member of said cylindrical outer die is higher than an upper surface of said magnetic powder supplied.

### Claim 2 (depends on 1)

The method for producing a radially anisotropic sintered ring magnet according to claim 1, wherein after the step of supplying said magnetic powder, said cylindrical outer die is moved until an upper end of said magnetic member of said cylindrical outer die becomes higher than an upper surface of said magnetic powder supplied.

### Claim 3 (depends on 1)

The method for producing a radially anisotropic sintered ring magnet according to claim 1, wherein the compression-molding pressure of said final green body is higher than that of a previous-step green body (preliminary green body).

### Claim 4 (depends on 3)

The method for producing a radially anisotropic sintered ring magnet according to claim 3, wherein said preliminary green body has a density of 3.1 g/cm3 or more, and wherein the density of said final green body is 0.2 g/cm3 or more higher than that of said preliminary green body.

### Claim 5

A radially anisotropic sintered ring magnet having a connection in a plane perpendicular to the axial direction, with no decrease in a surface magnetic flux density at said connection.

### Claim 6

A radially anisotropic sintered ring magnet having a connection in a plane perpendicular to the axial direction, a surface magnetic flux density (mT) at said connection being larger than a value obtained by subtracting 25 (mT) from an average of magnetic flux densities (mT) at positions of +5 mm and −5 mm, respectively, axially separate from the connection.

### Claim 7 (depends on 5)

The radially anisotropic sintered ring magnet according to claim 5, which is obtained by axially connecting pluralities of green bodies, and sintering the resultant multi-connection green body.