# US 2017/0287583 A1 · Improved methods and compositions for fabrication of superconducting wire

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0287583 A1
- Document ID: US20170287583A1
- Status: Published application
- Kind: A1
- Application number: 15/531,439
- Filed: 2015-12-18
- Published: 2017-10-05
- Earliest claimed: 2014-12-19
- Assignees: The Texas A&M University System
- Applicants: The Texas A&M University System
- Inventors: Nathaniel Pogue; Joshua N. Kellams; Peter Mclntyre
- Web page: https://patentgrep.com/patent/US20170287583A1

## CPC

- H01B 1/026: {Alloys based on copper}
- B22F 3/02: Compacting only
- B22F 3/20: by extruding
- B22F 3/24: After-treatment of workpieces or articles {(B22F3/1146 takes precedence)}
- B22F 5/12: of wires {(of tubes B22F5/10)}
- C22C 9/01: with aluminium as the next major constituent
- H01B 12/04: Single wire
- H10N 60/0268: {of devices comprising copper oxide}
- H10N 60/203: {comprising high-Tc ceramic materials}
- H10N 60/857: {comprising copper oxide}
- B22F 2003/242: {Coating}
- B22F 2301/255: Silver or gold
- B22F 2302/25: Oxide
- B22F 2304/054: Particle size between 1 and 100 nm
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR

## Abstract

The present disclosure relates generally to wires and more particularly to textured powder wires containing nanoscale metallic silver powder. The invention presents an improvement of the process of making compressed cores of textured-powder high-temperature superconductor previously using the micaceous high-temperature superconductor Bi-2212. Embodiments of the claimed methods are useful with the micaceous high-temperature superconductors, notably Bi2Sr2CaCu208+x (Bi-2212) and Bi2S-r2Ca2Cu3O10+x (Bi-2223) and rare earth barium copper oxide (REBCO).

## Claims

### Claim 1

A composition comprising a powder of a superconducting material and a silver nanopowder.

### Claim 2 (depends on 1)

The composition of claim 1, wherein the superconducting material is Bi-2212, Bi-2223, or rare earth barium copper oxide.

### Claim 3 (depends on 1)

The composition of claim 1, wherein the silver nanopowder has a mean particle size that is smaller than a mean particle size of the powder of the superconducting material.

### Claim 4 (depends on 1)

The composition of claim 1, wherein a mean particle size of the silver nanopowder ranges from 80-100 nm.

### Claim 5 (depends on 1)

The composition of claim 1, wherein a mean particle size of the powder of the superconducting material ranges from 1-2 micron.

### Claim 6 (depends on 1)

The composition of claim 1, wherein the silver nanopowder is a homegenously dispersed nanosilver powder.

### Claim 7

A method for fabricating a superconducting wire, the method comprising the steps of:
compressing a mixture of a superconductor powder with a silver nanopowder to produce a textured-powder core by compressing the mixture;
inserting the textured-powder core into a cylinder;
sealing the cylinder by inserting plugs into ends of the cylinder; and
processing the cylinder to form a wire.

### Claim 8 (depends on 7)

The method of claim 7, wherein the compressing further comprises:
placing the mixture into a female-forming die;
pressing a male-forming die into the female-forming die; and
wherein the male-forming die has side boundaries that for a close-sliding fit within the female-forming die.

### Claim 9 (depends on 7)

The method of claim 7, wherein the cylinder is a metal cylinder and the plugs are metal plugs that are welded to the metal cylinder.

### Claim 10 (depends on 7)

The method of claim 7, wherein the processing comprises an extruding process.

### Claim 11 (depends on 7)

The method of claim 7, wherein the processing comprises a drawing process.

### Claim 12 (depends on 7)

The method of claim 7, further comprising:
heat treating the cylinder at an elevated temperature in an oxygen-rich atmosphere to form a passivated oxide layer on a surface of the cylinder prior to the inserting; and
removing the passivated oxide layer from the surface of the cylinder after insertion of the textured-powder core.

### Claim 13 (depends on 7)

The method of claim 7, wherein:
the cylinder for processing comprises multiple cylinders arranged in parallel, each of the multiple cylinders being formed from the compressing, the inserting, and the sealing steps; and
the wire is a bonded composite wire comprising the multiple cylinders.

### Claim 14 (depends on 13)

The method of claim 13, further comprising:
heating the bonded composite wire to a temperature equal to a melt temperature of the superconducting powder;
holding the temperature at the melt temperature for a dwell time; and
ramping the temperature downward to an intermediate temperature for a second dwell time to provide for annealing of the bonded composite wire.

### Claim 15 (depends on 14)

The method of claim 14 wherein the melt temperature is approximately 878.4° C.

### Claim 16 (depends on 14)

The method of claim 14 further comprising:
heating the bonded composite wires to a temperature just below the melt temperature of the superconducting powder;
holding the temperature at just below the melt temperature for a first dwell time to provide for surface melting on crystal surfaces of the superconducting powder and solid-phase diffusion of atomic species within the superconducting powder; and
ramping the temperature down with provision of a second dwell time at an intermediate temperature to provide for annealing of the superconducting powder within cavities of the bonded composite wire.

### Claim 17 (depends on 16)

The method of claim 16 wherein the temperature for the first dwell time ranges from 860-877.5° C.

### Claim 18

A method for achieving homogeneous dispersal of silver nanopowder in a composition, the method comprising: mixing silver nanopowder with a superconductor powder via a high energy acoustic mixing by placing the silver nanopowder and the superconductor powder in a container that is in contact with a high-power audio-frequency acoustic oscillator.

### Claim 19 (depends on 18)

The method of claim 18, wherein the mixing is comprises using a 60 Hz acoustic modulator to produce 90 g of cyclic acceleration.

### Claim 20

A composite wire comprising:
a first sheet;
a plurality of cores arranged on the first sheet parallel to one another;
a second sheet placed on top of the plurality of cores to form a composite sheet that comprises the first sheet, the plurality of cores, and the second sheet;
a plurality of channels formed between adjacent cores and through the composite sheet; and
wherein the composite wire comprises a tube formed by rolling up the composite sheet.

### Claim 21 (depends on 20)

The composite wire of claim 20, further comprising a cylindrical metallic core rod around which the composite sheet is rolled.

### Claim 22 (depends on 20)

The composite wire of claim 20, further comprising:
a tube into which the composite wire is inserted; and
a pair of plugs that are inserted into ends of the tube; and
wherein the tube is extruded and/or drawn to form a fully bonded composite wire.

### Claim 23 (depends on 21)

The composite wire of claim 21, wherein the cylindrical metallic core rod is made of a metal alloy that is passive to high-temperature diffusion of metal ions and also passive to oxidation.

### Claim 24 (depends on 23)

The composite wire of claim 23, wherein the metal alloy is aluminum bronze containing ˜11% aluminum.