# US 2017/0287574 A1 · Method of making a nuclear fuel pellet for a nuclear power reactor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0287574 A1
- Document ID: US20170287574A1
- Status: Published application
- Kind: A1
- Application number: 15/509,056
- Filed: 2015-04-24
- Published: 2017-10-05
- Earliest claimed: 2014-09-08
- Assignees: Westinghouse Electric Sweden AB
- Applicants: Westinghouse Electric Sweden AB
- Inventors: Hans WIDEGREN; Edward J. LAHODA; Lars HALLSTADIUS
- Web page: https://patentgrep.com/patent/US20170287574A1

## CPC

- G21C 21/02: Manufacture of fuel elements or breeder elements contained in non-active casings
- G21C 3/044: {Fuel elements with porous or capillary structure}
- G21C 3/18: Internal spacers or other non-active material within the casing, e.g. compensating for expansion of fuel rods or for compensating excess reactivity (interlayers G21C3/20)
- G21C 3/20: with coating on fuel or on inside of casing; with non-active interlayer between casing and active material {with multiple casings or multiple active layers}
- G21C 3/623: {Oxide fuels}
- G21C 3/045: {Pellets}
- Y02E 30/30: Nuclear fission reactors
- G21C: NUCLEAR REACTORS (fusion reactors, hybrid fission-fusion reactors G21B; nuclear explosives G21J)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method of making a nuclear fuel pellet for a nuclear power reactor. The method includes providing a nuclear fuel material in powder form, providing an additive, forming a so-called green pellet, wherein said additive is added either to said nuclear fuel material in powder form or to the green pellet, sintering the green pellet, wherein said additive is such that it causes larger grains in the nuclear fuel pellet, and wherein said additive is made of or includes a substance which causes the larger grains and which substantially leaves at least an outer portion of the pellet before and/or during the sintering step.

## Claims

### Claim at position 1

1-13. (canceled)

### Claim 14

A method of making a nuclear fuel pellet for a nuclear power reactor, the method comprising the following steps:
providing a nuclear fuel material in powder form,
providing an additive,
pressing the powder such that a green pellet is obtained,
wherein said additive is added either to said nuclear fuel material in powder form or to the green pellet,
sintering the so obtained green pellet,
wherein said additive is such that larger grains in the nuclear fuel material are present in the pellet after the sintering step as compared with the grain size obtained if a pellet, which is produced according to the above manner but without the addition of the additive, is sintered in the same manner,
wherein said additive is made of or includes a substance which causes said larger grains in the sintered pellet, wherein said substance is selected and the method is performed such that at least to 90% of the substance, leaves at least an outer portion of the pellet before and/or during the sintering step.

### Claim 15 (depends on 14)

A method according to claim 14, wherein the produced nuclear fuel pellet has a substantially cylindrical shape with a radius r and wherein said outer portion is the part of the nuclear fuel pellet that is located between 0.8 r and r, or between 0.9 r and r, or between 0.95 r and r.

### Claim 16 (depends on 14)

A method according to claim 14, wherein said substance is made of, or comprises, B and/or Cr.

### Claim 17 (depends on 16)

A method according to claim 16, wherein said additive to at least 60% is selected from the group consisting of B, UB4, B4C, ZrB2, Cr, CrO, CrO2 and Cr2O3 or combinations thereof.

### Claim 18 (depends on 14)

A method according to claim 14, wherein said additive comprises B and wherein at least 90% of said B is 11B.

### Claim 19 (depends on 14)

A method according to claim 14, comprising arranging said additive such that an outer portion of the green pellet contains substantially more additive than an inner portion of the green pellet, such that the sintered pellet has a larger grain size in the outer portion than in the inner portion.

### Claim 20 (depends on 14)

A method according to claim 14, wherein said additive is provided in the form of particles.

### Claim 21 (depends on 20)

A method according to claim 20, comprising providing a liquid and arranging the additive in the liquid such that said additive is in the form of particles dispersed in said liquid, wherein the liquid with the additive is added either to said nuclear fuel material in powder form or to the green pellet.

### Claim 22 (depends on 21)

A method according to claim 21, comprising adding said liquid with the additive to the green pellet by contacting the green pellet with the liquid such that the liquid, with the additive, penetrates into the green pellet and controlling the penetration depth of the liquid, and thereby of the additive, into the green pellet.

### Claim 23 (depends on 22)

A method according to claim 22, wherein said step of controlling the penetration depth is done by selecting one or both of the following:
the viscosity of the liquid with included additive,
the amount of the liquid, with the additive, which is added to the green pellet when contacting the green pellet with the liquid, with the additive.

### Claim 24 (depends on 21)

A method according to claim 21, wherein said liquid is selected and said method is performed such that the liquid will at least to 99% leave the pellet before or during the sintering step.

### Claim 25 (depends on 21)

A method according to claim 21, wherein said liquid is an oil.

### Claim 26 (depends on 25)

A method according to claim 25, wherein said oil is a mineral oil.

### Claim 27 (depends on 14)

A method according to claim 14, wherein at least 95% of the substance leaves at least an outer portion of the pellet before and/or during the sintering step.

### Claim 28 (depends on 27)

A method according to claim 27, wherein at least 99% of the substance leaves at least an outer portion of the pellet before and/or during the sintering step.

### Claim 29 (depends on 17)

A method according to claim 17, wherein said additive to at least 80% is selected from the group consisting of B, UB4, B4C, ZrB2, Cr, CrO, CrO2 and Cr2O3 or combinations thereof.

### Claim 30 (depends on 29)

A method according to claim 29, wherein 100% of said additive is selected from the group consisting of B, UB4, B4C, ZrB2, Cr, CrO, CrO2 and Cr2O3 or combinations thereof.

### Claim 31 (depends on 14)

A method of making and using nuclear fuel, comprising:
making a plurality of nuclear fuel pellets as defined in the method of claim 14;
arranging the nuclear fuel pellets in cladding tubes;
arranging the cladding tubes, with the nuclear fuel pellets, in the core of a nuclear power reactor in a nuclear power plant, such that at least 20% of the nuclear fuel material in said core are made of pellets in accordance with the aforementioned method of making the plurality of nuclear fuel pellets; and
operating the nuclear reactor to produce energy.

### Claim 32 (depends on 31)

A method according to claim 31, wherein at least 50% of the nuclear fuel material in said core are made of pellets made in accordance with a method of making a nuclear fuel pellet for a nuclear power reactor comprising the following steps:
providing a nuclear fuel material in powder form,
providing an additive,
pressing the powder such that a green pellet is obtained,
wherein said additive is added either to said nuclear fuel material in powder form or to the green pellet,
sintering the so obtained green pellet,
wherein said additive is such that larger grains in the nuclear fuel material are present in the pellet after the sintering step as compared with the grain size obtained if a pellet, which is produced according to the above manner but without the addition of the additive, is sintered in the same manner,
wherein said additive is made of or includes a substance which causes said larger grains in the sintered pellet, wherein said substance is selected and the method is performed such that at least to 90% of the substance, leaves at least an outer portion of the pellet before and/or during the sintering step.

### Claim 33 (depends on 31)

A method according to claim 31, wherein 100% of the nuclear fuel material in said core are made of pellets made in accordance with a method of making a nuclear fuel pellet for a nuclear power reactor comprising the following steps:
providing a nuclear fuel material in powder form,
providing an additive,
pressing the powder such that a green pellet is obtained,
wherein said additive is added either to said nuclear fuel material in powder form or to the green pellet,
sintering the so obtained green pellet,
wherein said additive is such that larger grains in the nuclear fuel material are present in the pellet after the sintering step as compared with the grain size obtained if a pellet, which is produced according to the above manner but without the addition of the additive, is sintered in the same manner,
wherein said additive is made of or includes a substance which causes said larger grains in the sintered pellet, wherein said substance is selected and the method is performed such that at least to 90% of the substance, leaves at least an outer portion of the pellet before and/or during the sintering step.