# US 2017/0285413 A1 · Method for manufacturing liquid crystal display device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0285413 A1
- Document ID: US20170285413A1
- Status: Published application
- Kind: A1
- Application number: 15/608,273
- Filed: 2017-05-30
- Published: 2017-10-05
- Earliest claimed: 2011-08-29
- Assignees: Sharp Kabushiki Kaisha
- Applicants: Sharp Kabushiki Kaisha
- Inventors: Koichi MIYACHI; Isamu MIYAKE
- Web page: https://patentgrep.com/patent/US20170285413A1

## CPC

- G02F 1/133788: {by light irradiation, e.g. linearly polarised light photo-polymerisation}
- G02F 1/133711: {by organic films, e.g. polymeric films}
- G02F 1/1368: in which the switching element is a three-electrode device {(G02F1/136277 takes precedence)}
- G02F 1/133738: {for homogeneous alignment}
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS

## Abstract

The present invention provides a method for manufacturing a liquid crystal display device, which hardly causes display unevenness in joining parts in which mutually neighboring exposure regions are overlapped upon carrying out a photo-alignment treatment for forming a horizontal alignment film. The method for manufacturing a liquid crystal display device of the present invention includes a step of forming a horizontal alignment film by carrying out a photo-alignment treatment of irradiating a photo-alignment film material applied to at least one substrate of a pair of substrates with polarized light, wherein the photo-alignment treatment is carried out by exposure to a plurality of regions of one substrate surface; two neighboring regions among the plurality of regions to be exposed include an overlapped part; an irradiation amount of the polarized light to the overlapped part is gradually lowered in one of the two neighboring regions toward the other of the two neighboring regions; and the overlapped part of the two neighboring regions has a width of 20 mm or wider.

## Claims

### Claim 1

(canceled)

### Claim 2

A method for manufacturing a liquid crystal display device comprising:
forming an alignment film by performing a photo-alignment treatment of irradiating a photo-alignment film material applied to at least one substrate of a pair of substrates with a plurality of polarized light sources; wherein the plurality of polarized light sources includes a first light source and a second light source;
the photo-alignment treatment is performed by scanning the at least one substrate of the pair of substrates and the plurality of polarized light sources and exposing a substrate surface of the at least one substrate of the pair of substrates to polarized light applied from a direction perpendicular to the substrate surface;
the alignment film includes a first region which is exposed with the polarized light applied by the first light source and a second region which is exposed with the polarized light applied by the second light source;
a direction in which the first light source moves relatively to the at least one substrate of the pair of substrates in the photo-alignment treatment for the first region is defined as a first scan direction of the first light source, and a direction in which the second light source moves relatively to the at least one substrate of the pair of substrates in the photo-alignment treatment for the second region of the second light source is defined as a second scan direction, the first scan direction of the first light source is identical to the second scan direction of the second light source;
the second region includes an overlapping portion which overlaps with the first region;
the first light source and the second light source are adjacent to each other while scanning the photo-alignment treatment and;
exposing the first region with the polarized light by the first light source is performed simultaneously with exposing the second region with the polarized light by the second light source; and
the at least one substrate of the pair of substrates includes a multidomain structure.

### Claim 3 (depends on 2)

The method for manufacturing a liquid crystal display device according to claim 2, wherein
the alignment film is a horizontal alignment film;
a first irradiation amount of the polarized light by the first light source to the overlapping portion is gradually lowered in the first region toward the second region and a second irradiation amount of the polarized light by the second light source to the overlapping portion is gradually lowered in the second region toward the first region; and
the overlapping portion has a width of 20 mm or wider.

### Claim 4 (depends on 2)

The method for manufacturing a liquid crystal display device according to claim 2, wherein a variation of the first irradiation amount in the overlapping portion and/or a variation of the second irradiation amount in the overlapping portion satisfies a sine function.

### Claim 5 (depends on 2)

The method for manufacturing a liquid crystal display device according to claim 2, wherein a variation of the first irradiation amount in the overlapping portion and/or a variation of the second irradiation amount in the overlapping portion satisfies a linear function.

### Claim 6 (depends on 2)

The method for manufacturing a liquid crystal display device according to claim 2, further comprises:
forming a polymer layer for controlling alignment of liquid crystal molecules adjacent thereto on the alignment film by irradiating a liquid crystal composition containing a liquid crystal material and a monomer and being injected between the pair of substrates with light to polymerize the monomer;
wherein the liquid crystal material contains liquid crystal molecules including, in a molecular structure thereof, a multiple bond other than conjugated double bonds of a benzene ring.

### Claim 7 (depends on 2)

The method for manufacturing a liquid crystal display device according to claim 2, wherein the photo-alignment film material includes one or both of a photoisomerizable functional group and a photodimerizable functional group.

### Claim 8 (depends on 7)

The method for manufacturing a liquid crystal display device according to claim 7, wherein the first light source and the second light source are spaced from each other by intervals extending along a direction perpendicular to a scanning direction of the at least one substrate of the pair of substrates and the plurality of polarized light sources.

### Claim 9 (depends on 7)

The method for manufacturing a liquid crystal display device according to claim 7, wherein the first light source is provided in a first exposure head and the second light source is provided in a second exposure head.

### Claim 10 (depends on 7)

The method for manufacturing a liquid crystal display device according to claim 7, wherein the first exposure head and the second exposure head are connected to an exposure stage.

### Claim 11 (depends on 2)

The method for manufacturing a liquid crystal display device according to claim 2, wherein the first light source is provided in a first exposure head and the second light source is provided in a second exposure head.

### Claim 12 (depends on 2)

The method for manufacturing a liquid crystal display device according to claim 2, wherein the at least one substrate of the pair of substrates includes a thin film transistor including an oxide semiconductor.

### Claim 13 (depends on 12)

The method for manufacturing a liquid crystal display device according to claim 12, wherein the oxide semiconductor is indium-gallium-zinc-oxide.

### Claim 14 (depends on 2)

The method for manufacturing a liquid crystal display device according to claim 2, wherein the photo-alignment film material includes a photoisomerizable material, a photodimerizable material or a photodissociation material.

### Claim 15 (depends on 14)

The method for manufacturing a liquid crystal display device according to claim 14, wherein the photoisomerizable material includes an azobenzene derivative.

### Claim 16 (depends on 14)

The method for manufacturing a liquid crystal display device according to claim 14, wherein the photodimerizable material includes a cinnamate derivative.

### Claim 17 (depends on 14)

The method for manufacturing a liquid crystal display device according to claim 14, wherein the photodissociation material contains a cyclobutane skeleton.