# US 2017/0285412 A1 · Method for manufacturing liquid crystal display panel

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0285412 A1
- Document ID: US20170285412A1
- Status: Published application
- Kind: A1
- Application number: 15/120,750
- Filed: 2016-04-22
- Published: 2017-10-05
- Earliest claimed: 2016-04-05
- Assignees: Shenzhen China Star Optoelectronics Technology Co., Ltd.
- Applicants: Shenzhen China Star Optoelectronics Technology Co. Ltd.
- Inventors: Xiang LI; Chungching HSIEH; Yongchao ZHAO; Rentang ZHAO
- Web page: https://patentgrep.com/patent/US20170285412A1

## CPC

- G02F 1/133788: {by light irradiation, e.g. linearly polarised light photo-polymerisation}
- G02F 1/1337: Surface-induced orientation of the liquid crystal molecules, e.g. by alignment layers
- G02F 1/1341: Filling or closing of cells
- G02F 1/13415: {Drop filling process}
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS

## Abstract

A method for manufacturing a liquid crystal display panel is provided. The method includes the following steps of: drop-filling liquid crystal molecules on a color film substrate having a seal frame, wherein the liquid crystal molecules are doped with thermal reactive monomers; and heat-curing a frame, and simultaneously making the thermal reactive monomers in the liquid crystal molecules into a polymer on the surface of the alignment film. The reliability of the alignment film is improved by the present invention.

## Claims

### Claim 1

A method for manufacturing a liquid crystal display panel, comprising the following steps of:
coating an isotropic alignment film onto a color film substrate and an array substrate, respectively;
irradiating the isotropic alignment film by a linearly polarized ultraviolet light, to transform the isotropic alignment film into an anisotropic alignment film, thereby forming a pre-tilt angle of the alignment film;
drop-filling liquid crystal molecules on the color film substrate having a seal frame, wherein the liquid crystal molecules are doped with thermal reactive monomers;
aligning and bonding the color film substrate and the corresponding array substrate;
providing a frame around the liquid crystal display panel; and
heat-curing the frame, and simultaneously making the thermal reactive monomers in the liquid crystal molecules into a polymer on a surface of the alignment film, thereby improving an anchoring force of the alignment film to the liquid crystal molecules,
wherein the heat-curing has a temperature between 50° C. and 80° C., and the heat-curing has an operation time between 10 minutes and 20 minutes.

### Claim 2 (depends on 1)

The method for manufacturing the liquid crystal display panel of claim 1, wherein after the step in which the isotropic alignment film is coated, and before the step in which the isotropic alignment film is irradiated by the linearly polarized ultraviolet light, the method further comprises the following step of:
pre-baking the alignment film, so that the alignment film having a uniform thickness, and an organic solvent in the alignment film being volatilized.

### Claim 3 (depends on 2)

The method for manufacturing the liquid crystal display panel of claim 2, wherein the pre-baking has a temperature between 80° C. and 90° C.

### Claim 4 (depends on 2)

The method for manufacturing the liquid crystal display panel of claim 2, wherein the pre-baking has an operation time between 5 minutes and 10 minutes.

### Claim 5 (depends on 1)

The method for manufacturing the liquid crystal display panel of claim 1, wherein after the step in which the alignment film is pre-baked, and before the step in which the isotropic alignment film is irradiated by the linearly polarized ultraviolet light, the method further comprises the following step of:
baking the alignment film at high temperatures, thereby curing the alignment film.

### Claim 6 (depends on 1)

The method for manufacturing the liquid crystal display panel of claim 1, wherein after the step in which the isotropic alignment film is irradiated by the linearly polarized ultraviolet light, and before the step in which the liquid crystal molecules are drop-filled on the color film substrate having the seal frame, the method further comprises the following step of:
baking the alignment film at high temperatures, thereby curing the alignment film.

### Claim 7 (depends on 5)

The method for manufacturing the liquid crystal display panel of claim 5, wherein the baking at high temperatures has a temperature between 180° C. and 220° C., and the baking at high temperatures has an operation time between 40 minutes and 60 minutes.

### Claim 8 (depends on 6)

The method for manufacturing the liquid crystal display panel of claim 6, wherein the baking at high temperatures has a temperature between 180° C. and 220° C., and the baking at high temperatures has an operation time between 40 minutes and 60 minutes.

### Claim 9 (depends on 1)

The method for manufacturing the liquid crystal display panel of claim 1, wherein after the step in which the frame is provided around the liquid crystal display panel, and before the step in which the frame is heat-cured, the method further comprises the following step of:
ultraviolet-curing the frame.

### Claim 10

A method for manufacturing a liquid crystal display panel, comprising the following steps of:
coating an isotropic alignment film onto a color film substrate and an array substrate, respectively;
irradiating the isotropic alignment film by a linearly polarized ultraviolet light, to transform the isotropic alignment film into an anisotropic alignment film, thereby forming a pre-tilt angle of the alignment film;
drop-filling liquid crystal molecules on the color film substrate having a seal frame, wherein the liquid crystal molecules are doped with thermal reactive monomers;
aligning and bonding the color film substrate and the corresponding array substrate;
providing a frame around the liquid crystal display panel; and
heat-curing the frame, and simultaneously making the thermal reactive monomers in the liquid crystal molecules into a polymer on a surface of the alignment film, thereby improving an anchoring force of the alignment film to the liquid crystal molecules.

### Claim 11 (depends on 10)

The method for manufacturing the liquid crystal display panel of claim 10, wherein the heat-curing has a temperature between 50° C. and 80° C.

### Claim 12 (depends on 10)

The method for manufacturing the liquid crystal display panel of claim 10, wherein the heat-curing has an operation time between 10 minutes and 20 minutes.

### Claim 13 (depends on 10)

The method for manufacturing the liquid crystal display panel of claim 10, wherein after the step in which the isotropic alignment film is coated, and before the step in which the isotropic alignment film is irradiated by the linearly polarized ultraviolet light, the method further comprises the following step of:
pre-baking the alignment film, so that the alignment film having a uniform thickness, and an organic solvent in the alignment film being volatilized.

### Claim 14 (depends on 13)

The method for manufacturing the liquid crystal display panel of claim 13, wherein the pre-baking has a temperature between 80° C. and 90° C.

### Claim 15 (depends on 13)

The method for manufacturing the liquid crystal display panel of claim 13, wherein the pre-baking has an operation time between 5 minutes and 10 minutes.

### Claim 16 (depends on 10)

The method for manufacturing the liquid crystal display panel of claim 10, wherein after the step in which the alignment film is pre-baked, and before the step in which the isotropic alignment film is irradiated by the linearly polarized ultraviolet light, the method further comprises the following step of:
baking the alignment film at high temperatures, thereby curing the alignment film.

### Claim 17 (depends on 10)

The method for manufacturing the liquid crystal display panel of claim 10, wherein after the step in which the isotropic alignment film is irradiated by the linearly polarized ultraviolet light, and before the step in which the liquid crystal molecules are drop-filled on the color film substrate having the seal frame, the method further comprises the following step of:
baking the alignment film at high temperatures, thereby curing the alignment film.

### Claim 18 (depends on 16)

The method for manufacturing the liquid crystal display panel of claim 16, wherein the baking at high temperatures has a temperature between 180° C. and 220° C.

### Claim 19 (depends on 16)

The method for manufacturing the liquid crystal display panel of claim 16, wherein the baking at high temperatures has an operation time between 40 minutes and 60 minutes.

### Claim 20 (depends on 10)

The method for manufacturing the liquid crystal display panel of claim 10, wherein after the step in which the frame is provided around the liquid crystal display panel, and before the step in which the frame is heat-cured, the method further comprises the following step of:
ultraviolet-curing the frame.