# US 2017/0285295 A1 · Copper-titanium Alloy Foil Having Plated Layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0285295 A1
- Document ID: US20170285295A1
- Status: Published application
- Kind: A1
- Application number: 15/473,721
- Filed: 2017-03-30
- Published: 2017-10-05
- Earliest claimed: 2016-03-31
- Assignees: JX Nippon Mining & Metals Corporation
- Applicants: JX Nippon Mining & Metals Corporation
- Inventors: Kenta Tsujie
- Web page: https://patentgrep.com/patent/US20170285295A1

## CPC

- G02B 7/026: {using retaining rings or springs (G02B7/027 takes precedence)}
- B23K 1/0016: {Soldering of electronic components}
- B23K 1/19: taking account of the properties of the materials to be soldered
- B23K 1/20: Preliminary treatment of work or areas to be soldered, e.g. in respect of a galvanic coating
- B32B 15/01: all layers being exclusively metallic {(making layered metal workpieces by pressure cladding B23K20/22; making coatings with a metallic material characterised by its composition C23C30/00)}
- B32B 15/04: comprising metal as the main or only constituent of a layer, {which is} next to another layer of {the same or of} a {different material (next to a bituminous or tarry layer B32B11/08; next to a water-setting substance layer B32B13/06; next to a glass layer B32B17/061; next to a cellulosic plastic layer B32B23/042)}
- B32B 15/043: {of metal (B32B15/01 takes precedence)}
- B32B 15/20: comprising aluminium or copper {(B32B15/016 and B32B15/017 take precedence)}
- C22C 9/00: Alloys based on copper
- C22C 9/05: with manganese as the next major constituent
- C22C 9/06: with nickel or cobalt as the next major constituent
- C22C 9/10: with silicon as the next major constituent
- C23C 2/08: Tin or alloys based thereon
- C23C 30/00: Coating with metallic material characterised only by the composition of the metallic material, i.e. not characterised by the coating process (C23C26/00, C23C28/00 take precedence)
- C23C 30/005: {on hard metal substrates}
- C25D 3/30: of tin
- C25D 7/0614: {Strips or foils}
- G02B 7/09: adapted for automatic focusing or varying magnification
- G02B 7/10: by relative axial movement of several lenses, e.g. of varifocal objective lens
- B23K 2101/36: Electric or electronic devices
- B23K 2103/12: Copper or alloys thereof
- B23K 2103/18: Dissimilar materials
- Y10T 428/12438: Composite
- Y10T 428/12451: Macroscopically anomalous interface between layers
- Y10T 428/12472: Microscopic interfacial wave or roughness
- Y10T 428/12715: Next to Group IB metal-base component
- Y10T 428/12882: Cu-base component alternative to Ag-, Au-, or Ni-base component
- Y10T 428/12903: Cu-base component
- Y10T 428/12993: Surface feature [e.g., rough, mirror]
- Y10T 428/26: Web or sheet containing structurally defined element or component, the element or component having a specified physical dimension
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The present invention provides a titanium copper foil having improved adhesion to solder and higher resistance to discoloration due to a high temperature and high humidity environment, an acid solution or an alkaline solution, and as well as having improved etching processability. The present invention provides a titanium copper foil comprising a base metal, the base metal having a composition containing Ti of from 1.5 to 5.0% by mass, the balance being copper and inevitable impurities, and having a thickness of from 0.018 to 0.1 mm, wherein the titanium copper foil has an Sn plated layer on a surface of the base metal, and has an adhesive strength of 0.5 N or more as measured by a solder adhesive strength test according to the definition in the specification.

## Claims

### Claim 1

A titanium copper foil comprising a base metal, the base metal having a composition containing Ti of from 1.5% by mass to 5.0% by mass, optionally containing one or more elements selected from the group consisting of Ag, B, Co, Fe, Mg, Mn, Mo, Ni, P, Si, Cr, and Zr in a total amount of from 0% by mass to 1.0% by mass, the balance being copper and inevitable impurities, and the base metal having a thickness of from 0.018 mm to 0.1 mm, wherein the titanium copper foil has an Sn plated layer on a surface of the base metal, and has an adhesive strength of 0.5 N or more as measured by a solder adhesive strength test according to a definition in the specification.

### Claim 2 (depends on 1)

The titanium copper foil according to claim 1, wherein the Sn plated layer has a thickness of from 0.01 to 2.0 μm.

### Claim 3 (depends on 1)

The titanium copper foil according to claim 1, wherein the base metal further contains one or more elements selected from the group consisting of Ag, B, Co, Fe, Mg, Mn, Mo, Ni, P, Si, Cr, and Zr in a total amount of from 0% by mass to 1.0% by mass.

### Claim 4 (depends on 1)

The titanium copper foil according to claim 1, wherein the titanium copper foil has a tensile strength in a direction parallel to a rolling direction of 1100 MPa or more.

### Claim 5 (depends on 1)

The titanium copper foil according to claim 1, wherein the adhesive strength is 20 N or more.

### Claim 6 (depends on 1)

The titanium copper foil according to claim 1, wherein a decreasing rate of the adhesive strength after heating at a temperature of 85° C. for 100 hours relative to the adhesive strength before heating is less than 5%.

### Claim 7 (depends on 1)

The titanium copper foil according to claim 1, wherein the titanium copper foil is used for etching processing.

### Claim 8 (depends on 1)

An electronic component comprising the titanium copper foil according to claim 1.

### Claim 9 (depends on 1)

A joined body of the titanium copper foil according to claim 1 and a solder, wherein the joined body has a joined site to the solder on a surface of the plated layer on the titanium copper foil.

### Claim 10 (depends on 1)

A method for joining the titanium copper foil according to claim 1 to a conductive member, comprising shape processing the titanium copper foil by etching; and joining the resulting profiled product of the titanium copper foil to the conductive member at a location having the plated layer by soldering.

### Claim 11 (depends on 1)

An autofocus module comprising the titanium copper foil according to claim 1 as a spring material.

### Claim 12 (depends on 1)

An autofocusing camera module comprising a lens; a spring member made of the titanium copper foil according to claim 1 for elastically biasing the lens to an initial position in an optical axis direction; and an electromagnetic driving means configured to generate electromagnetic force for withstanding the biasing force of the spring member so that the lens can be driven in the optical axis direction, wherein the electromagnetic driving means comprises a coil, and wherein the spring member is joined to the coil at a location having the plated layer by soldering.

### Claim 13

A method for producing a titanium copper foil, comprising:
preparing a base metal having a composition containing Ti of from 1.5% by mass to 5.0% by mass, optionally containing one or more elements selected from the group consisting of Ag, B, Co, Fe, Mg, Mn, Mo, Ni, P, Si, Cr, and Zr in a total amount of from 0 to 1.0% by mass, the balance being copper and inevitable impurities, wherein the base metal has a thickness of from 0.018 mm to 0.1 mm, and has a surface glossiness of from 100 to 200; and
forming an Sn plated layer having 0.01 μm or more on a surface of the base metal.

### Claim 14 (depends on 13)

The method for producing the titanium copper foil according to claim 13, wherein the Sn plated layer has a thickness of from 0.01 μm to 2.0 μm.

### Claim 15 (depends on 13)

The method for producing the titanium copper foil according to claim 13, wherein the base metal further contains one or more elements selected from the group consisting of Ag, B, Co, Fe, Mg, Mn, Mo, Ni, P, Si, Cr, and Zr in a total amount of 0% by mass to 1.0% by mass.

### Claim 16 (depends on 13)

The method for producing the titanium copper foil according to claim 13, wherein the surface of the base metal having the surface glossiness of from 100 to 200 has arithmetic average roughness (Ra) of 0.5 μm or less.