# US 2017/0285228 A1 · Optical member and method of producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0285228 A1
- Document ID: US20170285228A1
- Status: Published application
- Kind: A1
- Application number: 15/626,594
- Filed: 2017-06-19
- Published: 2017-10-05
- Earliest claimed: 2011-07-21
- Assignees: Canon Kabushiki Kaisha
- Applicants: Canon Kabushiki Kaisha
- Inventors: Masanobu Ogane
- Web page: https://patentgrep.com/patent/US20170285228A1

## CPC

- G02B 1/11: Anti-reflection coatings
- B05D 1/005: {Spin coating}
- B05D 3/0254: {After-treatment}
- G02B 5/0247: {by means of voids or pores}
- G02B 5/0278: {used in transmission}
- B82Y 20/00: Nanooptics, e.g. quantum optics or photonic crystals
- Y10S 977/834: Optical properties of nanomaterial, e.g. specified transparency, opacity, or index of refraction
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

Provided are an optical member having abrasion resistance and transparency and a method of producing the optical member. The method of producing the optical member includes coating a coating material containing hollow particles and a solvent on a substrate and further coating a coating material containing a binder and a solvent to form a film in which the binder lies between the hollow particles; and then drying the film.

## Claims

### Claim 1

A method of producing an optical member having a substrate and an antireflection film having a layer containing particles and a binder, provided on the substrate,
the method comprising forming the layer including:
performing coating with a liquid having particles dispersed in a dispersion medium, and
then performing coating with a solution consisting essentially of a component forming the binder, and a solvent,
wherein shapes of the particles appear on a surface of the layer on a side opposite to the substrate.

### Claim 2 (depends on 1)

The method of producing an optical member according to claim 1, wherein the layer includes the particles at a two-dimensional density of 0.8 or more and 0.88 or less.

### Claim 3 (depends on 1)

The method of producing an optical member according to claim 1, wherein the liquid contains no component forming the binder.

### Claim 4 (depends on 1)

The method of producing an optical member according to claim 1, wherein the component forming the binder is an alkoxysilane hydrolysis-condensation product.

### Claim 5 (depends on 1)

The method of producing an optical member according to claim 1, wherein the coating with the liquid and the coating with the solution are performed by spin coating.

### Claim 6 (depends on 1)

The method of producing an optical member according to claim 1, wherein the dispersion medium contains any one of 1-methoxy-2-propanol, methyl cellosolve, ethyl cellosolve, and butyl cellosolve.

### Claim 7 (depends on 1)

The method of producing an optical member according to claim 1, wherein the particles are hollow particles containing silica.

### Claim 8 (depends on 1)

The method of producing an optical member according to claim 1, wherein the coating with the liquid having the particles dispersed in the dispersion medium is performed on a monolayer or multilayer provided on the substrate.

### Claim 9 (depends on 1)

The method of producing an optical member according to claim 1, wherein on the surface of the layer on the side opposite to the substrate, a part of surfaces of the particles exposes from the binder.

### Claim 10

A method of producing an optical member having a substrate, and an antireflection film having a layer containing particles and a binder, provided on the substrate,
the method comprising forming the layer including:
performing coating with a liquid having particles dispersed in a dispersion medium, and
then performing coating with a solution consisting essentially of a component forming the binder, and a solvent,
wherein a surface of the layer on a side opposite to the substrate has convex portions, and
a shape of the convex portions corresponds to a shape of the particles.

### Claim 11 (depends on 10)

The method of producing an optical member according to claim 10, wherein the layer includes the particles at a two-dimensional density of 0.8 or more and 0.88 or less.

### Claim 12 (depends on 10)

The method of producing an optical member according to claim 10, wherein on the surface of the layer on the side opposite to the substrate, a part of surfaces of the particles exposes from the binder.

### Claim 13

An optical member comprising:
a substrate; and
an antireflection film having a layer containing particles and a binder, provided on the substrate,
wherein shapes of the particles appear on a surface of the layer on a side opposite to the substrate, and
the layer includes the particles at a two-dimensional density of 0.8 or more and 0.88 or less.

### Claim 14 (depends on 13)

The optical member according to claim 13,
wherein the binder has a void, and
a volume ratio of the void to the layer is 5 vol % or more and 25 vol % or less.

### Claim 15 (depends on 13)

The optical member according to claim 13, wherein the particles are hollow particles containing silica.

### Claim 16 (depends on 13)

The optical member according to claim 13, wherein the antireflection film consists of the layer and a monolayer or multilayer provided between the substrate and the layer.

### Claim 17 (depends on 13)

The optical member according to claim 13, wherein a monolayer or multilayer having water repellency or oil repellency is provided on the antireflection film.

### Claim 18 (depends on 15)

The optical member according to claim 15,
wherein the layer contains 15 wt % or more and 50 wt % or less of the binder, and
the layer contains 50 wt % or more and 85 wt % or less of the hollow particles.

### Claim 19 (depends on 13)

The optical member according to claim 13,
wherein the particles are hollow particles,
the hollow particles have an average particle diameter of 15 nm or more and 100 nm or less,
the layer contains 15 wt % or more and 50 wt % or less of the binder,
the layer contains 50 wt % or more and 85 wt % or less of the hollow particles, and
a refractive index of the antireflection film is 1.23 or more and 1.27 or less.

### Claim 20

An optical member comprising:
a substrate; and
an antireflection film having a layer containing particles and a binder, provided on the substrate,
wherein a surface of the layer on a side opposite to the substrate has convex portions,
a shape of the convex portions corresponds to a shape of the particles, and
the layer includes the particles at a two-dimensional density of 0.8 or more and 0.88 or less.