# US 2017/0284741 A1 · Method for non-destructive testing for a refractory part

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0284741 A1
- Document ID: US20170284741A1
- Status: Published application
- Kind: A1
- Application number: 15/512,698
- Filed: 2015-09-14
- Published: 2017-10-05
- Earliest claimed: 2014-09-19
- Assignees: Saint-Gobain Centre De Recherches Et D'Etudes Europeen
- Applicants: Saint-Gobain Centre De Recherches Et D'Etudes Europeen
- Inventors: Olivier BORIES
- Web page: https://patentgrep.com/patent/US20170284741A1

## CPC

- F27D 21/0021: {Devices for monitoring linings for wear}
- G01N 22/02: Investigating the presence of flaws
- G01N 33/388: {Ceramics}
- C03B 5/43: Use of materials for furnace walls, e.g. fire-bricks
- F27D: DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS OR RETORTS, IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KIND OF FURNACE
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

A method for testing the internal structure of a refractory part, has the following steps: a) by a transmission antenna, sending at least one electromagnetic wave, termed a “pulse”, into the refractory part to be tested; b) by a reception antenna, receiving the pulse after reflection thereof by a reflecting zone of the refractory part; c) analyzing the time offset between the two preceding steps in order to deduce the position, in the refractory part, of the reflecting zone, the pulse having a duration less than or equal to 0.5 nanoseconds.

## Claims

### Claim 1

A method for inspecting the internal structure of a refractory part, said method including the following steps:
a) transmitting, by means of an emitting antenna, at least one electromagnetic wave, called the “pulse”, into the refractory part to be inspected;
b) receiving, by means of a receiving antenna, said pulse after it has been reflected by a reflecting zone of the refractory part; and
c) analyzing the time shift between the two preceding steps in order to deduce therefrom the position, in the refractory part, of the reflecting zone, said pulse having a duration shorter than or equal to 0.5 nanoseconds.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein the duration is shorter than 0.2 nanoseconds.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein the pulse is a wave train that has a central frequency higher than 3 gigahertz.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein, in step a), more than 1000 pulses per second are transmitted and/or wherein two successive pulses are separated by more than 100 ns.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein the emitting antenna and the receiving antenna are side-by-side.

### Claim 6 (depends on 1)

The method as claimed in claim 1, wherein the refractory part has a thickness smaller than 300 millimeters.

### Claim 7 (depends on 6)

The method as claimed in claim 6, wherein the refractory part has a thickness smaller than 200 millimeters.

### Claim 8 (depends on 1)

The method as claimed in claim 1, wherein the refractory part is made of a sintered or fused material.

### Claim 9 (depends on 1)

The method as claimed in claim 1, wherein the refractory part is made of a material that consists, for more than 90% of its weight, of one or more oxides chosen from the group made up of ZrO2, Al2O3, SiO2, Cr2O3, Y2O3, and CeO2.

### Claim 10 (depends on 1)

A method for manufacturing a furnace, said method including the following steps:
a) Manufacturing a refractory part; and
b) Inspecting the refractory part using an inspecting method as claimed in claim 1; and
c) If the inspection is passed, placing the refractory part in the furnace, in particular in a region in which it is liable to make contact with molten metal or glass.