# US 2017/0284468 A1 · Bearing ring with insulating coating

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0284468 A1
- Document ID: US20170284468A1
- Status: Published application
- Kind: A1
- Application number: 15/091,025
- Filed: 2016-04-05
- Published: 2017-10-05
- Earliest claimed: 2016-04-05
- Assignees: Schaeffler Technologies AG & Co. KG
- Applicants: Schaeffler Technologies AG & Co. KG
- Inventors: Michael White
- Web page: https://patentgrep.com/patent/US20170284468A1

## CPC

- F16C 33/62: Selection of substances
- F16C 33/64: Special methods of manufacture
- F16C 2202/30: Electric properties; Magnetic properties
- F16C 2206/44: based on aluminium oxide (Al2O3)
- F16C: SHAFTS; FLEXIBLE SHAFTS; ELEMENTS OR CRANKSHAFT MECHANISMS; ROTARY BODIES OTHER THAN GEARING ELEMENTS; BEARINGS

## Abstract

A non-conventional, low temperature, process for applying a thin electrically insulating coating arrangement with high density, high purity, minimal porosity, and improved adhesion strength to a steel bearing component is provided. The bearing component is formed from steel and machined or otherwise formed to a near net shape. A high purity aluminum is electro-chemically deposited on the steel bearing component using a non-aqueous electrolyte in an inert environment to form a high purity aluminum coating at least over a portion of the steel bearing component. A surface of the high purity aluminum coating is then converted by an acid-bath into aluminum oxide to form an insulating layer. A bearing component and a bearing having such components is also provided.

## Claims

### Claim 1

A method for providing an electrically insulating coating to a bearing component, comprising:
providing a bearing component formed from steel and machined or otherwise formed to a near net shape;
electro-chemically depositing a high purity aluminum on the steel bearing component using a non-aqueous electrolyte in an inert environment to form a high purity aluminum coating at least over a portion of the steel bearing component; and
converting a surface of the high purity aluminum coating using an acid-bath into aluminum oxide to form an insulating layer.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
sealing the insulating layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the high purity aluminum has a final thickness of 25-200 μm.

### Claim 4 (depends on 1)

The method of claim 1, wherein the insulating layer has a final thickness of 25-200 μm.

### Claim 5 (depends on 1)

The method of claim 1, wherein the high purity aluminum and the aluminum oxide insulating layer have less than 2% voids or inclusions.

### Claim 6 (depends on 5)

The method of claim 5, wherein the high purity aluminum and the aluminum oxide insulating layer virtually zero voids or inclusions in a test sample examined at a 2500:1 scale enlargement.

### Claim 7 (depends on 1)

The method of claim 1, further comprising:
roughening a surface of the steel bearing component to be coated with the high purity aluminum to a surface roughness Ra of greater than 6 μm.

### Claim 8 (depends on 1)

The method of claim 1, further comprising:
masking a raceway surface of the bearing component prior to at least one of the electro-chemical depositing of the high purity aluminum or the conversion of the surface of the high purity aluminum coating using the acid-bath into aluminum oxide.

### Claim 9 (depends on 1)

The method of claim 1, wherein the insulating layer has a resistance of at least 10 MΩ at 50 VDC.

### Claim 10 (depends on 1)

The method of claim 1, further comprising:
finishing a raceway surface of the steel bearing component after forming the insulating layer.

### Claim 11 (depends on 1)

A rolling bearing having a steel bearing component with the insulating layer formed by the method according to claim 1.

### Claim 12

A rolling bearing comprising:
an inner ring;
an outer ring;
a plurality of rolling elements located between the inner ring and the outer ring;
wherein at least one of the inner ring or the outer ring include, at least over a portion thereof, an insulating coating arrangement comprised of a layer of high purity aluminum located on a steel base component used to form the inner ring or the outer ring and an aluminum oxide insulating layer formed on the high purity aluminum.

### Claim 13 (depends on 12)

The rolling bearing of claim 12, further comprising a sealing layer on the aluminum oxide insulating layer.

### Claim 14 (depends on 12)

The rolling bearing of claim 12, wherein an outer mounting surface of the outer ring includes the insulating layer arrangement.

### Claim 15 (depends on 12)

The rolling bearing of claim 12, wherein an inner mounting surface of the inner ring includes the insulating layer arrangement.

### Claim 16 (depends on 12)

The rolling bearing of claim 12, wherein an outer mounting surface of the outer ring and an inner mounting surface of the inner ring include the insulating layer arrangement.

### Claim 17 (depends on 12)

The rolling bearing of claim 12, wherein the layer of the high purity aluminum has a final thickness of 25-200 μm.

### Claim 18 (depends on 12)