# US 2017/0284018 A1 · Suede type artificial leather with antifouling property and preparation method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0284018 A1
- Document ID: US20170284018A1
- Status: Published application
- Kind: A1
- Application number: 15/512,235
- Filed: 2015-09-23
- Published: 2017-10-05
- Earliest claimed: 2014-09-29
- Assignees: Kolon Industries, Inc.
- Applicants: Kolon Industries, Inc.
- Inventors: Hyuk-jae YOU; Gyoung-cherl GO; Dae-young JUNG; Zhequan PIAO
- Web page: https://patentgrep.com/patent/US20170284018A1

## CPC

- D06N 3/146: {characterised by the macromolecular diols used}
- D06N 3/0004: {using ultra-fine two-component fibres, e.g. island/sea, or ultra-fine one component fibres (< 1 denier)}
- D06N 3/0011: {using non-woven fabrics}
- D06N 3/0075: {Napping, teasing, raising or abrading of the resin coating (raising, napping of the web before coating D06N3/004)}
- D06N 3/14: with polyurethanes
- D06N 3/147: {characterised by the isocyanates used}
- D06N 2209/147: Stainproof, stain repellent
- D06N: WALL, FLOOR, OR LIKE COVERING MATERIALS, e.g. LINOLEUM, OILCLOTH, ARTIFICIAL LEATHER, ROOFING FELT, CONSISTING OF A FIBROUS WEB COATED WITH A LAYER OF MACROMOLECULAR MATERIAL; FLEXIBLE SHEET MATERIAL NOT OTHERWISE PROVIDED FOR

## Abstract

A suede type artificial leather having an antifouling property is provided. A polymeric elastomer is impregnated in a nonwoven fabric formed by three-dimensionally interlacing ultrafine fibers and raising is formed, wherein the polymeric elastomer is a fluorine-containing modified polyurethane, and the fluorine-containing modified polyurethane is obtained by a polymerization of a urethane prepolymer having isocyanate groups at terminals, obtained by reacting a diol and a diisocyanate, and a fluorinated carbon compound having hydroxy functional groups at both terminals. The fluorine-containing modified polyurethane has a weight average molecular weight of 500,000 to 800,000. The suede type artificial leather is prepared by using the fluorine-containing polyurethane elastomer.

## Claims

### Claim 1

A suede type artificial leather having antifouling property in which a polymeric elastomer is impregnated in a nonwoven fabric formed by three-dimensionally interlacing ultrafine fibers and raising is formed,
wherein the polymeric elastomer is a fluorine-containing modified polyurethane, and
the fluorine-containing modified polyurethane is a product obtained by a polymerization reaction between a urethane prepolymer having isocyanate groups at terminals, obtained by reacting a diol and a diisocyanate, and a fluorinated carbon compound having hydroxy functional groups at both terminals, and has a weight average molecular weight (Mw) of 500,000 to 800,000.

### Claim 2 (depends on 1)

The suede type artificial leather having antifouling property according to claim 1, wherein the urethane prepolymer has a weight average molecular weight (Mw) of 400,000 to 700,000.

### Claim 3 (depends on 1)

The suede type artificial leather having antifouling property according to claim 1, wherein the fluorinated carbon compound having hydroxy functional groups at both terminals, has 8 to 14 fluorine groups bonded to one side chain and fluorine content of 50 to 70 mol % in one functional group and is an ether diol having hydroxy functional groups at both terminals.

### Claim 4

A method of preparing a suede type artificial leather having antifouling property in which a polymeric elastomer is impregnated in a nonwoven fabric formed by three-dimensionally interlacing ultrafine fibers and raising is formed,
wherein the polymeric elastomer is a fluorine-containing modified polyurethane, and the fluorine-containing modified polyurethane is prepared by a method comprising:
preparing a urethane prepolymer having a weight average molecular weight (Mw) of 400,000 to 700,000 by reacting a diol and a diisocyanate; and
preparing a polymerization product having a weight average molecular weight (Mw) of 500,000 to 800,000 by reacting the prepolymer and a fluorinated carbon compound having hydroxy functional groups at both terminals.

### Claim 5 (depends on 4)

The method of preparing a suede type artificial leather according to claim 4, wherein the diol and the diisocyanate is reacted at a molar ratio of 1:1.2 to 1:1.4 to prepare the urethane prepolymer.

### Claim 6 (depends on 4)

The method of preparing a suede type artificial leather according to claim 4, wherein the fluorinated carbon compound having hydroxy functional groups at both terminals, has 8 to 14 fluorine groups bonded to one side chain and fluorine content of 50 to 70 mol % in one functional group and is an ether diol having hydroxy functional groups at both terminals.