# US 2017/0283990 A1 · Polyimide fibre and method for producing polyimide fibre

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283990 A1
- Document ID: US20170283990A1
- Status: Published application
- Kind: A1
- Application number: 15/425,249
- Filed: 2017-02-06
- Published: 2017-10-05
- Earliest claimed: 2016-03-31
- Assignees: I.S.T. Corporation
- Applicants: I.S.T Corporation
- Inventors: Ryuta NAKAGAKI; Katsuki MORISHIMA; Koji MORIUCHI
- Web page: https://patentgrep.com/patent/US20170283990A1

## CPC

- D01F 6/74: from polycondensates of cyclic compounds, e.g. polyimides, polybenzimidazoles
- B29C 48/022: {characterised by the choice of material}
- B29C 48/05: Filamentary, e.g. strands
- C08G 73/1067: {Wholly aromatic polyimides, i.e. having both tetracarboxylic and diamino moieties aromatically bound}
- D01D 5/06: Wet spinning methods {(D01D5/0046 takes precedence)}
- D01F 1/10: Other agents for modifying properties
- B29K 2079/08: {PI, i.e. polyimides or derivatives thereof}
- D01F 6/88: from mixtures of polycondensation products as major constituent with other polymers or low-molecular-weight compounds
- D10B 2401/04: Heat-responsive characteristics
- D10B 2401/061: elastic
- D10B 2401/063: high strength
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- D10B: INDEXING SCHEME ASSOCIATED WITH SUBLASSES OF SECTION D, RELATING TO TEXTILES

## Abstract

The method for producing a polyimide fiber includes a coagulation step of forming a polyimide precursor fiber by extruding a polyimide precursor solution containing a polyimide precursor and a compound having an acid dissociation constant (pKa) of a conjugate acid in water at 25° C. of 6.0 to 10 inclusive and an octanol-water partition coefficient (Log P) at 25° C. of −0.75 to 0.75 inclusive into a poor solvent or nonsolvent for the polyimide precursor; and a heat drawing step of forming the polyimide fiber by drawing the polyimide precursor fiber while heating same. The polyimide fiber of the present disclosure has a physical property such that the coefficient of thermal expansion thereof is in the range of −15 ppm/K to 0 ppm/K inclusive.

## Claims

### Claim 1

A polyimide fiber having a coefficient of thermal expansion in the range of −15 ppm/K to 0 ppm/K inclusive.

### Claim 2 (depends on 1)

The polyimide fiber according to claim 1, having an elastic modulus in the range of 320 cN/dtex to 1,100 cN/dtex inclusive.

### Claim 3 (depends on 1)

The polyimide fiber according to claim 1, having a strength in the range of 6.5 cN/dtex to 25 cN/dtex inclusive.

### Claim 4 (depends on 1)

The polyimide fiber according to claim 1, having a specific gravity in the range of 1.45 to 1.55 inclusive.

### Claim 5 (depends on 1)

The polyimide fiber according to claim 1, having an equilibrium moisture regain of at or below 2%.

### Claim 6

A method for producing a polyimide fiber comprising:
a coagulation step of forming a polyimide precursor fiber by extruding a polyimide precursor solution containing a polyimide precursor and a compound having an acid dissociation constant (pKa) of a conjugate acid in water at 25° C. in the range of 6.0 to 10 inclusive and an octanol-water partition coefficient (Log P) at 25° C. in the range of −0.75 to 0.75 inclusive into a poor solvent or nonsolvent for the polyimide precursor; and
a heat drawing step of forming the polyimide fiber by drawing the polyimide precursor fiber while heating same.

### Claim 7 (depends on 6)

The method for producing the polyimide fiber according to claim 6, wherein the poor solvent or the nonsolvent contains water as a main component.

### Claim 8 (depends on 6)

The method for producing the polyimide fiber according to claim 6, wherein:
the polyimide precursor contains a tetracarboxylic acid-based compound-derived unit, and
the polyimide precursor solution contains the compound in the range of 0.1 moles to 1.0 mole inclusive relative to 1 mole of the tetracarboxylic acid-based compound-derived unit.

### Claim 9 (depends on 8)

The method for producing the polyimide fiber according to claim 8, wherein the tetracarboxylic acid-based compound-derived unit is derived from at least either of a 3,3′,4,4′-biphenyltetracarboxylic acid-based compound and a pyromellitic acid-based compound.

### Claim 10 (depends on 6)

The method for producing the polyimide fiber according to claim 6, wherein:
the method further comprises a precursor formation step of obtaining the polyimide precursor by polymerising a tetracarboxylic acid-based compound and a diamine compound in an organic polar solvent; and
the polyimide precursor solution contains the compound in the range of 0.1 moles to 1.0 mole inclusive relative to 1 mole of the tetracarboxylic acid-based compound.

### Claim 11 (depends on 10)

The method for producing the polyimide fiber according to claim 10, wherein the tetracarboxylic acid-based compound is at least either of 3,3′,4,4′-biphenyltetracarboxylic dianhydride and pyromellitic dianhydride.

### Claim 12 (depends on 10)

The method for producing the polyimide fiber according to claim 10, wherein the diamine compound is at least either of para-phenylenediamine and 4,4′-diaminodiphenyl ether.

### Claim 13

A method of using, in production of a polyimide fiber using a polyimide precursor solution as a starting material, a compound having an acid dissociation constant (pKa) of a conjugate acid in water at 25° C. in the range of 6.0 to 10 inclusive and an octanol-water partition coefficient (Log P) at 25° C. in the range of −0.75 to 0.75 inclusive as a coagulation alleviating agent of a polyimide precursor in the polyimide precursor solution.