# US 2017/0283982 A1 · METHOD FOR PRODUCING P-TYPE SiC SINGLE CRYSTAL

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283982 A1
- Document ID: US20170283982A1
- Status: Published application
- Kind: A1
- Application number: 15/508,937
- Filed: 2015-08-31
- Published: 2017-10-05
- Earliest claimed: 2014-09-11
- Assignees: Nippon Steel & Sumitomo Metal Corporation
- Applicants: Nippon Steel & Sumitomo Metal Corporation
- Inventors: Kazuhiko KUSUNOKI; Kazuhito KAMEI; Kazuaki SEKI; Yutaka KISHIDA; Koji MORIGUCHI; Hiroshi KAIDO
- Web page: https://patentgrep.com/patent/US20170283982A1

## CPC

- C30B 17/00: Single-crystal growth onto a seed which remains in the melt during growth, e.g. Nacken-Kyropoulos method (C30B15/00 takes precedence)
- C30B 19/04: the solvent being a component of the crystal composition
- C30B 29/36: Carbides
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

A production method according to an embodiment includes a formation step (S1), a first growth step (S2), a recovery step (S3), and a second growth step (S4). In the formation step (S1), a Si—C solution containing Si, Al and C is formed in a crucible. In the first growth step (S2), a seed shaft is moved down to bring a SiC seed crystal attached to the bottom edge of the seed shaft onto contact with the Si—C solution, and thereafter, an Al-doped p-type SiC single crystal is grown on the SiC seed crystal. After the first growth step (S2), the Al concentration in the Si—C solution is increased in the recovery step (S3). After the recovery step (S3), the Al-doped p-type SiC single crystal is further grown in the second growth step (S4).

## Claims

### Claim 1

A method for producing a p-type SiC single crystal by a solution growth technique by use of a production apparatus comprising a crucible and a seed shaft, wherein, the seed shaft including a bottom edge to which a SiC seed crystal is attachable and being movable up and down, the method comprising:
a formation step of forming a Si—C solution in the crucible, wherein the Si—C solution containing Si, Al and C;
a first growth step of moving down the seed shaft to bring the SiC seed crystal attached to the bottom edge of the seed shaft onto contact with the Si—C solution and thereafter growing an Al-doped p-type SiC single crystal on the SiC seed crystal;
a recovery step of increasing an Al concentration in the Si—C solution after the first growth step; and
a second growth step of further growing the p-type SiC single crystal after the recovery step.

### Claim 2 (depends on 1)

The method for producing a p-type SiC single crystal according to claim 1, wherein
the recovery step includes:
a separation step of moving up the seed shaft to separate the p-type SiC single crystal grown on the SiC seed crystal from the Si—C solution;
a concentration adjustment step of increasing the Al concentration in the Si—C solution after the separation step; and
after the concentration adjustment step, a contact step of moving down the seed shaft to bring the p-type SiC seed crystal onto contact with the Si—C solution.

### Claim 3 (depends on 2)

The method for producing a p-type SiC single crystal according to claim 2, wherein
the recovery step further includes a temperature adjustment step of adjusting a temperature of the Si—C solution to a crystal growth temperature after the concentration adjustment step and before the contact step.

### Claim 4 (depends on 2)

The method for producing a p-type SiC single crystal according to claim 2, wherein
in the concentration adjustment step, an Al—Si-based alloy is supplied to the Si—C solution.

### Claim 5 (depends on 3)

The method for producing a p-type SiC single crystal according to claim 3, wherein
in the concentration adjustment step, an Al—Si-based alloy is supplied to the Si—C solution.

### Claim 6 (depends on 1)

The method for producing a p-type SiC single crystal according to claim 1, wherein:
the Si—C solution formed in the formation step further contains Cu; and
in the recovery step, a Cu concentration as well as the Al concentration in the Si—C solution is increased.

### Claim 7 (depends on 2)

The method for producing a p-type SiC single crystal according to claim 2, wherein:
the Si—C solution formed in the formation step further contains Cu; and
in the recovery step, a Cu concentration as well as the Al concentration in the Si—C solution is increased.

### Claim 8 (depends on 3)

The method for producing a p-type SiC single crystal according to claim 3, wherein:
the Si—C solution formed in the formation step further contains Cu; and
in the recovery step, a Cu concentration as well as the Al concentration in the Si—C solution is increased.

### Claim 9 (depends on 4)

The method for producing a p-type SiC single crystal according to claim 4, wherein:
the Si—C solution formed in the formation step further contains Cu; and
in the recovery step, a Cu concentration as well as the Al concentration in the Si—C solution is increased.

### Claim 10 (depends on 5)

The method for producing a p-type SiC single crystal according to claim 5, wherein:
the Si—C solution formed in the formation step further contains Cu; and
in the recovery step, a Cu concentration as well as the Al concentration in the Si—C solution is increased.