# US 2017/0283966 A1 · Additive for high-purity copper electrolytic refining and method of producing high-purity copper

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283966 A1
- Document ID: US20170283966A1
- Status: Published application
- Kind: A1
- Application number: 15/509,495
- Filed: 2015-10-02
- Published: 2017-10-05
- Earliest claimed: 2014-10-04
- Assignees: Mitsubishi Materials Corporation
- Applicants: Mitsubishi Materials Corporation
- Inventors: Yoshie Tarutani; Kenji Kubota; Kiyotaka Nakaya
- Web page: https://patentgrep.com/patent/US20170283966A1

## CPC

- C25C 1/12: of copper
- C08G 65/329: with organic compounds
- C08L 71/02: Polyalkylene oxides
- C25C: PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY OR REFINING OF METALS; APPARATUS THEREFOR
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The additive for high-purity copper electrolytic refining of the present invention is an additive which is added to a copper electrolyte in electrolytic refining for high-purity copper and is formed of a non-ionic surfactant that includes a hydrophobic group containing an aromatic ring and a hydrophilic group containing a polyoxyalkylene group, in which a dispersion term dD of the Hansen solubility parameters satisfies 10≦dD≦20, a polarity term dP of the Hansen solubility parameters satisfies 6≦dP≦9, and a hydrogen bonding term dH of the Hansen solubility parameters satisfies 9≦dH≦11.

## Claims

### Claim 1

An additive for high-purity copper electrolytic refining which is added to a copper electrolyte in electrolytic refining for high-purity copper and is formed of a non-ionic surfactant that includes a hydrophobic group containing an aromatic ring and a hydrophilic group containing a polyoxyalkylene group, wherein
a dispersion term dD of Hansen solubility parameters satisfies 10≦dD≦20,
a polarity term dP of the Hansen solubility parameters satisfies 6≦dP≦9, and
a hydrogen bonding term dH of the Hansen solubility parameters satisfies 9≦dH≦11.

### Claim 2 (depends on 1)

The additive for high-purity copper electrolytic refining according to claim 1, wherein
the dispersion term dD of the Hansen solubility parameters of the additive satisfies 12≦dD≦17,
the polarity term dP thereof satisfies 7dP≦9, and
the hydrogen bonding term dH thereof satisfies 9≦dH≦11.

### Claim 3

A method of producing high-purity copper comprising:
performing electrolysis using a copper electrolyte to which an additive is added which is formed of a non-ionic surfactant that includes a hydrophobic group containing an aromatic ring and a hydrophilic group containing a polyoxyalkylene group and in which a dispersion term dD of the Hansen solubility parameters satisfies 10≦dD≦20, a polarity term dP of the Hansen solubility parameters satisfies 6≦dP≦9, and a hydrogen bonding term dH of the Hansen solubility parameters satisfies 9≦dH≦11.

### Claim 4 (depends on 3)

The method of producing high-purity copper according to claim 3, wherein
a concentration of the additive in the copper electrolyte is in a range of 2 to 500 mg/L.

### Claim 5 (depends on 3)

The method of producing high-purity copper according to claim 3, wherein
the copper electrolyte is one of the group consisting of a copper sulfate solution, a copper nitrate solution, and a copper chloride solution.

### Claim 6 (depends on 5)

The method of producing high-purity copper according to claim 5, wherein
the copper electrolyte has a copper concentration of 5 to 90 g/L and is one of the group consisting of a copper sulfate solution having a sulfuric acid concentration of 10 to 300 g/L, a copper nitrate solution having a nitric acid concentration of 0.1 to 100 g/L, and a copper chloride solution having a hydrochloric acid concentration of 10 to 300 g/L.

### Claim 7 (depends on 3)

The method of producing high-purity copper according to claim 3, wherein
high-purity copper is produced in which both of the sulfur concentration and the silver concentration are 1 ppm or less.

### Claim 8 (depends on 4)

The method of producing high-purity copper according to claim 4, wherein
the copper electrolyte is one of the group consisting of a copper sulfate solution, a copper nitrate solution, and a copper chloride solution.

### Claim 9 (depends on 8)

The method of producing high-purity copper according to claim 8, wherein
the copper electrolyte has a copper concentration of 5 to 90 g/L and is one of the group consisting of a copper sulfate solution having a sulfuric acid concentration of 10 to 300 g/L, a copper nitrate solution having a nitric acid concentration of 0.1 to 100 g/L, and a copper chloride solution having a hydrochloric acid concentration of 10 to 300 g/L.

### Claim 10 (depends on 4)

The method of producing high-purity copper according to claim 4, wherein
high-purity copper is produced in which both of the sulfur concentration and the silver concentration are 1 ppm or less.

### Claim 11 (depends on 5)

The method of producing high-purity copper according to claim 5, wherein
high-purity copper is produced in which both of the sulfur concentration and the silver concentration are 1 ppm or less.

### Claim 12 (depends on 6)

The method of producing high-purity copper according to claim 6, wherein
high-purity copper is produced in which both of the sulfur concentration and the silver concentration are 1 ppm or less.

### Claim 13 (depends on 8)

The method of producing high-purity copper according to claim 8, wherein
high-purity copper is produced in which both of the sulfur concentration and the silver concentration are 1 ppm or less.

### Claim 14 (depends on 9)

The method of producing high-purity copper according to claim 9, wherein
high-purity copper is produced in which both of the sulfur concentration and the silver concentration are 1 ppm or less.