# US 2017/0283924 A1 · Copper alloy sheet material and method for producing copper alloy sheet material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283924 A1
- Document ID: US20170283924A1
- Status: Published application
- Kind: A1
- Application number: 15/466,912
- Filed: 2017-03-23
- Published: 2017-10-05
- Earliest claimed: 2016-03-31
- Assignees: JX Nippon Mining & Metals Corporation
- Applicants: Jx Nippon Mining & Metals Corporation
- Inventors: KEI SAEGUSA
- Web page: https://patentgrep.com/patent/US20170283924A1

## CPC

- C22F 1/08: of copper or alloys based thereon
- C22C 9/00: Alloys based on copper
- C22C 9/06: with nickel or cobalt as the next major constituent
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A copper alloy sheet material which contains 0.5 to 2.5% by mass of Ni, 0.5 to 2.5% by mass of Co, 0.30 to 1. 2% by mass of Si and 0.0 to 0.5% by mass of Cr, the balance being Cu and unavoidable impurities. The material fulfills the relationships 1.0≦I {200}/I0 {200}≦5.0 and 5.0 μm≦GS≦60.0 μm, and these have the relationship (Equation 1): 5.0≦{(I {200}/I0 {200})/GS}×100≦21.0, in which the I {200} represents an X-ray diffraction intensity of a {200} crystal plane, the I0 {200} represents an X-ray diffraction intensity of a {200} crystal plane of standard pure copper powder, and the GS (μm) represents an average crystal grain size. An electrical conductivity is 43.5% to 55.0% IACS and 0.2% yield strength is 720 to 900 MPa.

## Claims

### Claim 1

A copper alloy sheet material comprising 0.5 to 2.5% by mass of Ni, 0.5 to 2.5% by mass of Co, 0.30 to 1. 2% by mass of Si and 0.0 to 0.5% by mass of Cr, the balance being Cu and unavoidable impurities, wherein the copper alloy sheet material fulfills the relationships 1.0≦I {200}/I0 {200}≦5.0 and 5.0 μm≦GS≦60.0 μm, and these have the relationship (Equation 1): 5.0≦{(I {200}/I0 {200})/GS}×100≦21.0, in which the I {200} represents an X-ray diffraction intensity of a {200} crystal plane on the plate surface, the I0 {200} represents an X-ray diffraction intensity of a {200} crystal plane of standard pure copper powder, and the GS (μm) represents an average crystal grain size as determined by a cutting method of JIS H 0501, and wherein the copper alloy sheet material has an electrical conductivity of 43.5% IACS or more and 55.0% IACS or less, and 0.2% yield strength of 720 MPa or more and 900 MPa or less.

### Claim 2 (depends on 1)

The copper alloy sheet material according to claim 1, further comprising a total of up to 0.5% by mass of one or more elements selected from the group consisting of Mg, Sn, Ti, Fe, Zn and Ag.

### Claim 3

A method for producing a copper alloy sheet material, comprising the successive steps of:
melting and casting a raw material of a copper alloy comprising 0.5 to 2.5% by mass of Ni, 0.5 to 2.5% by mass of Co, 0.30 to 1.2% by mass of Si, and 0.0 to 0.5% by mass of Cr, the balance being Cu and unavoidable impurities;
hot-rolling the material while lowering the temperature from 950° C. to 400° C.;
cold-rolling the material at a rolling rate of 30% or more;
pre-annealing the material by carrying out a heat treatment for the purpose of deposition, at a heating temperature of 350 to 500° C. for 5.0 to 9.5 hours (calculation formula (Equation 2): t=38.0×exp (−0.004 K) is satisfied between the time of the pre-annealing step (t) and a temperature K (° C.);
cold-rolling the material at a rolling rate of 70% or more;
solutionizing the material at a heating temperature of 700 to 980° C.;
aging-treating the material at 350 to 600° C.; and
finish-cold-rolling the material at a rolling rate of 10% or more and 40% or less,
wherein the producing conditions are adjusted such that calculation formula (Equation 3): K=4.5×(I {200}/I0 {200}×exp (0.049a)+76.3) is satisfied among a degree of processing a in the finish cold rolling step, I {200}/I0 {200} after the finish cold rolling step, and a temperature K (° C.) in the pre-annealing step.

### Claim 4 (depends on 3)

The method for producing the copper alloy sheet material according to claim 3, wherein the copper apply sheet material further comprises a total of up to 0.5% by mass of one or more elements selected from the group consisting of Mg, Sn, Ti, Fe, Zn and Ag.