# US 2017/0283919 A1 · Method of manufacturing a cold-rolled steel plate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283919 A1
- Document ID: US20170283919A1
- Status: Published application
- Kind: A1
- Application number: 15/624,981
- Filed: 2017-06-16
- Published: 2017-10-05
- Earliest claimed: 2013-01-31
- Assignees: Nisshin Steel Co., Ltd.
- Applicants: Nisshin Steel Co., Ltd.
- Inventors: Tomohiro Imanaka; Kouji Omosako; Masahito Suzuki
- Web page: https://patentgrep.com/patent/US20170283919A1

## CPC

- C22C 38/28: with titanium or zirconium
- B21B 1/22: for rolling {plates, strips,} bands or sheets of indefinite length (B21B1/42 takes precedence)
- B21B 45/004: {Heating the product}
- C21D 6/001: {containing Ni (C21D6/004 takes precedence)}
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0263: {following hot rolling}
- C21D 9/46: for sheet metals
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/26: with niobium or tantalum
- C22C 38/54: with boron
- C21D 2201/03: Amorphous or microcrystalline structure
- C21D 2211/004: Dispersions; Precipitations
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- Y02P 10/20: Recycling
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B21B: ROLLING OF METAL (auxiliary operations used in connection with metal-working operations covered in B21, see B21C; bending by rolling B21D; manufacture of particular objects, e.g. screws, wheels, rings, barrels, balls, by rolling B21H; pressure welding by means of a rolling mill B23K20/04)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Manufacturing a cold-rolled steel plate by smelting a steel slab having the chemical composition containing on the basis of percent by mass, C from 0.03 to 0.12%, Si from 0 to 1.0%, Mn from 0.2 to 0.8%, P at 0.03% or less, S at 0.03% or less, Ti from 0.04 to 0.3%, and Al at 0.05% or less, with a residue being formed of Fe and unavoidable impurities, the chemical composition satisfying 5*C%-Si %+Mn %−1.5 *Al %<1, and an average diameter of particles of a Ti-based carbide as a precipitate is from 20 to 100 nm; heating the slab to 1200° C. or more and hot rolling, forming a hot-rolled steel plate; winding the hot-rolled steel plate from 500 to 700° C. to form a hot-rolled coil; and cold rolling or annealing and cold rolling the coil obtaining cross-sectional hardness from 200 to 400 HV.

## Claims

### Claim 1

A method of manufacturing a cold-rolled steel plate, comprising the steps of:
smelting a steel slab having the chemical composition containing on the basis of percent by mass, C from 0.03 to 0.12%, Si from 0 to 1.0%, Mn from 0.2 to 0.8%, P at 0.03% or less, S at 0.03% or less, Ti from 0.04 to 0.3%, and Al at 0.05% or less, with a residue being formed of Fe and unavoidable impurities, the chemical composition satisfying 5*C %−Si %+Mn %−1.5*Al %<1, and an average diameter of particles of a Ti-based carbide as a precipitate is from 20 to 100 nm;
heating the steel slab to 1200° C. or more and hot rolling to form a hot-rolled steel plate;
winding the hot-rolled steel plate from 500 to 700° C. to form a hot-rolled coil; and
at least one of cold rolling or annealing and cold rolling the hot-rolled coil obtaining cross-sectional hardness from 200 to 400 HV.

### Claim 2

A method of manufacturing a cold-rolled steel plate, comprising the steps of:
smelting a steel slab having the chemical composition containing, on the basis of percent by mass, at least one of Cr from 0.10 to 2.0%, Ni from 0.05 to 0.5%, Mo from 0.05 to 0.5%, B from 0.0002 to 0.002%, Nb from 0.01 to 0.2%, and V from 0.01 to 0.2%, the chemical composition satisfying 5*C %−Si %+Mn %+1.6*Cr %+0.8*Ni %−1.5*Al %<1;
heating the steel slab to 1200° C. or more and hot rolling to form a hot-rolled steel plate;
winding the hot-rolled steel plate from 500 to 700° C. to form a hot-rolled coil; and
at least one of cold rolling or annealing and cold rolling the hot-rolled coil obtaining cross-sectional hardness from 200 to 400 HV.