# US 2017/0283908 A1 · System and method for enhanced metal recovery during atmospheric leaching of metal sulfides

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283908 A1
- Document ID: US20170283908A1
- Status: Published application
- Kind: A1
- Application number: 15/509,147
- Filed: 2015-09-14
- Published: 2017-10-05
- Earliest claimed: 2014-09-12
- Assignees: FLSmidth A/S
- Applicants: FLSmidth A/S
- Inventors: David J. Chaiko; Frank Baczek; Tom Walters; Sarah (Sally) Rocks; Carlos Eyzaguirre
- Web page: https://patentgrep.com/patent/US20170283908A1

## CPC

- C22B 15/001: {with modification of the copper constituent}
- C22B 1/00: Preliminary treatment of ores or scrap
- C22B 3/02: Apparatus therefor
- C22B 3/04: by leaching (C22B3/18 takes precedence)
- C22B 15/0065: {Leaching or slurrying (with organic compounds C22B3/16)}
- Y02P 10/20: Recycling
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method of improving metal leach kinetics and recovery during atmospheric or substantially atmospheric leaching of a metal sulfide is disclosed. In some embodiments, the method may comprise the steps of: (a) producing a metal sulfide flotation concentrate; (b) processing the metal sulfide concentrate in a reductive activation circuit that operates at a first redox potential, to produce a reductively-activated metal sulfide concentrate; and, (c) subsequently processing the activated metal sulfide concentrate in an oxidative leach circuit to extract metal values. In some disclosed embodiments, reductive activation steps may be employed prior to oxidative leaching steps (including heap leap leaching or bio-leaching steps). In some embodiments, physico-chemical processing steps may be employed during reductive activation and/or oxidative leaching. Systems for practicing the aforementioned methods are also disclosed.

## Claims

### Claim 1

(canceled)

### Claim 2

A method of improving metal leach kinetics and recovery during atmospheric or substantially atmospheric leaching of a metal sulfide, the method comprising:
(a) producing a metal sulfide concentrate via flotation;
(b) processing the metal sulfide concentrate in one or more reductive activation reactors which are held at a first redox potential, to produce a reductively-activated metal sulfide concentrate via a copper metathesis reaction; and,
(c) subsequently processing the reductively-activated metal sulfide concentrate in an oxidative leach process to extract and recover metal values;
wherein the reductively-processed metal sulfide concentrate comprises activated particles composed of chalcopyrite and a transitory, metastable non-stoichiometric binary metal sulfide phase with point defects substantially throughout the entirety of the activated particles.

### Claim 3

A method of improving metal leach kinetics and recovery during atmospheric or substantially atmospheric leaching of a metal sulfide, the method comprising:
(a) producing a metal sulfide concentrate via flotation;
(b) processing the metal sulfide concentrate in one or more reductive activation reactors which are held at a first redox potential, to produce a reductively-activated metal sulfide concentrate via a copper metathesis reaction; and,
(c) subsequently processing the reductively-activated metal sulfide concentrate in an oxidative leach process to extract and recover metal values;
wherein the metal sulfide concentrate comprises chalcopyrite particles and wherein the reductively-processed metal sulfide concentrate comprises converted chalcopyrite particles having a transitionary metastable non-stoichiometric binary metal sulfide mineral phase which differs from covellite.

### Claim 4

(canceled)

### Claim 5

(canceled)

### Claim 6

(canceled)

### Claim 7

(canceled)

### Claim 8

(canceled)

### Claim 9

(canceled)

### Claim 10

A method of improving metal leach kinetics and recovery during atmospheric or substantially atmospheric leaching of a metal sulfide, the method comprising:
(a) producing a metal sulfide concentrate via flotation;
(b) processing the metal sulfide concentrate in one or more reductive activation reactors which are held at a first redox potential, to produce a reductively-activated metal sulfide concentrate via a copper metathesis reaction; and,
(c) subsequently processing the reductively-activated metal sulfide concentrate in an oxidative leach process to extract and recover metal values;
wherein the step of processing the reductively-processed metal sulfide concentrate within a plurality oxidative leach reactors to extract a metal from said reductively-activated concentrate via dissolution further comprises moving the reductively-processed metal sulfide concentrate from a plurality of oxidative, stirred-tank reactors to one or more shear-tank reactors.

### Claim 11 (depends on 10)

The method of claim 10, wherein the plurality of oxidative stirred-tank reactors are in series with said one or more shear-tank reactors.

### Claim 12 (depends on 10)

The method of claim 10, wherein the plurality of oxidative stirred-tank reactors are in parallel with said one or more shear-tank reactors.

### Claim 13

A method of improving metal leach kinetics and recovery during atmospheric or substantially atmospheric leaching of a metal sulfide, the method comprising:
(a) producing a metal sulfide concentrate via flotation;
(b) processing the metal sulfide concentrate in one or more reductive activation reactors which are held at a first redox potential, to produce a reductively-activated metal sulfide concentrate via a copper metathesis reaction; and,
(c) subsequently processing the reductively-activated metal sulfide concentrate in an oxidative leach process to extract and recover metal values;
further comprising converting an outer portion of a metal sulfide within the metal sulfide concentrate to a metastable non-stoichiometric binary metal sulfide mineral phase within the one or more reductive activation reactors so as to introduce point defects substantially throughout the entirety of the activated particle.

### Claim 14

A method of extracting a metal from a metal sulfide particle, comprising:
activating a metal sulfide particle by changing a portion of the metal sulfide particle from a primary metal sulfide to a non-stoichiometric, metastable binary metal sulfide phase to introduce point defects substantially throughout the entirety of the activated particle; and
extracting a metal from the activated metal sulfide particle.

### Claim 15 (depends on 14)

The method of claim 14, wherein extracting the metal from the activated metal sulfide particle comprises an oxidative leaching process.

### Claim 16

(canceled)

### Claim 17

(canceled)

### Claim 18 (depends on 14)

The method of claim 14, wherein the portion of the metal sulfide particle changed to a non-stoichiometric, metastable binary metal sulfide phase is less than about one tenth of the metal sulfide particle by weight or less than about one tenth by volume.

### Claim 19 (depends on 14)

The method of claim 14, wherein activating the metal sulfide particle is performed in a reductive environment ranging from about 200 to about 650 mV (SHE).

### Claim 20

(canceled)

### Claim 21

(canceled)

### Claim 22

(canceled)

### Claim 23

(canceled)

### Claim 24

(canceled)

### Claim 25

(canceled)

### Claim 26

(canceled)

### Claim 27

(canceled)

### Claim 28

(canceled)

### Claim 29 (depends on 14)

The method of claim 14, wherein the primary metal sulfide phase comprises chalcopyrite.

### Claim 30

A method of leaching a metal sulfide concentrate, comprising:
processing a metal sulfide concentrate in a reactor at a first redox potential to produce a reductively-processed metal sulfide concentrate comprising an activated particle having a non-stoichiometric metastable binary metal sulfide phase with point defects introduced substantially throughout the entirety of the activated particle; and
leaching a metal from the reductively-processed metal sulfide concentrate via oxidative dissolution.

### Claim 31

(canceled)

### Claim 32

(canceled)

### Claim 33 (depends on 30)

The method of claim 30, wherein the non-stoichiometric metastable binary metal sulfide phase comprises less than about 10 wt. % or less than about 10 vol. % of the activated particle.

### Claim 34 (depends on 30)

The method of claim 30, wherein the oxidative dissolution occurs in an oxidative leach reactor at a second redox potential greater than a rest potential of the activated particle.

### Claim 35 (depends on 30)

The method of claim 30, wherein the first redox potential ranges from about 200 to about 650 mV (SHE).

### Claim 36 (depends on 30)

The method of claim 30, wherein the second redox potential ranges from about 600 to about 750 mV (SHE).

### Claim 37 (depends on 30)

The method of claim 30, wherein the metal sulfide concentrate comprises chalcopyrite.

### Claim 38 (depends on 30)

The method of claim 30, wherein the metal leached from the metal sulfide concentrate is copper.

### Claim 39

A method of extracting a metal from a metal sulfide particle, comprising:
activating a metal sulfide particle by changing a portion of the metal sulfide particle from a primary metal sulfide to a binary metal sulfide phase; and
if there is a sufficient amount of activated binary metal sulfide present, extracting a metal from the metal sulfide by an oxidative leach process.

### Claim 40 (depends on 39)

The method of claim 39, wherein the oxidative leach process substantially reduces the physical and electrochemical passivation of the activated metal sulfide particle by a physicochemical process.

### Claim 41 (depends on 39)

The method of claim 39, wherein the binary metal sulfide phase comprises a non-stoichiometric metastable binary metal sulfide phase with point defects substantially throughout the entirety of the activated particle.

### Claim 42

(canceled)

### Claim 43

(canceled)

### Claim 44 (depends on 41)

The method of claim 41, wherein the non-stoichiometric metastable binary metal sulfide phase comprises less than about 10 wt. % or less than about 10 vol. % of the activated metal sulfide particle.

### Claim 45