# US 2017/0283905 A1 · Method for producing granular metallic iron

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283905 A1
- Document ID: US20170283905A1
- Status: Published application
- Kind: A1
- Application number: 15/509,729
- Filed: 2015-09-03
- Published: 2017-10-05
- Earliest claimed: 2014-09-10
- Assignees: Kabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.)
- Applicants: Kabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.)
- Inventors: Yui HOSONO; Masaki SHIMAMOTO; Shingo YOSHIDA; Masataka TATEISHI
- Web page: https://patentgrep.com/patent/US20170283905A1

## CPC

- C22B 1/16: Sintering; Agglomerating
- C21B 13/00: Making spongy iron or liquid steel, by direct processes
- C22B 1/244: organic
- C22B 1/245: with carbonaceous material for the production of coked agglomerates
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C21B: MANUFACTURE OF IRON OR STEEL (preliminary treatment of ferrous ores or scrap C22B1/00)

## Abstract

A method for producing granular metallic iron of the present invention includes: an agglomeration step of obtaining agglomerates through agglomeration of a mixture that contains an iron oxide-containing material and a carbonaceous reducing agent; and a granulation step of obtaining granular metallic iron by heating the agglomerates, reducing iron oxides in the agglomerates, aggregating generated metallic iron to be granular while separating the metallic iron from slag generated as a by-product, and thereafter cooling and solidifying the metallic iron, wherein agglomerates satisfying all the conditions given by formulas (1) to (3) below are used as the agglomerates: (1) [(total CaO amount+total SiO2 amount+total Al2O3 amount)/total Fe amount]≧0.250; (2) (total CaO amount/total SiO2 amount)≧0.9; (3) [total Al2O3 amount/(total CaO amount+total SiO2 amount+total Al2O3 amount)]×100≧9.7. In the formulas, the total CaO amount, the total SiO2 amount, the total Al2O3 amount and the total Fe amount respectively represent the mass percentage of CaO, the mass percentage of SiO2, the mass percentage of Al2O3 and the mass percentage of Fe contained in the agglomerates.

## Claims

### Claim 1

A method for producing granular metallic iron, comprising:
an agglomeration step of obtaining agglomerates through agglomeration of a mixture that contains an iron oxide-containing material and a carbonaceous reducing agent; and
a granulation step of obtaining granular metallic iron by heating the agglomerates, reducing iron oxides in the agglomerates, aggregating generated metallic iron to be granular while separating the metallic iron from slag generated as a by-product, and thereafter cooling and solidifying the metallic iron;
wherein agglomerates satisfying all the conditions given by formulas (1) to (3) below are used as the agglomerates:
[(total CaO amount+total SiO2 amount+total Al2O3 amount)/total Fe amount]≧0.250 (1);
(total Cat) amount/total SiO2 amount)≧0.9 (2);
[total Al2O3 amount/(total CaO amount+total SiO2 amount+total Al2O3 amount)]×100≧9.7 (3),
wherein the total CaO amount, the total SiO2 amount, the total Al2O3 amount and the total Fe amount in the formulas (1) to (3) respectively represent the mass percentage of CaO, the mass percentage of SiO2, the mass percentage of Al2O3 and the mass percentage of Fe comprised in the agglomerates.

### Claim 2 (depends on 1)

The method for producing granular metallic iron of claim 1, wherein in the agglomeration step an Al2O3-containing material is added to the mixture, before the agglomeration of the mixture.