# US 2017/0283900 A1 · High-strength hot-dip galvanized steel sheet and method for manufacturing the same (as amended)

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283900 A1
- Document ID: US20170283900A1
- Status: Published application
- Kind: A1
- Application number: 15/506,968
- Filed: 2015-08-14
- Published: 2017-10-05
- Earliest claimed: 2014-08-28
- Assignees: Jfe Steel Corporation
- Applicants: Jfe Steel Corporation
- Inventors: Hiroshi Hasegawa; Koichiro Fujita
- Web page: https://patentgrep.com/patent/US20170283900A1

## CPC

- C21D 9/46: for sheet metals
- C21D 8/0436: {Cold rolling}
- C22C 18/04: with aluminium as the next major constituent
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/16: containing copper
- C22C 38/38: with more than 1.5% by weight of manganese
- C23C 2/28: Thermal after-treatment, e.g. treatment in oil bath
- C23C 2/29: {Cooling or quenching}
- C23C 2/40: Plates; Strips
- C21D 2211/001: Austenite
- C21D 2211/008: Martensite
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A high-strength hot-dip galvanized steel sheet and a method for manufacturing the steel sheet are provided. The high-strength hot-dip galvanized steel sheet has a specific composition including C, Si, Mn, etc. In this chemical composition, the content of Ti [Ti] and the content of N [N] satisfy [Ti]>4[N]. The high-strength hot-dip galvanized steel sheet has a microstructure including martensite at an area fraction of 60% or more and 90% or less, polygonal ferrite at an area fraction of more than 5% and 40% or less, and retained austenite at an area fraction of less than 3% (including 0%). The average hardness of the martensite is 450 or more and 600 or less in terms of Vickers hardness, and the average crystal grain diameter of the martensite is 10 μm or less. The standard deviation of the crystal grain diameters of the martensite is 4.0 μm or less.

## Claims

### Claim 1

A high-strength hot-dip galvanized steel sheet having a chemical composition comprising, in mass %, C: 0.13 to 0.25%, Si: 0.01 to 1.00%, Mn: 1.5 to 4.0%, P: 0.100% or less, S: 0.02% or less, Al: 0.01 to 1.50%, N: 0.001 to 0.010%, Ti: 0.005 to 0.100%, and B: 0.0005 to 0.0050%, with the balance being Fe and inevitable impurities, the content of Ti and the content of N satisfying formula (1) below, and
the high-strength hot-dip galvanized steel sheet having a microstructure including martensite at an area fraction of 60% or more and 90% or less, polygonal ferrite at an area fraction of more than 5% and 40% or less, and retained austenite at an area fraction of less than 3% (including 0%), wherein the martensite has an average hardness of 450 or more and 600 or less in terms of Vickers hardness, wherein the martensite has an average crystal grain diameter of 10 μm or less, and wherein the standard deviation of crystal grain diameters of the martensite is 4.0 μm or less:
[Ti]>4[N] (1),
where [Ti] represents the content of Ti (mass %), and [N] represents the content of N (mass %).

### Claim 2 (depends on 1)

The high-strength hot-dip galvanized steel sheet according to claim 1, further comprising, in mass %, at least one element selected from Cr: 0.005 to 2.000%, Mo: 0.005 to 2.000%, V: 0.005 to 2.000%, Ni: 0.005 to 2.000%, Cu: 0.005 to 2.000%, and Nb: 0.005 to 2.000%.

### Claim 3 (depends on 1)

The high-strength hot-dip galvanized steel sheet according to claim 1, further comprising, in mass %, at least one element selected from Ca: 0.001 to 0.005% and REM: 0.001 to 0.005%.

### Claim 4 (depends on 1)

A method for manufacturing a high-strength hot-dip galvanized steel sheet, the method comprising: a hot rolling step of subjecting a steel slab having the chemical composition according to claim 1 to hot rolling to thereby obtain a hot-rolled sheet, cooling the hot-rolled sheet after completion of finishing rolling in the hot rolling such that a total residence time at 600 to 700° C. is 10 seconds or shorter, and then coiling the resulting hot-rolled sheet such that an average coiling temperature is 400° C. or higher and lower than 600° C. and that the difference between an average value of coiling temperature in a 100 mm-wide region at a widthwise central position of the steel sheet and an average value of the coiling temperature in a 100 mm-wide region at a lateral edge position of the steel sheet is 70° C. or lower; a cold rolling step of cold-rolling the hot-rolled sheet at a rolling reduction of more than 20% to thereby obtain a cold-rolled sheet; an annealing step of heating the cold-rolled sheet to 700° C. or lower at an average heating rate of 5° C./s or more, then heating the resulting cold-rolled sheet to 720° C. or higher and 850° C. or lower at an average heating rate of 1° C./s or less, and holding the resulting cold-rolled sheet at 720° C. or higher and 850° C. or lower for 30 seconds or longer and 1,000 seconds or shorter; a cooling step of cooling the cold-rolled sheet subjected to the annealing step at an average cooling rate of 3° C./s or more; a hot-dip galvanizing step of subjecting the cold-rolled sheet subjected to the cooling step to hot-dip galvanizing treatment to thereby obtain a hot-dip galvanized sheet; and a post-plating cooling step of cooling the hot-dip galvanized sheet subjected to the hot-dip galvanizing step such that a residence time in a temperature range of (an Ms point −50° C.) to the Ms point is 2 seconds or longer.

### Claim 5 (depends on 4)

The method for manufacturing a high-strength hot-dip galvanized steel sheet according to claim 4, the method further comprising, after the hot-dip galvanizing step and before the post-plating cooling step, a galvannealing step of subjecting the hot-dip galvanized steel sheet to galvannealing treatment.

### Claim 6 (depends on 4)

The method for manufacturing a high-strength hot-dip galvanized steel sheet according to claim 4, the method further comprising, after the post-plating cooling step, a tempering step of performing tempering treatment at a temperature of 350° C. or lower.

### Claim 7 (depends on 2)

The high-strength hot-dip galvanized steel sheet according to claim 2, further comprising, in mass %, at least one element selected from Ca: 0.001 to 0.005% and REM: 0.001 to 0.005%.

### Claim 8 (depends on 5)

The method for manufacturing a high-strength hot-dip galvanized steel sheet according to claim 5, the method further comprising, after the post-plating cooling step, a tempering step of performing tempering treatment at a temperature of 350° C. or lower.

### Claim 9 (depends on 2)

A method for manufacturing a high-strength hot-dip galvanized steel sheet, the method comprising: a hot rolling step of subjecting a steel slab having the chemical composition according to claim 2 to hot rolling to thereby obtain a hot-rolled sheet, cooling the hot-rolled sheet after completion of finishing rolling in the hot rolling such that a total residence time at 600 to 700° C. is 10 seconds or shorter, and then coiling the resulting hot-rolled sheet such that an average coiling temperature is 400° C. or higher and lower than 600° C. and that the difference between an average value of coiling temperature in a 100 mm-wide region at a widthwise central position of the steel sheet and an average value of the coiling temperature in a 100 mm-wide region at a lateral edge position of the steel sheet is 70° C. or lower; a cold rolling step of cold-rolling the hot-rolled sheet at a rolling reduction of more than 20% to thereby obtain a cold-rolled sheet; an annealing step of heating the cold-rolled sheet to 700° C. or lower at an average heating rate of 5° C./s or more, then heating the resulting cold-rolled sheet to 720° C. or higher and 850° C. or lower at an average heating rate of 1° C./s or less, and holding the resulting cold-rolled sheet at 720° C. or higher and 850° C. or lower for 30 seconds or longer and 1,000 seconds or shorter; a cooling step of cooling the cold-rolled sheet subjected to the annealing step at an average cooling rate of 3° C./s or more; a hot-dip galvanizing step of subjecting the cold-rolled sheet subjected to the cooling step to hot-dip galvanizing treatment to thereby obtain a hot-dip galvanized sheet; and a post-plating cooling step of cooling the hot-dip galvanized sheet subjected to the hot-dip galvanizing step such that a residence time in a temperature range of (an Ms point −50° C.) to the Ms point is 2 seconds or longer.

### Claim 10 (depends on 3)

A method for manufacturing a high-strength hot-dip galvanized steel sheet, the method comprising: a hot rolling step of subjecting a steel slab having the chemical composition according to claim 3 to hot rolling to thereby obtain a hot-rolled sheet, cooling the hot-rolled sheet after completion of finishing rolling in the hot rolling such that a total residence time at 600 to 700° C. is 10 seconds or shorter, and then coiling the resulting hot-rolled sheet such that an average coiling temperature is 400° C. or higher and lower than 600° C. and that the difference between an average value of coiling temperature in a 100 mm-wide region at a widthwise central position of the steel sheet and an average value of the coiling temperature in a 100 mm-wide region at a lateral edge position of the steel sheet is 70° C. or lower; a cold rolling step of cold-rolling the hot-rolled sheet at a rolling reduction of more than 20% to thereby obtain a cold-rolled sheet; an annealing step of heating the cold-rolled sheet to 700° C. or lower at an average heating rate of 5° C./s or more, then heating the resulting cold-rolled sheet to 720° C. or higher and 850° C. or lower at an average heating rate of 1° C./s or less, and holding the resulting cold-rolled sheet at 720° C. or higher and 850° C. or lower for 30 seconds or longer and 1,000 seconds or shorter; a cooling step of cooling the cold-rolled sheet subjected to the annealing step at an average cooling rate of 3° C./s or more; a hot-dip galvanizing step of subjecting the cold-rolled sheet subjected to the cooling step to hot-dip galvanizing treatment to thereby obtain a hot-dip galvanized sheet; and a post-plating cooling step of cooling the hot-dip galvanized sheet subjected to the hot-dip galvanizing step such that a residence time in a temperature range of (an Ms point −50° C.) to the Ms point is 2 seconds or longer.

### Claim 11 (depends on 7)

A method for manufacturing a high-strength hot-dip galvanized steel sheet, the method comprising: a hot rolling step of subjecting a steel slab having the chemical composition according to claim 7 to hot rolling to thereby obtain a hot-rolled sheet, cooling the hot-rolled sheet after completion of finishing rolling in the hot rolling such that a total residence time at 600 to 700° C. is 10 seconds or shorter, and then coiling the resulting hot-rolled sheet such that an average coiling temperature is 400° C. or higher and lower than 600° C. and that the difference between an average value of coiling temperature in a 100 mm-wide region at a widthwise central position of the steel sheet and an average value of the coiling temperature in a 100 mm-wide region at a lateral edge position of the steel sheet is 70° C. or lower; a cold rolling step of cold-rolling the hot-rolled sheet at a rolling reduction of more than 20% to thereby obtain a cold-rolled sheet; an annealing step of heating the cold-rolled sheet to 700° C. or lower at an average heating rate of 5° C./s or more, then heating the resulting cold-rolled sheet to 720° C. or higher and 850° C. or lower at an average heating rate of 1° C./s or less, and holding the resulting cold-rolled sheet at 720° C. or higher and 850° C. or lower for 30 seconds or longer and 1,000 seconds or shorter; a cooling step of cooling the cold-rolled sheet subjected to the annealing step at an average cooling rate of 3° C./s or more; a hot-dip galvanizing step of subjecting the cold-rolled sheet subjected to the cooling step to hot-dip galvanizing treatment to thereby obtain a hot-dip galvanized sheet; and a post-plating cooling step of cooling the hot-dip galvanized sheet subjected to the hot-dip galvanizing step such that a residence time in a temperature range of (an Ms point −50° C.) to the Ms point is 2 seconds or longer.

### Claim 12 (depends on 9)

The method for manufacturing a high-strength hot-dip galvanized steel sheet according to claim 9, the method further comprising, after the hot-dip galvanizing step and before the post-plating cooling step, a galvannealing step of subjecting the hot-dip galvanized steel sheet to galvannealing treatment.

### Claim 13 (depends on 9)

The method for manufacturing a high-strength hot-dip galvanized steel sheet according to claim 9, the method further comprising, after the post-plating cooling step, a tempering step of performing tempering treatment at a temperature of 350° C. or lower.

### Claim 14 (depends on 12)

The method for manufacturing a high-strength hot-dip galvanized steel sheet according to claim 12, the method further comprising, after the post-plating cooling step, a tempering step of performing tempering treatment at a temperature of 350° C. or lower.

### Claim 15 (depends on 10)

The method for manufacturing a high-strength hot-dip galvanized steel sheet according to claim 10, the method further comprising, after the hot-dip galvanizing step and before the post-plating cooling step, a galvannealing step of subjecting the hot-dip galvanized steel sheet to galvannealing treatment.

### Claim 16 (depends on 10)

The method for manufacturing a high-strength hot-dip galvanized steel sheet according to claim 10, the method further comprising, after the post-plating cooling step, a tempering step of performing tempering treatment at a temperature of 350° C. or lower.

### Claim 17 (depends on 15)

The method for manufacturing a high-strength hot-dip galvanized steel sheet according to claim 15, the method further comprising, after the post-plating cooling step, a tempering step of performing tempering treatment at a temperature of 350° C. or lower.

### Claim 18 (depends on 11)

The method for manufacturing a high-strength hot-dip galvanized steel sheet according to claim 11, the method further comprising, after the hot-dip galvanizing step and before the post-plating cooling step, a galvannealing step of subjecting the hot-dip galvanized steel sheet to galvannealing treatment.

### Claim 19 (depends on 11)

The method for manufacturing a high-strength hot-dip galvanized steel sheet according to claim 11, the method further comprising, after the post-plating cooling step, a tempering step of performing tempering treatment at a temperature of 350° C. or lower.

### Claim 20 (depends on 18)

The method for manufacturing a high-strength hot-dip galvanized steel sheet according to claim 18, the method further comprising, after the post-plating cooling step, a tempering step of performing tempering treatment at a temperature of 350° C. or lower.