# US 2017/0283896 A1 · Low-temperature high-strength-and-ductility high manganese steel, and high manganese steel plate and high manganese steel tube manufacturing process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0283896 A1
- Document ID: US20170283896A1
- Status: Published application
- Kind: A1
- Application number: 15/310,085
- Filed: 2015-04-15
- Published: 2017-10-05
- Earliest claimed: 2014-08-14
- Assignees: Yanshan University
- Applicants: Yanshan University
- Inventors: Yu hui WANG; Xiao xu HUANG; Tian sheng WANG; Yan PENG; Yan ming HE; Ya nan ZHENG; Bo LIAO
- Web page: https://patentgrep.com/patent/US20170283896A1

## CPC

- C21D 9/08: for tubular bodies or pipes
- B21B 1/026: {Rolling}
- B21B 1/30: in a non-continuous process {(B21B1/224 takes precedence)}
- B21B 3/02: Rolling special iron alloys {, e.g. stainless steel}
- B21C 1/003: {Drawing materials of special alloys so far as the composition of the alloy requires or permits special drawing methods or sequences}
- B21C 1/22: specially adapted for making tubular articles (bending sheet metal into tubular form by drawing B21D5/10)
- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- C21D 6/005: {containing Mn}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/021: involving particular fabrication steps or treatments of ingots or slabs
- C21D 8/0236: {Cold rolling}
- C21D 8/0263: {following hot rolling}
- C21D 8/10: during manufacturing of tubular bodies
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/04: containing manganese
- B21B 2001/221: {by cold-rolling}
- C21D 1/26: Methods of annealing
- C21D 8/0221: characterised by the working steps
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B21B: ROLLING OF METAL (auxiliary operations used in connection with metal-working operations covered in B21, see B21C; bending by rolling B21D; manufacture of particular objects, e.g. screws, wheels, rings, barrels, balls, by rolling B21H; pressure welding by means of a rolling mill B23K20/04)
- B21C: MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES, PROFILES OR LIKE SEMI-MANUFACTURED PRODUCTS OTHERWISE THAN BY ROLLING; AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKING WITHOUT ESSENTIALLY REMOVING MATERIAL
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The present invention discloses a machining technology of a low-temperature high-strength-ductility high manganese steel, high manganese steel plate, and high manganese steel tube, and a high manganese steel comprises the following components in percentage by weight: Mn 30%-36%, C 0.02%-0.06%, S≦0.01%, P≦0.008% and the balance being Fe. Smelted steel ingots are subject to solution treatment and are rolled and homogenized to obtain a high manganese steel plate or are drawn to form a high manganese steel tube. The hot-rolled or cold-rolled steel plate after being hot-rolled has tremendous application value in the fields of low-temperature applications, such as the steel plate used for a low temperature pressure container.

## Claims

### Claim 1

A low-temperature high-strength-ductility high manganese steel, comprising the following components in percentage by weight: Mn 30%-36%, C 0.02%-0.06%, S≦0.01%, P<0.008% and the balance being Fe.

### Claim 2 (depends on 1)

The low-temperature high-strength-ductility high manganese steel of claim 1, wherein the content of Mn in percentage by weight is 32%-35%.

### Claim 3 (depends on 1)

The low-temperature high-strength-ductility high manganese steel of claim 1, wherein the content of Mn in percentage by weight is 34%-34.5%.

### Claim 4

A machining technology of the low-temperature high-strength-ductility high manganese steel plate, comprising process steps of smelting high manganese steel, post-treating a steel ingot, and cogging and rolling to form a plate, wherein the process steps comprise the following parameters:
A. smelting the high manganese steel: calculating a feeding ratio according to the percentage by weight of components in the high manganese steel: Mn 30%-36%, C 0.02%-0.06%, S≦0.01%, P≦0.008% and the balance being Fe, and smelting the components into the steel ingot;
B. post-treating the steel ingot: keeping the steel ingot smelted in step A under the condition of 1150 DEG C.-1200 DEG C. and performing heat treatment for 2-4 hours, and then transferring the steel ingot into a water quenching tank at room temperature to complete solid solution treatment; and
C. cogging and rolling the steel ingot to form a plate: performing hot rolling, tempering and homogenizing after cogging the steel ingot after solid solution treatment.

### Claim 5 (depends on 4)

The machining technology of the low-temperature high-strength-ductility high manganese steel plate of claim 4, wherein the content of Mn in percentage by weight in the high manganese steel obtained in step A is 32%-35%, and an industrial frequency electric induction furnace and a furnace argon positive pressure environment are adopted for the melting of the high manganese steel.

### Claim 6 (depends on 4)

The machining technology of the low-temperature high-strength-ductility high manganese steel plate of claim 4, wherein the technology conditions of hot-rolling and homogenizing in step C comprise: firstly, heating steel ingot blanks to 800-1000 DEG C.; then, hot-rolling the steel ingot blanks to obtain a crude plate with a thickness of 10-20 mm; then, maintaining the crude plate at 1000-1100 DEG C. for 1-2 hours, and transferring the crude plate to a room-temperature water quenching tank for homogenization.

### Claim 7 (depends on 4)

The machining technology of the low-temperature high-strength-ductility high manganese steel plate of claim 4, wherein further comprising step D: performing cold-rolling, annealing and homogenizing forming on the crude plate after being hot-rolled and homogenized.

### Claim 8 (depends on 7)

The machining technology of the low-temperature high-strength-ductility high manganese steel plate of claim 7, wherein the conditions of cold-rolling and homogenizing in step D comprise: performing cold-rolling for 10-20 passes at room temperature on the crude plate after being hot-rolled and homogenized to form a plate with a thickness of 1.0-2.0 mm, the rolling reduction is 90%-93%; maintaining the steel plate under 500-1000 DEG C. for 0.5-2 hours, then transferring the steel plate to the room temperature water quenching tank for homogenization.

### Claim 9 (depends on 8)

The machining technology of the low-temperature high-strength-ductility high manganese steel plate of claim 8, wherein comprising the steps of maintaining the steel plate after being cold-rolled in step D at 500-710 DEG C. for 1 hour, and then transferring the steel plate to the room temperature water quenching tank for homogenization, the obtained steel plate has dimple fractures in toughness cracks under the conditions of −196 DEG C. to −180 DEG C. and constant pressure, and the product strength and uniform elongation exceeds 50 GPa • %.

### Claim 10 (depends on 8)

The machining technology of the low-temperature high-strength-ductility high manganese steel plate of claim 8, wherein comprising the steps of maintaining the steel plate after being cold-rolled in step D at 800-1000 DEG C. for 1 hour, and then transferring the steel plate to the room temperature water quenching tank for homogenization, the obtained steel plate has the characteristic of intergranular fractures under the conditions of −196 DEG C. to −170 DEG C. and constant pressure, and mechanical performance indexes comprise: yield strength: higher than 410 MPa, tensile strength: higher than 620 MPa, and elongation: greater than 8%.

### Claim 11

A machining technology of a low-temperature high-strength-ductility high manganese steel tubular product, comprising process steps of smelting high manganese steel, post-treating a steel ingot, and cogging and rolling to form a plate, wherein the process steps comprise the following parameters:
step A. calculating a feeding ratio according to the percentage by weight of components in the high manganese steel: Mn 30%-36%, C 0.02%-0.06%, S≦0.01%, P≦0.008% and the balance being Fe, and smelting the components into the steel ingot;
step B. post-treating the steel ingot: maintaining the steel ingot smelted in step A under the condition of 1150 DEG C.-1200 DEG C., performing heat treatment for 2-4 hours, and then transferring the steel ingot into the room temperature water quenching tank to complete solid solution treatment; and
step C. cogging and drawing to obtain the tubular product: performing hot rolling, tempering and homogenizing on the steel ingot after cogging the steel ingot on which solid solution treatment is performed.

### Claim 12 (depends on 11)

The machining technology of a low-temperature high-strength-ductility high manganese steel tubular product of claim 11, wherein further comprising step D: cold-drawing the tubular product at room temperature after the hot drawing and homogenizing into a thin-wall tubular product with a wall thickness of 1.0 mm-2.0 mm, maintaining the thin-wall tubular product at 600 DEG C. to 850 DEG C. for 0.5-2 hours, and then transferring into a water quenching tank for homogenization.

### Claim 13 (depends on 11)

The machining technology of the low-temperature high-strength-ductility high manganese tubular product of claim 11, wherein the content of Mn in percentage by weight in the components of the high manganese steel is 32%-35%, and the content of C in percentage by weight is 0.04%.